共 13 条
[1]
TRANSVERSE MICROSTRUCTURE OF AN OXIDE SCALE FORMED ON A 20-PERCENT-CR-25-PERCENT-NI-NIOBIUM STABILIZED STAINLESS-STEEL
[J].
PROCEEDINGS OF THE ROYAL SOCIETY OF LONDON SERIES A-MATHEMATICAL PHYSICAL AND ENGINEERING SCIENCES,
1987, 412 (1842)
:223-&
[2]
CLAY BD, 1982, MECH BEHAV NUCL APPL, P122
[3]
EVANS HE, 1995, INT MATER REV, V40, P1, DOI 10.1179/095066095790151124
[4]
GAROFALO F, 1963, JOINT INT C CREEP, P1
[5]
EVALUATION OF STRESSES IN NI-NIO AND CR-CR2O3 DURING HIGH-TEMPERATURE OXIDATION BY IN-SITU X-RAY-DIFFRACTION
[J].
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING,
1994, 177 (1-2)
:115-124
[8]
NODEN JD, 1968, BR CORROS J, V3, P47
[9]
ROLE OF OXIDE MICROSTRUCTURE AND GROWTH STRESSES IN HIGH-TEMPERATURE SCALING OF NICKEL
[J].
METALLURGICAL TRANSACTIONS,
1970, 1 (06)
:1701-&