Effect of hydrofluoric acid concentration and etching time on resin-bond strength to different glass ceramics

被引:36
作者
Verissimo, Aretha Heitor [1 ]
Duarte Moura, Dayanne Monielle [1 ]
Mendes Tribst, Joao Paulo [2 ]
Medeiros de Araujo, Arthur Magno [1 ]
Pereira Leite, Fabiola Pessoa [3 ]
de Assuncao e Souza, Rodrigo Othavio [1 ]
机构
[1] Univ Fed Rio Grande Norte UFRN, Dept Dent, Natal, RN, Brazil
[2] Univ Estadual Paulista Unesp, Inst Sci & Technol, Dept Dent Mat & Prosthodont, Sao Jose Dos Campos, SP, Brazil
[3] Univ Fed Juiz de Fora UFJF, Dept Dent, Juiz De Fora, MG, Brazil
来源
BRAZILIAN ORAL RESEARCH | 2019年 / 33卷
关键词
Ceramics; Acid Etching; Dental; Shear Strength; LITHIUM-DISILICATE; CAD/CAM; PORCELAIN; RESTORATIONS; SURFACE; INTERFACE; CEMENT;
D O I
10.1590/1807-3107bor-2019.vol33.0041
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
The objective of this study was to evaluate the effect of the hydrofluoridric acid (HF) concentration and time of acid conditioning on bond strength of three glass ceramics to a resin cement. Thus, fifty blocks (10 mm x 5 mm x 2 mm) of each ceramic (LDCAD: IPS e.max CAD; LCAD: IPS Empress CAD and LDHP: IPS e.max Press) were made and embedded in acrylic resin. The surfaces were polished with sandpaper (#600, 800, 1000, and 1200 grits) and blocks were randomly divided into 15 groups (n = 10) according to the following factors: Concentration of HF (10% and 5%), conditioning time (20 s and 60 s) and ceramic (LDCAD, LDHP, and L). After conditioning, silane (Prosil / FGM) was applied and after 2 min, cylinders ((O)empty set = 2 mm; h = 2 mm) of dual resin cement (AllCem / FGM) were made in the center of each block using a Teflon strip as matrix and light cured for 40 s (1,200 mW/cm(2)). Then, the samples were thermocycled (10,000 cycles, 5/55 degrees C, 30s) and submitted to the shear bond test (50 KgF, 0.5 mm/min). The data (MPa) were analyzed with 3-way ANOVA and Tukey's test (5%). Failure analysis was performed using a stereomicroscope (20x) and a scanning electron microscope (SEM). ANOVA revealed that the "concentration" factor (p = 0.01) and the interaction "acid concentration X ceramic" (p = 0.009) had a significant effect, however, the "ceramic" (p = 0.897) and "conditioning time" (p = 0.260) factors did not influence the results. The LDHP10%(60s) (10.98 MPa)(aA*) group presented significantly higher bond strength than LDHP10%(20s) (6.57 MPa)(bA), LCAD5%(20s) (6,90 +/- 3,5)(aB) and LDHP5%(60s) (5.66 +/- 2,9MPa)(aA*) groups (Tukey). Failure analysis revealed that 100% of specimens had mixed failure. In conclusion, etching with 5% HF for 20 seconds is recommended for lithium disilicate and leucite-reinforced CAD/CAM ceramics. However, for pressed lithium disilicate ceramic, 10% HF for 60 s showed significantly higher bond strength to resin cement.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] The effect of hydrofluoric acid and resin cement formulation on the bond strength to lithium disilicate ceramic
    Sundfeld, Daniel
    Muniz Palialol, Alan Rodrigo
    Fugolin, Ana Paula Piovesan
    Bovi Ambrosano, Glaucia Maria
    Correr-Sobrinho, Lourenco
    Marcondes Martins, Luis Roberto
    Pfeifer, Carmem Silvia
    BRAZILIAN ORAL RESEARCH, 2018, 32
  • [22] Evaluation of the Microtensile Bond Strength between Resin Composite and Hydrofluoric Acid Etched Ceramic in Different Storage Media
    Ho, Gary W.
    Matinlinna, Jukka P.
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2011, 25 (19) : 2671 - 2685
  • [23] Influence of Hydrofluoric Acid Etching, Resin Bonding and Resin Removal Treatments on the Surface Roughness of Ceramics
    Alhamzah, Najd Burhan
    Alsahil, Njoud Hamad
    Afzal, Irshad
    Naseem, Mustafa
    Alqahtani, Ibrahim M.
    Alruhaymi, Adel A.
    Vohra, Fahim
    BIOSCIENCE BIOTECHNOLOGY RESEARCH COMMUNICATIONS, 2020, 13 (01): : 43 - 47
  • [24] Effect of hydrofluoric acid etching time on flexural and adhesive properties of lithium disilicate
    De Angelis, Francesco
    Vadini, Mirco
    D'Amario, Maurizio
    Buonvivere, Matteo
    D'Arcangelo, Camillo
    DENTAL CADMOS, 2019, 87 (07) : 430 - 439
  • [25] Effect of etching with distinct hydrofluoric acid concentrations on the flexural strength of a lithium disilicate-based glass ceramic
    Prochnow, Catina
    Venturini, Andressa B.
    Grasel, Rafaella
    Bottino, Marco C.
    Valandro, Luiz Felipe
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2017, 105 (04) : 885 - 891
  • [26] Effect of milling, fitting adjustments, and hydrofluoric acid etching on the strength and roughness of CAD-CAM glass-ceramics: A systematic review and meta-analysis
    May, Michele Mirian
    Fraga, Sara
    May, Liliana Gressler
    JOURNAL OF PROSTHETIC DENTISTRY, 2022, 128 (06) : 1190 - 1200
  • [27] Airborne-Particle Abrasion vs. Hydrofluoric Acid Etching of Dental Ceramics: Impact on the Tensile Bond Strength
    Lankes, Valerie
    Coldea, Andrea
    Meinen, John
    Schwendicke, Falk
    Stawarczyk, Bogna
    MATERIALS, 2024, 17 (23)
  • [28] Effect of Ceramic Etching Protocols on Resin Bond Strength to a Feldspar Ceramic
    Bottino, M. A.
    Snellaert, A.
    Bergoli, C. D.
    Oezcan, M.
    Bottino, M. C.
    Valandro, L. F.
    OPERATIVE DENTISTRY, 2015, 40 (02) : E40 - E46
  • [29] Effect of Repressing Lithium Disilicate Glass Ceramics on The Shear Bond Strength of Resin Cements
    Abu Haimed, Tariq S.
    Alzahrani, Saeed J.
    Attar, Esraa A.
    AL-Turki, Lulwa E.
    MATERIALS, 2023, 16 (18)
  • [30] Effect of sandblasting, etching and resin bonding on the flexural strength/bonding of novel glass-ceramics
    Uwalaka, Chinwe O.
    Karpukhina, Natalia
    Cao, Xu
    Bissasu, Sami
    Wilson, Rory M.
    Cattell, Michael J.
    DENTAL MATERIALS, 2018, 34 (10) : 1566 - 1577