Limiting Retained Austenite Decomposition in Quenched and Tempered Steels: Influences of Rapid Tempering and Silicon

被引:20
作者
Euser, Virginia Katherine [1 ,2 ]
Williamson, Don Lee [1 ]
Clarke, Amy Jean [1 ]
Speer, John Gordon [1 ]
机构
[1] Colorado Sch Mines, 1500 Illinois St, Golden, CO 80401 USA
[2] Los Alamos Natl Lab, POB 1663, Los Alamos, NM 87545 USA
关键词
martensite; tempering; retained austenite; cementite; silicon; rapid processing; IRON-CARBON MARTENSITE; X-RAY-DIFFRACTION; THERMAL-STABILITY; CEMENTITE PRECIPITATION; ATOM-PROBE; TENSILE BEHAVIOR; SELF-DIFFUSION; EMBRITTLEMENT; MOSSBAUER; STRENGTH;
D O I
10.2355/isijinternational.ISIJINT-2020-263
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Tempering reactions are critical to microstructure and property control in martensitic steels. Here, retained austenite decomposition and cementite precipitation are monitored using Mossbauer spectroscopy in 4340 and 300-M steel under conventional and rapid tempering conditions. Tempering times are compared at a constant tempered hardness by increasing tempering temperatures associated with short time conditions to achieve equivalent matrix softening to that of longer tempering times. Time-temperature combinations that provide equivalent tempered hardness generated microstructures with similar dislocation densities and cementite precipitation fractions; these mechanisms are controlled by self-diffusion. However, systematic differences in retained austenite content were observed at a given degree of softening, where shorter tempering times exhibited higher levels of retained austenite compared to more conventional conditions. At low temperatures, the differences in retained austenite preservation between explored time-temperature conditions are attributed to corresponding differences in carbon diffusion distance (in austenite), the controlling diffusional process of retained austenite decomposition. At higher temperatures, retained austenite decomposition exhibits C-curve kinetic behavior in 4340. Thus, reduced thermodynamic driving force for cementite and ferrite formation at higher temperature is believed to play a role in restricting retained austenite decomposition within some short-time, high temperature tempering regimes. The addition of silicon pushes cementite precipitation and retained austenite decomposition to higher temperatures, although retained austenite decomposition is suppressed to a greater extent than cementite precipitation. Potential is illustrated for coupling rapid tempering with silicon alloying to produce appreciably tempered martensite (similar to 490 HV) with relatively less retained austenite decomposition compared to conventional tempering conditions.
引用
收藏
页码:2990 / 3000
页数:11
相关论文
共 82 条
[1]  
ANDREWS KW, 1965, J IRON STEEL I, V203, P721
[2]  
ANGERS R, 1968, CAN METALL QUART, V7, P73
[3]  
[Anonymous], 2013, ASTM International E975-13, DOI DOI 10.1520/E0975-13
[4]  
Antia D. P., 1944, Trans. Am. Soc. Met., V32, P290
[5]   Retained austenite thermal stability in a nanostructured bainitic steel [J].
Avishan, Behzad ;
Garcia-Mateo, Carlos ;
Yazdani, Sasan ;
Caballero, Francisca G. .
MATERIALS CHARACTERIZATION, 2013, 81 :105-110
[6]   ATOM-PROBE FIELD-ION MICROSCOPY STUDY OF THE PARTITIONING OF SUBSTITUTIONAL ELEMENTS DURING TEMPERING OF A LOW-ALLOY STEEL MARTENSITE [J].
BABU, SS ;
HONO, K ;
SAKURAI, T .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1994, 25 (03) :499-508
[7]   APFIM STUDIES ON MARTENSITE TEMPERING OF FE-C-SI-MN LOW-ALLOY STEEL [J].
BABU, SS ;
HONO, K ;
SAKURAI, T .
APPLIED SURFACE SCIENCE, 1993, 67 (1-4) :321-327
[8]   EFFECT OF 1ST AND 2ND STAGES OF TEMPERING ON MICROCRACKING IN MARTENSITE OF AN FE 1.22 C-ALLOY [J].
BALLIETT, TA ;
KRAUSS, G .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1976, 7 (01) :81-86
[9]  
Balluffi RW, 2005, KINETICS OF MATERIALS, P533
[10]  
Bhadeshia H. K. D. H., 1979, Metal Science, V13, P325