Improving the oxidation resistance of Ti3SiC2 by forming a Ti3Si0.9Al0.1C2 solid solution

被引:116
作者
Zhang, HB [1 ]
Zhou, YC [1 ]
Bao, YW [1 ]
Li, MS [1 ]
机构
[1] Chinese Acad Sci, Shenyang Natl Lab Mat Sci, Inst Met Res, Shenyang 110016, Peoples R China
关键词
ceramics; oxidation; layered structures; activity; solid solution;
D O I
10.1016/j.actamat.2004.04.015
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The oxidation behavior of the Ti3Si0.9Al0.1C2 solid solution in air was investigated at 1000-1350 degreesC. The parabolic rate constants of Ti3Si0.9Al0.1C2 were decreased by 2-4 orders of magnitude compared with those of Ti3SiC2 at 1000-1300 degreesC. At 1000-1100 degreesC, the oxide scales displayed a continuous alpha-Al-2-O-3 inner layer and a discontinuous TiO2 (rutile) outer layer. At 1200-1300 degreesC, the continuous inner layer was still alpha-Al2O3, but the outer layer was a mixture of TiO2 (rutile) and Al2TiO5. The oxide layers were dense, adherent and resistant to thermal cycling. However, the oxidation resistance of Ti3Si0.9Al0.1C2 deteriorated at 1350 degreesC because of the depletion of alpha-Al2O3. This depletion was caused by the extensive reaction between TiO2 (rutile) and alpha-Al2O3 to form Al2TiO5. The high activity and diffusion of Al and the low solubility of oxygen in the solid solution were the key factors for the formation of a continuous alpha-Al2O3 layer during high-temperature oxidation. (C) 2004 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:3631 / 3637
页数:7
相关论文
共 28 条
[1]   IDENTIFICATION OF OXIDATION MECHANISMS IN SILICON-NITRIDE CERAMICS BY TRANSMISSION ELECTRON-MICROSCOPY STUDIES OF OXIDE SCALES [J].
BACKHAUSRICOULT, M ;
GOGOTSI, YG .
JOURNAL OF MATERIALS RESEARCH, 1995, 10 (09) :2306-2321
[2]   Oxidation of Ti3SiC2 in air [J].
Barsoum, MW ;
ElRaghy, T ;
Ogbuji, LUJT .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1997, 144 (07) :2508-2516
[3]   Synthesis and characterization of a remarkable ceramic: Ti3SiC2 [J].
Barsoum, MW ;
ElRaghy, T .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1996, 79 (07) :1953-1956
[4]   OXIDATION BEHAVIOR OF ELECTROCONDUCTIVE SI3N4-TIN COMPOSITES [J].
BELLOSI, A ;
TAMPIERI, A ;
LIU, YZ .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1990, 127 (01) :115-122
[5]   SUSTAINED POTENTIATION OF NMDA RECEPTOR MEDIATED GLUTAMATE RESPONSES THROUGH ACTIVATION OF PROTEIN-KINASE-C BY A MU-OPIOID [J].
CHEN, L ;
HUANG, LYM .
NEURON, 1991, 7 (02) :319-326
[6]   Diffusion kinetics of the carburization and silicidation of Ti3SiC2 [J].
El-Raghy, T ;
Barsoum, MW .
JOURNAL OF APPLIED PHYSICS, 1998, 83 (01) :112-119
[7]   PARTICULATE SILICON NITRIDE-BASED COMPOSITES [J].
GOGOTSI, YG .
JOURNAL OF MATERIALS SCIENCE, 1994, 29 (10) :2541-2556
[8]   OXIDATION BEHAVIOR OF MONOLITHIC TIN AND TIN DISPERSED IN CERAMIC MATRICES [J].
GOGOTSI, YG ;
PORZ, F ;
DRANSFIELD, G .
OXIDATION OF METALS, 1993, 39 (1-2) :69-91
[9]   THE OXIDATION OF PARTICULATE-REINFORCED SI3N4-TIN COMPOSITES [J].
GOGOTSI, YG ;
PORZ, F .
CORROSION SCIENCE, 1992, 33 (04) :627-640
[10]   Effects of testing temperature and thermal treatments on some mechanical properties of a Si3N4-TiN composite [J].
Guicciardi, S ;
Melandri, C ;
Medri, V ;
Bellosi, A .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 360 (1-2) :35-45