Effects of Agitation and Morphology of Primary Crystalline Phase on Crystallization Behavior of CaO-SiO2-CaF2 Supercooled Melts

被引:13
作者
Harada, Yusuke [1 ]
Kusada, Kakeru [2 ]
Sukenaga, Sohei [3 ]
Yamamura, Hideaki [4 ]
Ueshima, Yoshiyuki [4 ]
Mizoguchi, Toshiaki [4 ]
Saito, Noritaka [1 ]
Nakashima, Kunihiko [1 ]
机构
[1] Kyushu Univ, Dept Mat Sci & Engn, Nishi Ku, Fukuoka 8190395, Japan
[2] Japan Steel Works Ltd, Hiroshima Reserch Lab, Res & Dev, Aki Ku, Hiroshima 7368602, Japan
[3] Tohoku Univ, Inst Multidisciplinary Res Adv Mat, Aoba Ku, Sendai, Miyagi 9808577, Japan
[4] Nippon Steel & Sumitomo Met Corp, Tech Res & Dev Bur, Chiba 2938511, Japan
关键词
primary crystallization; electrical capacitance; morphology; agitation; oxyfluoride; THERMAL-CONDUCTIVITY; SURFACE-TENSION; HEAT-TRANSFER; MOLD FLUXES; DENSITY; SLAG; STEEL; VISCOSITY; WETTABILITY; CAPACITANCE;
D O I
10.2355/isijinternational.54.2071
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The effects of the agitation field and the crystal morphology on the primary and secondary crystallization temperatures of CaO-SiO2-CaF2 supercooled melts were systematically investigated by measuring the electrical capacitance. Two-stage decreases in electrical capacitance were observed for most samples investigated. These stages correspond to the primary crystallization and the eutectic reaction resulting from the compositional change in the supercooled melts associated with the primary crystallization, respectively. The primary crystallization of dendritic CaO center dot SiO2 was affected by the agitation in the same manner as reported previously, but the crystallization of faceted 3CaO center dot 2SiO(2)center dot CaF2 revealed little dependence on the agitation. This indicates that the effects of the agitation are different for different morphologies of the primary crystalline phase because of shifts in the rate-determining step of crystallization.
引用
收藏
页码:2071 / 2076
页数:6
相关论文
共 34 条
  • [1] The Effect of CaF2 in the Slag in Ladle Refining
    Andersson, Emma
    Sichen, Du
    [J]. STEEL RESEARCH INTERNATIONAL, 2009, 80 (08) : 544 - 551
  • [2] Asanishi M., 2007, AES ATEMA INT C SER, P195
  • [3] ASKARI M, 1991, CAN METALL QUART, V30, P207
  • [4] Effect of alumina on slag-metal separation during iron nugget formation from high alumina Indian iron ore fines
    Borra, C. R.
    Dwarapudi, S.
    Kapure, G.
    Tathavadkar, V.
    Denys, M. B.
    [J]. IRONMAKING & STEELMAKING, 2013, 40 (06) : 443 - 451
  • [5] CHANG HY, 1987, T IRON STEEL I JPN, V27, P797
  • [6] Wetting of solid Al2O3 with molten CaO-Al2O3-SiO2
    Choi, JY
    Lee, HG
    [J]. ISIJ INTERNATIONAL, 2003, 43 (09) : 1348 - 1355
  • [7] VISCOSITY, DENSITY, AND ELECTRICAL RESISTIVITY OF MOLTEN ALKALINE-EARTH BORATE GLASSES WITH 3 MOLE PERCENT OF POTASSIUM OXIDE
    COUGHANOUR, LW
    SHARTSIS, L
    SHERMER, HF
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1958, 41 (08) : 324 - 329
  • [8] VISCOSITY AND DENSITY OF BAO/B2O3/BAF2 FLUXES AND SOLUTIONS
    ELWELL, D
    CAPPER, P
    LAWRENCE, CM
    [J]. JOURNAL OF CRYSTAL GROWTH, 1974, 24 (OCT) : 651 - 655
  • [9] HARA S, 1981, CAN METALL QUART, V20, P113
  • [10] Hayashi M, 2001, PHYS CHEM GLASSES, V42, P6