Atomic layer deposition of TiO2 and Al2O3 thin films for the electrochemical study of corrosion protection in aluminum alloy cans used in beverage

被引:14
作者
Dias, V. M. [1 ,2 ]
Chiappim, W. [3 ]
Fraga, M. A. [4 ]
Maciel, H. S. [1 ,5 ]
Marciano, F. R. [6 ]
Pessoa, R. S. [1 ,5 ]
机构
[1] Inst Tecnol Aeronaut, Lab Plasmas & Proc, BR-12228900 Sao Jose Dos Campos, SP, Brazil
[2] Univ Vale Paraiba, Lab Nanotecnol & Proc Plasma, BR-12244000 Sao Jose Dos Campos, SP, Brazil
[3] Univ Aveiro, I3N, Dept Fis, Campus Univ Santiago, P-3810193 Aveiro, Portugal
[4] Univ Fed Sao Paulo, Inst Ciencia & Tecnol, BR-12231280 Sao Jose Dos Campos, SP, Brazil
[5] Univ Brasil, Inst Ciencia & Tecnol, BR-08230030 Sao Paulo, SP, Brazil
[6] Univ Fed Piaui, BR-64049550 Teresina, PI, Brazil
基金
巴西圣保罗研究基金会;
关键词
thin films; atomic layer deposition; titanium dioxide; aluminum oxide; electrochemical impedance spectroscopy; CHLORIDE-ION; COATINGS; BEHAVIOR; COPPER; RESISTANCE; GROWTH;
D O I
10.1088/2053-1591/aba557
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Titanium dioxide (TiO2) and aluminum oxide (Al2O3) thin films, with thicknesses around 100 nm, were grown on commercial pure- and resin-coated Al substrates using the atomic layer deposition (ALD). A comprehensive and comparative study of corrosion protection was carried out by linear sweep voltammetry (LSV) and electrochemical impedance spectroscopy (EIS) measurements for a set of six samples: two reference samples (Al-bare and Al-resin), and four ALD coated samples (Al-TiO2, Al-Al2O3, Al-resin-TiO2, and Al-resin-Al2O3). The LSV and EIS results display good mutual agreement, indicating a higher protection efficiency of all ALD-coated samples after immersion in NaCl. When compared to Al-bare, all ALD coated samples (TiO2 or Al2O3) showed a corrosion inhibition enhancement factor of 99%. Besides, our results demonstrated that Al-resin+Al2O3 has 24.95% and 33.40% more corrosion inhibition than Al-Al2O3 and Al-resin, respectively. EIS data were fitted by an equivalent electric circuit (EEC). The Nyquist and Bode plots from the experiments showed that ALD films are a potential candidate for altering/improving commercial resin-coated Al cans.
引用
收藏
页数:13
相关论文
共 70 条
  • [1] Abd EI, 2012, CORROS SCI, V68, P14
  • [2] Al2O3 and TiO2 Atomic Layer Deposition on Copper for Water Corrosion Resistance
    Abdulagatov, A. I.
    Yan, Y.
    Cooper, J. R.
    Zhang, Y.
    Gibbs, Z. M.
    Cavanagh, A. S.
    Yang, R. G.
    Lee, Y. C.
    George, S. M.
    [J]. ACS APPLIED MATERIALS & INTERFACES, 2011, 3 (12) : 4593 - 4601
  • [3] Aguilar J, 2016, KERNEL ADV MATH PHYS, V2016
  • [4] STUDIES ON THE INFLUENCE OF CHLORIDE-ION AND PH ON THE ELECTROCHEMICAL-BEHAVIOR OF ALUMINUM ALLOY-8090 AND ALLOY-2014
    AMBAT, R
    DWARAKADASA, ES
    [J]. JOURNAL OF APPLIED ELECTROCHEMISTRY, 1994, 24 (09) : 911 - 916
  • [5] [Anonymous], 2017, Tribollet Electrochemical Impedance Spectroscopy, DOI DOI 10.1002/9781119363682
  • [6] Surface analysis of Cu coated with ALD Al2O3 and its corrosion protection enhancement in NaCl solution: EIS and polarization
    Bahari, Helma Sadat
    Savaloni, Hadi
    [J]. MATERIALS RESEARCH EXPRESS, 2019, 6 (08)
  • [7] AC-IMPEDANCE MEASUREMENTS ON ALUMINUM BARRIER TYPE OXIDE-FILMS
    BESSONE, J
    MAYER, C
    JUTTNER, K
    LORENZ, WJ
    [J]. ELECTROCHIMICA ACTA, 1983, 28 (02) : 171 - 175
  • [8] THE ANALYSIS OF ELECTRODE IMPEDANCES COMPLICATED BY THE PRESENCE OF A CONSTANT PHASE ELEMENT
    BRUG, GJ
    VANDENEEDEN, ALG
    SLUYTERSREHBACH, M
    SLUYTERS, JH
    [J]. JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 1984, 176 (1-2): : 275 - 295
  • [9] Degradation behaviour of 6013-T6, 2024-T3 alloys and pure aluminium in different aqueous media
    Carbonini, P
    Monetta, T
    Mitton, DB
    Bellucci, F
    Mastronardi, P
    Scatteia, B
    [J]. JOURNAL OF APPLIED ELECTROCHEMISTRY, 1997, 27 (10) : 1135 - 1142
  • [10] Ultra-thin Al2O3 films grown by atomic layer deposition for corrosion protection of copper
    Chai, Zhimin
    Liu, Yuhong
    Li, Jing
    Lu, Xinchun
    He, Dannong
    [J]. RSC ADVANCES, 2014, 4 (92) : 50503 - 50509