Effects of ambient-temperature curing agents on the thermal stability of poly(methylphenylsiloxane)

被引:71
作者
Sun, JT [1 ]
Huang, YD [1 ]
Cao, HL [1 ]
Gong, GF [1 ]
机构
[1] Harbin Inst Technol, Fac Sci, Dept Appl Chem, Harbin 150001, Peoples R China
关键词
polymethylphenylsiloxane; polysilazane; triethanolamine; thermal stability; tbermogravimetric analysis;
D O I
10.1016/j.polymdegradstab.2004.03.018
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Two kinds of curing agents, triethanolamine and polysilazane (KH-CL), were used to make polymethylphenylsiloxne (PMPS) cured at room temperature. Their effects on the short-term and long-term thermal stability of PMPS are reported and discussed. The influences of the curing agents on the thermal degradation mechanisms of PMPS were studied by thermogravimetric analysis (TG), differential thermogravimetry (DTG) and Fourier-transform infrared spectroscopy (FTIR). The results indicate that both kinds of PMPS had higher short-term thermal stability than traditional heat-cured PMPS. For long-term thermal stability, the PMPS cured with KH-CL was much higher than the one cured with triethanolamine. The "unzip degradation" of PMPS was eliminated through the reaction between KH-CL and silanol groups, and then the thermal stability of PMPS was improved. However, it was initiated at a low temperature (about 300 degreesC) with catalysis by triethanolamine, and the thermal stability was decreased. (C) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:725 / 731
页数:7
相关论文
共 26 条
[1]  
BALISHAH G, 1998, J APPL POLYM SCI, V70, P2235
[2]   Polydimethylsiloxane thermal degradation - Part 1. Kinetic aspects [J].
Camino, G ;
Lomakin, SM ;
Lazzari, M .
POLYMER, 2001, 42 (06) :2395-2402
[3]   Characterisation and oxidative degradation of a room-temperature vulcanised poly(dimethylsiloxane) rubber [J].
Chaudhry, AN ;
Billingham, NC .
POLYMER DEGRADATION AND STABILITY, 2001, 73 (03) :505-510
[4]   Kinetic aspects of the thermal degradation of poly(dimethyl siloxane) and poly(dimethyl diphenyl siloxane) [J].
Deshpande, G ;
Rezac, ME .
POLYMER DEGRADATION AND STABILITY, 2002, 76 (01) :17-24
[5]   The effect of phenyl content on the degradation of poly(dimethyl diphenyl) siloxane copolymers [J].
Deshpande, G ;
Rezac, ME .
POLYMER DEGRADATION AND STABILITY, 2001, 74 (02) :363-370
[6]  
DOUCETTE J J J, 1999, Three dimensionally reinforced ablative/insulative composite, Patent No. 5985405
[7]   THERMAL-DEGRADATION OF POLYSILOXANES .2. POLY(METHYLPHENYLSILOXANE) [J].
GRASSIE, N ;
MACFARLANE, IG ;
FRANCEY, KF .
EUROPEAN POLYMER JOURNAL, 1979, 15 (05) :415-422
[8]   Influence of Ti-based fillers on the thermal decomposition and phase development of polysiloxane derived materials [J].
Hönack, F ;
Riedel, R .
ADVANCED ENGINEERING MATERIALS, 2003, 5 (03) :122-125
[9]   The thermogravimetric analysis of some polysiloxanes [J].
Jovanovic, JD ;
Govedarica, MN ;
Dvornic, PR ;
Popovic, IG .
POLYMER DEGRADATION AND STABILITY, 1998, 61 (01) :87-93
[10]  
Keijman K, 1997, OIL GAS-EUR MAG, V23, P38