Highly durable, coking and sulfur tolerant, fuel-flexible protonic ceramic fuel cells

被引:652
作者
Duan, Chuancheng [1 ]
Kee, Robert J. [1 ]
Zhu, Huayang [1 ]
Karakaya, Canan [1 ]
Chen, Yachao [1 ]
Ricote, Sandrine [1 ]
Jarry, Angelique [2 ]
Crumlin, Ethan J. [3 ]
Hook, David [4 ]
Braun, Robert [1 ]
Sullivan, Neal P. [1 ]
O'Hayre, Ryan [1 ]
机构
[1] Colorado Sch Mines, Golden, CO 80401 USA
[2] Univ Maryland, Dept Mat Sci & Engn, College Pk, MD 20742 USA
[3] Lawrence Berkeley Natl Lab, Adv Light Source, Berkeley, CA USA
[4] CoorsTek, Golden, CO USA
关键词
GAS SHIFT REACTION; NI-YSZ ANODE; IN-SITU; ELECTROCHEMICAL PERFORMANCE; CARBON DEPOSITION; OXIDE; PEROVSKITE; CATALYST; HYDROGEN; METHANE;
D O I
10.1038/s41586-018-0082-6
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
Protonic ceramic fuel cells, like their higher-temperature solid-oxide fuel cell counterparts, can directly use both hydrogen and hydrocarbon fuels to produce electricity at potentially more than 50 per cent efficiency(1,2). Most previous direct-hydrocarbon fuel cell research has focused on solid-oxide fuel cells based on oxygen-ion-conducting electrolytes, but carbon deposition (coking) and sulfur poisoning typically occur when such fuel cells are directly operated on hydrocarbon-and/or sulfur-containing fuels, resulting in severe performance degradation over time(3-6). Despite studies suggesting good performance and anti-coking resistance in hydrocarbon-fuelled protonic ceramic fuel cells(2,7,8), there have been no systematic studies of long-term durability. Here we present results from long-term testing of protonic ceramic fuel cells using a total of 11 different fuels (hydrogen, methane, domestic natural gas (with and without hydrogen sulfide), propane, n-butane, i-butane, iso-octane, methanol, ethanol and ammonia) at temperatures between 500 and 600 degrees Celsius. Several cells have been tested for over 6,000 hours, and we demonstrate excellent performance and exceptional durability (less than 1.5 per cent degradation per 1,000 hours in most cases) across all fuels without any modifications in the cell composition or architecture. Large fluctuations in temperature are tolerated, and coking is not observed even after thousands of hours of continuous operation. Finally, sulfur, a notorious poison for both low-temperature and high-temperature fuel cells, does not seem to affect the performance of protonic ceramic fuel cells when supplied at levels consistent with commercial fuels. The fuel flexibility and long-term durability demonstrated by the protonic ceramic fuel cell devices highlight the promise of this technology and its potential for commercial application.
引用
收藏
页码:217 / +
页数:19
相关论文
共 52 条
[1]  
Albrecht K. J., 2015, ECS Transactions, V68, P3165, DOI 10.1149/06801.3165ecst
[2]   Advanced anodes for high-temperature fuel cells [J].
Atkinson, A ;
Barnett, S ;
Gorte, RJ ;
Irvine, JTS ;
Mcevoy, AJ ;
Mogensen, M ;
Singhal, SC ;
Vohs, J .
NATURE MATERIALS, 2004, 3 (01) :17-27
[3]   Hybrid HF-DFT modeling of monolayer water adsorption on (001) surface of cubic BaHfO3 and BaZrO3 crystals [J].
Bandura, A. V. ;
Evarestov, R. A. ;
Kuruch, D. D. .
SURFACE SCIENCE, 2010, 604 (19-20) :1591-1597
[4]   Mechanisms of catalyst deactivation [J].
Bartholomew, CH .
APPLIED CATALYSIS A-GENERAL, 2001, 212 (1-2) :17-60
[5]   Raman spectroscopic monitoring of carbon deposition on hydrocarbon-fed solid oxide fuel cell anodes [J].
Blinn, Kevin S. ;
Abernathy, Harry ;
Li, Xiaxi ;
Liu, Mingfei ;
Bottomley, Lawrence A. ;
Liu, Meilin .
ENERGY & ENVIRONMENTAL SCIENCE, 2012, 5 (07) :7913-7917
[6]  
Borglum B., 2015, ECS Transactions, V68, P89, DOI 10.1149/06801.0089ecst
[7]   DFT Study of the Water-Gas Shift Reaction and Coke Formation on Ni(111) and Ni(211) Surfaces [J].
Catapan, Rafael C. ;
Oliveira, Amir A. M. ;
Chen, Ying ;
Vlachos, Dionisios G. .
JOURNAL OF PHYSICAL CHEMISTRY C, 2012, 116 (38) :20281-20291
[8]   Direct-methane solid oxide fuel cells with hierarchically porous Ni-based anode deposited with nanocatalyst layer [J].
Chen, Yu ;
Zhang, Yanxiang ;
Lin, Ye ;
Yang, Zhibin ;
Su, Dong ;
Han, Minfang ;
Chen, Fanglin .
NANO ENERGY, 2014, 10 :1-9
[9]   A robust symmetrical electrode with layered perovskite structure for direct hydrocarbon solid oxide fuel cells: PrBa0.8Ca0.2Mn2O5+δ [J].
Choi, S. ;
Sengodan, S. ;
Park, S. ;
Ju, Y-W. ;
Kim, J. ;
Hyodo, J. ;
Jeong, H. Y. ;
Ishihara, T. ;
Shin, J. ;
Kim, G. .
JOURNAL OF MATERIALS CHEMISTRY A, 2016, 4 (05) :1747-1753
[10]   Surface strontium enrichment on highly active perovskites for oxygen electrocatalysis in solid oxide fuel cells [J].
Crumlin, Ethan J. ;
Mutoro, Eva ;
Liu, Zhi ;
Grass, Michael E. ;
Biegalski, Michael D. ;
Lee, Yueh-Lin ;
Morgan, Dane ;
Christen, Hans M. ;
Bluhm, Hendrik ;
Shao-Horn, Yang .
ENERGY & ENVIRONMENTAL SCIENCE, 2012, 5 (03) :6081-6088