Joining of silicon nitride ceramic composites with Y2O3-Al2O3-SiO2 mixtures

被引:0
|
作者
Fei, Z [1 ]
机构
[1] Jiangsu Univ, Sch Mat Sci & Engn, Zhenjiang 212013, Peoples R China
关键词
silicon nitride; bonding; Y2O3-Al2O3-SiO2; joint strength; interface reaction;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hot-pressure sintered silicon nitride ceramic composites were joined to themselves using Y2O3-Al2O3-SiO2 mixtures. Reaction behavior at interface between Si3N4 and Y2O3-Al2O3-SiO2 mixtures during silicon nitride composite joining was studied by means of SEM, EPMA and XRD. The joint strength under different bonding conditions was measured by four-point bending tests. The results of EPMA and XRD analyses show that the liquid glass solders react with silicon nitride at interface, forming the Si3N4/Si2N2O/Y-Si-Al-O-N glass/Y-Si-Al-O glass gradient interface. From the results of four-point bending tests, it is known that with increasing joining temperature and holding time, the joint strength first increased, reaching a peak, and then decreased. The maximum joining strength of 315 MPa measured by the four-point bending test is achieved for the Si3N4 composite-Si3N4 composite joint bonded at 1823 K for 15 min. Destructed part is considered to start at the diffusion layer, indicating that the joining strength will be much higher than that value. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:293 / 297
页数:5
相关论文
共 50 条
  • [1] TiC particle reinforced silicon nitride composite joined with Y2O3-Al2O3-SiO2 mixture
    Zhou, F
    Li, ZZ
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2001, 16 (02): : 13 - +
  • [3] Effect of the fourth element on bonding of silicon nitride ceramics with Y2O3-Al2O3-SiO2 glass solders
    Zhou, F
    JOURNAL OF RARE EARTHS, 2001, 19 (02) : 90 - 96
  • [5] Joining of Cf/SiC composites and Si3N4 ceramic with Y2O3-Al2O3-SiO2 glass filler for high-temperature applications
    Sun, Liangbo
    Shi, Xiaosong
    Liu, Xinyu
    Fang, Jian
    Liu, Chunfeng
    Zhang, Jie
    CERAMICS INTERNATIONAL, 2021, 47 (11) : 15622 - 15630
  • [6] Interfacial reaction and joint strength of silicon nitride ceramic composites bonded with Y2O3-Al2O3-SiO2-Si3N4 mixture
    Zhou, F
    Suh, CM
    Kim, SS
    MATERIALS LETTERS, 2002, 55 (1-2) : 55 - 60
  • [7] Crystallization, thermal expansion and hardness of Y2O3-Al2O3-SiO2 glasses
    Wang, Mitang
    Zheng, Qingshuang
    Chen, Aiying
    Li, Ying
    Zhang, Xiaowei
    Zhang, Dongliang
    Jin, Siqingaowa
    Xiong, Dehua
    Deng, Wei
    CERAMICS INTERNATIONAL, 2021, 47 (17) : 25059 - 25066
  • [8] Liquid-phase bonding of silicon nitride ceramics using Y2O3-Al2O3-SiO2-TiO2 mixtures
    Zhou, F
    Pan, JY
    Chen, KM
    MATERIALS LETTERS, 2004, 58 (7-8) : 1383 - 1386
  • [9] Bonding of silicon nitride ceramic composite with RE2O3-Al2O3-SiO2 glass solders
    Zhou, F
    Li, ZZ
    Luo, QF
    JOURNAL OF RARE EARTHS, 1999, 17 (03) : 194 - 199
  • [10] Bonding of Silicon Nitride Ceramic Composite with RE2O3Al2O3SiO2 Glass Solders
    周飞
    李志章
    罗启富
    JournalofRareEarths, 1999, (03) : 194 - 199