Effects of Microcrystallinity and Morphology on Physical Aging and Its Associated Effects on Tensile Mechanical and Environmental Stress Cracking Properties of Poly(ethylene terephthalate)

被引:17
作者
Zhou, Hongxia [1 ]
Lofgren, Elizabeth A. [1 ]
Jabarin, Saleh A. [1 ]
机构
[1] Univ Toledo, Coll Engn, Dept Chem & Environm Engn, Inst Polymer, Toledo, OH 43606 USA
关键词
poly(ethylene terephthalate); physical aging; crystallinity; enthalpy of relaxation; tensile mechanical properties; environmental stress cracking; GLASS-TRANSITION; CRYSTALLINE POLY(ETHYLENE-TEREPHTHALATE); POLY(ETHYLENE TEREPHTHALATE); POLY(VINYL ACETATE); POLYMERS; RELAXATION; FRACTURE; POLYETHYLENE; POLYSTYRENE; BEHAVIOR;
D O I
10.1002/app.29822
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Poly(ethylene terephthalate) samples with volume fraction levels of crystallinity up to 27% have been evaluated in terms of physical aging, tensile mechanical properties, and environmental stress cracking failures. Specific enthalpy recovery values were found to correspond with transitions from ductile to brittle modes of tensile mechanical failures, exhibited by samples with each level of crystallinity. For samples exposed to aging temperatures from 45 to 60 degrees C, these critical enthalpies decrease linearly with increased crystallinity. The environmental stress cracking behavior of semicrystalline PET was found to depend on both crystallinity levels and physical aging. Samples with higher levels of crystallinity undergo stress cracking failures at lower critical stresses than their less crystalline counterparts. Physical aging, before environmental stress cracking exposure, further decreases these critical stress values and leads to much shorter critical times for failures. It has been shown that the interspherulitic amorphous portion of the material is primarily responsible for the differences in tensile mechanical and environmental stress cracking behaviors, observed as a result of aging and exposure. This amorphous region becomes progressively more restricted with increasing crystallinity as well as with increased aging. It, therefore, requires shorter exposure times to exhibit brittle tensile mechanical failure and environmental stress cracking rupture. (C) 2009 Wiley Periodicals, Inc. J Appl Polym Sci 112: 2906-2917, 2009
引用
收藏
页码:2906 / 2917
页数:12
相关论文
共 37 条
  • [1] [Anonymous], 1986, FAILURE PLASTICS
  • [2] THE EFFECTS OF PHYSICAL AGING ON THE BRITTLE-FRACTURE BEHAVIOR OF POLYMERS
    ARNOLD, JC
    [J]. POLYMER ENGINEERING AND SCIENCE, 1995, 35 (02) : 165 - 169
  • [3] Arnold JC, 1996, TRENDS POLYM SCI, V4, P403
  • [4] Birley A.W., 1991, Physics of Plastics: Processing Porperties and Materials Engineering
  • [5] BOYD T, 1995, THESIS U TOLEDO TOLE
  • [6] Boyer R.F., 1975, J. Polym. Sci. Polym. Symp, V50, P189
  • [7] BROWSTOW W, 1986, FAILURE PLASTICS, P98
  • [8] BUNN CW, 1954, P ROY SOC LOND A MAT, V226, P531
  • [9] Physical ageing in poly(vinyl acetate) - 3. Structural relaxation and its effect on the stress relaxation modulus
    Cowie, JMG
    Ferguson, R
    Harris, S
    McEwen, IJ
    [J]. POLYMER, 1998, 39 (18) : 4393 - 4397
  • [10] Physical aging in poly(vinyl acetate). 2. Relative rates of volume and enthalpy relaxation
    Cowie, JMG
    Harris, S
    McEwen, IJ
    [J]. MACROMOLECULES, 1998, 31 (08) : 2611 - 2615