Effect of preparation temperature on the formation of Sr2CeO4 phosphor particles in the spray pyrolysis

被引:3
|
作者
Hong, Seung Kwon [1 ]
Jung, Dae Soo [1 ]
Lee, Hyo Jin [1 ]
Kang, Yun Chan [1 ]
机构
[1] Konkuk Univ, Dept Chem Engn, Seoul 143701, South Korea
关键词
phosphor; spray pyrolysis; ceramic;
D O I
10.1007/BF02706755
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Sr2CeO4 phosphor particles were prepared by spray pyrolysis at various preparation temperatures. The effect of preparation temperatures on the morphology, crystal structure and photoluminescence characteristics of the post-treated Sr2CeO4 phosphor particles was studied. Phase pure Sr2CeO4 phosphor particles were not produced by spray pyrolysis without post-treatment. The optimum post-treatment temperature to produce the Sr2CeO4 phosphor particles with high photoluminescence intensity was 1,000 degrees C in spray pyrolysis. The spherical morphology of the as-prepared particles obtained at high preparation temperatures above 1,400 degrees C had maintained after post-treatment at 1,000 degrees C. The relative photoluminescence intensities of the Sr2CeO4 phosphor particles varied with the preparation temperatures in the spray pyrolysis. The as-prepared particles obtained by spray pyrolysis at preparation temperatures below 1,400 degrees C converted into phase pure Sr2CeO4 phosphor particles after post-treatment at 1,000 degrees C. The optimum preparation temperature of the as-prepared particles was 1,400 degrees C to produce the Sr2CeO4 phosphor particles with spherical shape and high photoluminescence intensity in the spray pyrolysis.
引用
收藏
页码:496 / 498
页数:3
相关论文
共 50 条
  • [1] Effect of preparation temperature on the formation of Sr2CeO4 phosphor particles in the spray pyrolysis
    Seung Kwon Hong
    Dae Soo Jung
    Hyo Jin Lee
    Yun Chan Kang
    Korean Journal of Chemical Engineering, 2006, 23 : 496 - 498
  • [2] Preparation of Sr2CeO4 blue phosphor by ultrasonic spray pyrolysis: effect of NH4NO3 addition
    Myung-Jin Kang
    Se-Young Choi
    Journal of Materials Science, 2002, 37 : 2721 - 2729
  • [3] Fine size Sr2CeO4 phosphor particles prepared by spray pyrolysis from polymeric precursor solution
    Hong, SK
    Ju, SH
    Koo, HY
    Jung, DS
    Kang, YC
    MATERIALS LETTERS, 2006, 60 (03) : 334 - 338
  • [4] Preparation and characterization of fine Sr2CeO4 blue phosphor powders
    Chen, SJ
    Chen, XT
    Yu, Z
    Hong, JM
    Xue, ZL
    You, XZ
    SOLID STATE COMMUNICATIONS, 2004, 130 (3-4) : 281 - 285
  • [5] Synthesis and characterization of spherical Sr2CeO4 phosphors by spray pyrolysis for field emission displays
    Liu, XM
    Luo, Y
    Lin, J
    JOURNAL OF CRYSTAL GROWTH, 2006, 290 (01) : 266 - 271
  • [6] Hydrothermal combustion synthesis and characterization of Sr2CeO4 phosphor powders
    Yang, Yanfei
    Zuo, Xiangyu
    Shi, Shikao
    Li, Jibiao
    Wang, Jiye
    Geng, Lina
    Fu, Lianshe
    MATERIALS RESEARCH BULLETIN, 2019, 112 : 159 - 164
  • [7] A new synthetic pathway of Sr2CeO4 phosphor and its characterization
    Seema, R.
    Nandakumar, K.
    JOURNAL OF LUMINESCENCE, 2011, 131 (10) : 2181 - 2184
  • [8] Characteristics of Sr2CeO4 powder phosphor prepared by combustion route
    Shi, SK
    Wang, JY
    Li, JM
    Zong, RL
    Zhou, J
    HIGH-PERFORMANCE CERAMICS III, PTS 1 AND 2, 2005, 280-283 : 639 - 641
  • [9] Effect of preparation temperature on the characteristics of Eu-doped borate phosphor particles in the spray pyrolysis
    Koo, Hye Young
    Jung, Dae Soo
    Ju, Seo Hee
    Hong, Seung Kwon
    Kang, Yun Chan
    MATERIALS LETTERS, 2006, 60 (25-26) : 3091 - 3095
  • [10] Synthesis of Sr2CeO4 blue phosphor by solid-state reaction
    Huang Jian-feng
    Cao Li-yun
    Wu Jian-peng
    He Hai-yan
    Zhang Guo-yun
    SILICATES INDUSTRIELS, 2006, 71 (9-10): : 155 - 159