Gigacycle fatigue properties of a modified-ausformed Si-Mn steel and effects of microstructure

被引:24
作者
Furuya, Y [1 ]
Matsuoka, S
机构
[1] Natl Inst Mat Sci, Fatigue Grp, Ibaraki 3050047, Japan
[2] Natl Inst Mat Sci, Mat Informat Technol Stn, Ibaraki 3050047, Japan
来源
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 2004年 / 35A卷 / 06期
关键词
D O I
10.1007/s11661-004-0080-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fatigue tests were conducted for modified-ausformed, oil-quenched, and water-quenched versions of a Si-Mn steel (JIS-SMn443) with a chemical composition of 0.42C-0.2Si-1.52Mn (in mass pct). The Si-Mn Steel has an advantage with respect to recycling, since it contains no Cr or Mo, although the steel has disadvantages with respect to tempering resistance and hardenablility. Although the tempering resistance was not improved by modified ausforming, the problem of hardenability was minimized, since modified ausforming created fine and uniform martensite. The gigacycle fatigue properties of the Si-Mn steel were improved by the modified ausforming. The low-strength modified-ausformed steel (AF1400) was free of fish-eye fractures and had a fatigue limit of 770 MPa at 10(9) cycles. In spite of the occurrence of fish-eye fractures, the high-strength modified-ausformed steel (AF2000) achieved a fatigue limit of 830 MPa at 10(10) cycles, higher than the 710 MPa limit of the water-quenched steel (QT2000W). The fatigue limits of the oil-quenched steels (QT1400 and QT2000), which contained numerous and large nonuniform structures, could not be determined because of the temperature increase of specimens during the 20 kHz tests. The fracture surfaces revealed optically dark areas (ODAs) even in the modified-ausformed steel when the specimens failed at over 10(7) cycles, since the steel was partially recrystallized during modified ausforming. The gap of fatigue limit between the AF2000 and QT200OW steels was not entirely explained by the difference of the ODA sizes. Also, the sizes of the nonuniform structures were likely to play an important role in the gigacycle fatigue properties, since the sizes in AF2000 were smaller than those in QT2000W.
引用
收藏
页码:1715 / 1723
页数:9
相关论文
共 24 条
[1]   Significance of size and type of inclusions on giga-cycle fatigue in high-strength steels [J].
Abe, T ;
Furuya, Y ;
Matsuoka, S .
TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2003, 89 (06) :711-717
[2]  
Abe T., 2001, T JPN SOC MECH ENG A, V67-664, P1988
[3]  
ABE T, 2001, T JSSR, V46, P19
[4]  
BOCK RA, 1968, MET PROG, V94, P107
[5]   1010-cycle fatigue properties of 1800 MPa-class JIS-SUP7 spring steel [J].
Furuya, Y ;
Abe, T ;
Matsuoka, S .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2003, 26 (07) :641-645
[6]   Improvement of gigacycle fatigue properties by modified ausforming in 1600 and 2000 MPA-class low-alloy steels [J].
Furuya, Y ;
Matsuoka, S .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2002, 33 (11) :3421-3431
[7]   Gigacycle fatigue properties for high-strength low-alloy steel at 100 Hz, 600 Hz, and 20 kHz [J].
Furuya, Y ;
Matsuoka, S ;
Abe, T ;
Yamaguchi, K .
SCRIPTA MATERIALIA, 2002, 46 (02) :157-162
[8]   Microstructural analyses of modified-ausformed medium-carbon steel with high resistance to hydrogen embrittlement by atomic force microscopy [J].
Hayakawa, M ;
Terasaki, S ;
Hara, T ;
Tsuzaki, K ;
Matsuoka, S .
JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2002, 66 (07) :745-753
[9]   Atomic force microscopy of induction- and furnace-heating-tempered prestressed steels with different delayed fracture properties [J].
Hayakawa, M ;
Matsuoka, S ;
Tsuzaki, K ;
Hanada, H ;
Sugisaki, M .
SCRIPTA MATERIALIA, 2002, 47 (10) :655-661
[10]  
ISHII H, 2001, SPECIAL TECHNICAL PU, V1, P59