Cytotoxicity of Soft Denture Lining Materials Depending on Their Component Types

被引:7
|
作者
Song, Yo-Han [1 ,2 ]
Song, Ho-Jun [1 ,2 ]
Han, Mi-Kyung [1 ,2 ]
Yang, Hong-So [3 ]
Park, Yeong-Joon [1 ,2 ]
机构
[1] Chonnam Natl Univ, Sch Dent, Dept Dent Mat, Kwangju 500757, South Korea
[2] Chonnam Natl Univ, Sch Dent, Res Ctr Biomineralizat Disorders, Kwangju 500757, South Korea
[3] Chonnam Natl Univ, Sch Dent, Dept Prosthodont, Kwangju 500757, South Korea
基金
新加坡国家研究基金会;
关键词
IN-VITRO; PHTHALATE; PLASTICIZERS; CHEMICALS; CELLS; HARD;
D O I
10.11607/ijp.3848
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: To evaluate the difference in cytotoxicity of soft denture lining materials depending on their component types. Materials and Methods: Ten commercially available soft denture lining materials (SDLM) consisting of five silicone-based materials and five acrylic-based materials were evaluated. For the MTT test, cured SDLM samples were extracted in a culture medium for 24 hours, and L-929 cells were incubated in the extracted medium for 24 hours. Cell viability was determined using a microplate reader and compared with those of the negative control, which were cultured in a culture medium without test material. Agar overlay test was performed for the cured SDLM samples according to International Organization for Standardization (ISO) 7405. Results: Among silicone-based lining materials, GC Reline Soft, Mollosil plus, and Dentusil showed a cell viability of 107.2% +/- 4.5%, 102.3% +/- 2.84%, and 93.0% +/- 8.0%, respectively, compared with the control. Mucopren and Sofreliner Tough displayed significantly lower cell viability (86.4% +/- 10.3% and 81.5% +/- 4.3%, respectively) compared with the control (P < .05). Among acrylic-based materials, Kooliner, Visco-gel, Soft liner, Dura Base, and Coe-Soft displayed cell viability of 99.2% +/- 14.6%, 93.1% +/- 9.5%, 89.1% +/- 9.8%, 87.6% +/- 7.9%, and 75.9% +/- 15.7%, respectively, compared with the control. Dura Base and Coe-Soft displayed significantly lower cell viability compared to the control. However, for all tested materials, cell viability exceeded the requirement limit of 70% specified in ISO 10993-5. In the agar overlay test, all five silicone-based materials and acrylic-based Kooliner were ranked as "noncytotoxic." However, Visco-gel was ranked as "mildly cytotoxic," and Soft liner, Coe-Soft, and Dura Base were ranked as "moderately cytotoxic." Conclusion: When an acrylic-based soft denture lining material is used, the possibility of a cytotoxic effect should be considered.
引用
收藏
页码:229 / 235
页数:7
相关论文
共 50 条
  • [1] Cytotoxicity of hard and soft denture lining materials
    Atay, Ayse
    Cetintas, Vildan Bozok
    Cal, Ebru
    Kosova, Buket
    Kesercioglu, Atilla
    Guneri, Pelin
    DENTAL MATERIALS JOURNAL, 2012, 31 (06) : 1082 - 1086
  • [2] Effect of aging on tear strength and cytotoxicity of soft denture lining materials; in vitro
    Landayan, Jordi Izzard Andaya
    Manaloto, Adrian Carlos Francisco
    Lee, Jeong-Yol
    Shin, Sang-Wan
    JOURNAL OF ADVANCED PROSTHODONTICS, 2014, 6 (02): : 115 - 120
  • [3] Effect of artificial saliva with different pH levels on the cytotoxicity of soft denture lining materials
    Akay, Canan
    Tanis, Merve C.
    Sevim, Handan
    INTERNATIONAL JOURNAL OF ARTIFICIAL ORGANS, 2017, 40 (10): : 581 - 588
  • [4] Effect of artificial saliva with different ph levels on the cytotoxicity of soft denture lining materials
    Akay, Canan (cnngcr2@hotmail.com), 1600, Wichtig Publishing Srl (40):
  • [5] EFFECTS OF DENTURE CLEANSERS ON DIRECT SOFT DENTURE LINING MATERIALS
    NIKAWA, H
    IWANAGA, H
    HAMADA, T
    YUHTA, S
    JOURNAL OF PROSTHETIC DENTISTRY, 1994, 72 (06): : 657 - 662
  • [6] DENTURE SOFT LINING MATERIALS - CLINICAL INDICATIONS
    MACK, PJ
    AUSTRALIAN DENTAL JOURNAL, 1989, 34 (05) : 454 - 458
  • [7] RHEOLOGY AND STRENGTH OF DENTURE SOFT LINING MATERIALS
    JONES, DW
    SUTOW, EJ
    GRAHAM, BS
    OPIE, GK
    BRIAND, ML
    JOURNAL OF DENTAL RESEARCH, 1983, 62 : 661 - 661
  • [8] WETTABILITY OF DENTURE SOFT-LINING MATERIALS
    WATERS, MGJ
    JAGGER, RG
    JEROLIMOV, V
    WILLIAMS, KR
    JOURNAL OF PROSTHETIC DENTISTRY, 1995, 74 (06): : 644 - 646
  • [9] MYCOTIC GROWTH AND SOFT DENTURE LINING MATERIALS
    MAKILA, E
    HOPSUHAVU, V
    ACTA ODONTOLOGICA SCANDINAVICA, 1977, 35 (04) : 197 - 205
  • [10] THE COMPATIBILITY OF SOFT LINING MATERIALS AND DENTURE CLEANSERS
    DAVENPORT, JC
    WILSON, HJ
    SPENCE, D
    BRITISH DENTAL JOURNAL, 1986, 161 (01) : 13 - 17