Preparation of TaB2-SiC oxidation protective coating for carbon materials by liquid phase sintering

被引:23
作者
Ren, Xuanru [1 ]
Wang, Lifeng [1 ]
Feng, Peizhong [1 ]
Zhang, Ping [1 ]
Guo, LiTong [1 ]
Li, Ziyu [1 ]
机构
[1] China Univ Min & Technol, Sch Mat Sci & Engn, Xuzhou 221116, Peoples R China
基金
中国国家自然科学基金;
关键词
TaB2; Powders; Costing; Liquid phase sintering; Oxidation protection; Borides; COATED CARBON/CARBON COMPOSITES; C/C COMPOSITES; ABLATION RESISTANCE; MICROSTRUCTURE;
D O I
10.1016/j.ceramint.2018.03.105
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
To control the microstructure and amounts of TaB2 phase in the TaB2-SiC coating, a novel liquid phase sintering method was developed on the basis of in -situ reaction method to prepare the TaB2-SiC coating, which includes synthesis of TaB2 powders and further preparation of TaB2-SiC coating. With Ta2O5, B2O3 and C employed as raw materials, hexagonal TaB2 powders were prepared by carbothermal reduction method at 1500 degrees C, whose mean particle size is 491 nm. The TaB2, SiC, C powders, and the low melting point phases Si and silica sol were used to prepare the TaB2-SiC coating by liquid phase sintering at 2373 K. The thickness of the coating is about 350 gm. Compared with the SiC coating, the weight loss of the samples modified by TaB2 decreased from 17.7% to 11.8%, and the average weight loss rate of the fastest weightloss zone reduced from -6 x 10 (-3) mg cm (-2) s-(1) to -5 x 10(-3) mg cm (-2) s (-1). During oxidation, the Ta-oxides would gradually dissolve in the silicate glass to form Ta-Si-O glass ceramics with dendritic structure, which significantly improved the toughness and stability of the glass layer. The Ta-Si-O glass ceramics possesses the ability of sealing and arresting the microcracks, which can enhance the oxidation protective ability of the coating.
引用
收藏
页码:10708 / 10715
页数:8
相关论文
共 18 条
  • [11] Ablation resistance of HfC coating reinforced by HfC nanowires in cyclic ablation environment
    Ren, Jincui
    Zhang, Yulei
    Zhang, Pengfei
    Li, Tao
    Li, Jinhua
    Yang, Yang
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2017, 37 (08) : 2759 - 2768
  • [12] Ultra-high temperature ceramic TaB2-TaC-SiC coating for oxidation protection of SiC-coated carbon/carbon composites
    Ren, Xuanru
    Li, Hejun
    Fu, Qiangang
    Li, Kezhi
    [J]. CERAMICS INTERNATIONAL, 2014, 40 (07) : 9419 - 9425
  • [13] Preparation of oxidation protective ZrB2-SiC coating by in-situ reaction method on SiC-coated carbon/carbon composites
    Ren, Xuanru
    Li, Hejun
    Chu, Yanhui
    Fu, Qiangang
    Li, Kezhi
    [J]. SURFACE & COATINGS TECHNOLOGY, 2014, 247 : 61 - 67
  • [14] TaB2-SiC-Si multiphase oxidation protective coating for SiC-coated carbon/carbon composites
    Ren, Xuanru
    Li, Hejun
    Fu, Qiangang
    Chu, Yanhui
    Li, Kezhi
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2013, 33 (15-16) : 2953 - 2959
  • [15] Improving oxidation resistance of MoSi2 coating by reinforced with Al2O3 whiskers
    Wang, Lu
    Fu, Qiangang
    Zhao, Fengling
    [J]. INTERMETALLICS, 2018, 94 : 106 - 113
  • [16] ZrB2/SiC as a protective coating for C/SiC composites: Effect of high temperature oxidation on mechanical properties and anti-ablation property
    Xiang Yang
    Li Wei
    Wang Song
    Zhang Bi-feng
    Chen Zhao-hui
    [J]. COMPOSITES PART B-ENGINEERING, 2013, 45 (01) : 1391 - 1396
  • [17] A mullite oxidation protective coating on SiC coated carbon/carbon composites by hot dipping
    Zhang, Bo
    Huang, Jianfeng
    Ouyang, Haibo
    Cao, Liyun
    Li, Cuiyan
    [J]. CERAMICS INTERNATIONAL, 2016, 42 (15) : 17932 - 17935
  • [18] A carbon nanotube-enhanced SiC coating for the oxidation protection of C/C composite materials
    Zheng, Guo-Bin
    Sano, Hideaki
    Uchiyama, Yasuo
    [J]. COMPOSITES PART B-ENGINEERING, 2011, 42 (08) : 2158 - 2162