Effect of Tin on Hot Ductility and High-temperature Oxidation Behavior of 20CrMnTi Steel

被引:18
作者
Peng Hong-bing [1 ]
Chen Wei-qing [1 ]
Chen Lie [2 ]
Guo Dong [2 ]
机构
[1] Univ Sci & Technol Beijing, State Key Lab Adv Met, Beijing 100083, Peoples R China
[2] Xining Special Steel Co Ltd, Xining 810005, Peoples R China
关键词
tin; 20CrMnTi steel; hot ductility; high-temperature oxidation behavior; CARBON-MANGANESE; SHORTNESS; SN; EMBRITTLEMENT; COPPER; CU;
D O I
10.1515/htmp-2013-0028
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The hot ductility and high-temperature oxidation behavior of 20CrMnTi steel with 0.02% Cu and x% Sn (0.004 <= x <= 0.049) were investigated. The results show that tin has no significant effect on tensile strength of sample with less than 0.049% Sn. The critical temperature where the hot ductility reduces dramatically rises with the increase of tin content while the hot ductility decreases with its increase. The average tin content at austenite grain boundaries (GB) and substrate is 0.108% and 0.045% respectively in the specimen containing 0.049% tin quenched after heated to 1223 K and held for 600 s. Sn-segregation at the GB deteriorates the hot ductility. There is no direct relationship between the cause of the ductility trough and tin. However, Sn-segregation at the GB causes it to deepen a lot. The tin content should be controlled below 0.021%, which would not deteriorate the hot ductility significantly. There is no tin-enrichment at the scale/substrate interface when tin content is less than 0.049%. Moreover, although Sn is enriched under the steel surface, any liquid Sn-enrichment wasn't observed at the oxide/steel interface even in as high as 0.45% Sn-bearing steel with 0.02% Cu.
引用
收藏
页码:179 / 185
页数:7
相关论文
共 50 条
[31]   Effect of Austenitization Temperature on Hot Ductility of C-Mn-Al HSLA Steel [J].
Prislupcak, Peter ;
Kvackaj, Tibor ;
Bidulska, Jana ;
Zahumensky, Pavol ;
Homolova, Viera ;
Juhar, Lubos ;
Zubko, Pavol ;
Zimovcak, Peter ;
Gburik, Roman ;
Demjan, Ivo .
MATERIALS, 2022, 15 (03)
[32]   Unveiling the influence of TiN on the microstructure and high-temperature oxidation behavior of Ti-Al-Cr composite coating [J].
Sui, Xinmeng ;
Lu, Jian ;
Wei, Deqiang ;
Zhang, Lin ;
Wang, Rong ;
Zhao, Wei ;
Zhang, Weiping .
CORROSION SCIENCE, 2022, 206
[33]   Development of High Chromium Steel for Fast Breeder Reactors with High-temperature Strength, Ductility, and Microstructural Stability [J].
Onizawa, Takashi ;
Asayama, Tai ;
Kikuchi, Kenji .
ISIJ INTERNATIONAL, 2013, 53 (06) :1081-1088
[34]   Effect of rare earth cerium and impurity tin on the hot ductility of a Cr-Mo low alloy steel [J].
宋申华 ;
徐野威 ;
陈贤淼 ;
姜雪 .
Journal of Rare Earths, 2016, 34 (10) :1062-1068
[35]   High-Temperature Oxidation Behavior of TiN-Ti5Si3 Ceramic Composites Manufactured by Polymer Pyrolysis [J].
Kim, Beom-Seob ;
Kim, Deug-Joong ;
Lee, Dong-Bok .
JOURNAL OF THE KOREAN CERAMIC SOCIETY, 2006, 43 (08) :486-491
[36]   Alloying Effect of Niobium and Tin on the Zirconium Alloy Fuel Cladding Behavior at High Temperature Oxidation in Steam [J].
Malgin, Andrey ;
Markelov, Vladimir A. ;
Gusev, Anatoly ;
Nikulina, Antonina ;
Novikov, Vladimir ;
Shelepov, Ivan ;
Donnikov, Vladimir ;
Latynin, Vyacheslav ;
Kosihina, Julia .
ZIRCONIUM IN THE NUCLEAR INDUSTRY: 18TH INTERNATIONAL SYMPOSIUM, 2018, 1597 :983-1010
[37]   STUDY OF BEHAVIOR OF TIN-ZINC-ALUMINIUM ALLOYS FOR HIGH-TEMPERATURE APPLICATIONS [J].
Drapala, Jaromir ;
Musiol, Jan ;
Petlak, Daniel ;
Burkovic, Rostislav ;
Vodarek, Vlastimil .
METAL 2010: 19TH INTERNATIONAL METALLURGICAL AND MATERIALS CONFERENCE, 2010, :776-781
[38]   High-Temperature Oxidation Behavior of TiN-, Cr-, and TiN-Cr PVD-Coated Zircaloy 4 Alloy at 1200 °C [J].
Tang, Yan-Yu ;
Chang, Yin-Lin ;
Luo, Wen ;
Tang, De-Wen .
MATERIALS, 2025, 18 (08)
[39]   Effect of Strain Rate on the Hot Ductility Behavior of a Continuously Cast Ti-Nb Microalloyed Steel [J].
Gontijo, Marina ;
Hoflehner, Christian ;
Estermann, Paul ;
Ilie, Sergiu ;
Six, Jakob ;
Sommitsch, Christof .
STEEL RESEARCH INTERNATIONAL, 2020, 91 (12)
[40]   High-Temperature Oxidation Behaviour of CrSi Coatings on 316 Austenitic Stainless Steel [J].
Gurtaran, Mikdat ;
Zhang, Zhenxue ;
Li, Xiaoying ;
Dong, Hanshan .
MATERIALS, 2023, 16 (09)