Mechanical properties of reaction sintered SiC-TiC composite

被引:37
作者
Ahmoye, Daniel [1 ]
Bucevac, Dusan [1 ]
Krstic, Vladimir D. [1 ]
机构
[1] Queens Univ, Dept Mech & Mat Engn, Kingston, ON K7L 3N6, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
sintering; composites; mechanical properties; SiC; FRACTURE-TOUGHNESS; MICROSTRUCTURE; TIO2;
D O I
10.1016/j.ceramint.2018.05.050
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
SiC-TiC composite containing 5-30 vol% TiC particles was fabricated by conversion of TiO2 to TiC during pressureless sintering. The presence of very fine and uniformly distributed, in-situ created TiC particles increased driving force for sintering allowing fabrication of high density SiC-TiC composite without the use of external pressure. The highest mechanical properties were measured in samples sintered at 1885 degrees C for 1 h. The highest values for hardness (similar to 20 GPa) and fracture strength (similar to 490 MPa) were measured in samples containing 5 vol% TiC, whereas the highest fracture toughness (similar to 5.5 MPa.m(1/2) ) was measured in samples containing 10 vol% TiC. The presence of in-situ created, uniformly distributed TiC particles was beneficial for activation of not only the crack deflection mechanism but also mechanism called toughening by residual stress crated due to the difference of thermal expansion between SiC matrix and TiC particles. The compressive stress field around TiC particles acts to close the propagating crack and thus to increase fracture toughness.
引用
收藏
页码:14401 / 14407
页数:7
相关论文
共 23 条
[1]   Reaction sintering of SiC composites with in situ converted TiO2 to TiC [J].
Ahmoye, Daniel ;
Krstic, Vladimir D. .
JOURNAL OF MATERIALS SCIENCE, 2015, 50 (07) :2806-2812
[2]   Effect of initial α-phase content of SiC on microstructure and mechanical properties of SiC-TiC composites [J].
An, HG ;
Kim, YW ;
Lee, JG .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2001, 21 (01) :93-98
[3]  
[Anonymous], 1969, THEORY ELASTICITY
[4]   A CRITICAL-EVALUATION OF INDENTATION TECHNIQUES FOR MEASURING FRACTURE-TOUGHNESS .1. DIRECT CRACK MEASUREMENTS [J].
ANSTIS, GR ;
CHANTIKUL, P ;
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (09) :533-538
[5]   Characterization of sintered TiC-SiC composites [J].
Chen, Jing ;
Li, WenJun ;
Jiang, Wan .
CERAMICS INTERNATIONAL, 2009, 35 (08) :3125-3129
[6]   Microstructure and fracture toughness of in-situ toughened SiC-TiC composites [J].
Cho, KS ;
Choi, HJ ;
Lee, JG ;
Kim, YW .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1998, 17 (13) :1081-1084
[7]  
Dong SM, 1996, J MATER SCI LETT, V15, P394
[8]   MICROSTRUCTURE AND MECHANICAL-PROPERTIES OF HOT-PRESSED SIC-TIC COMPOSITES [J].
ENDO, H ;
UEKI, M ;
KUBO, H .
JOURNAL OF MATERIALS SCIENCE, 1991, 26 (14) :3769-3774
[9]   CRACK DEFLECTION PROCESSES .1. THEORY [J].
FABER, KT ;
EVANS, AG .
ACTA METALLURGICA, 1983, 31 (04) :565-576
[10]   The assessment of thermodynamic parameters in the Al2O3-Y2O3 system and phase relations in the Y-Al-O system [J].
Fabrichnaya, O ;
Seifert, HJ ;
Ludwig, T ;
Aldinger, F ;
Navrotsky, A .
SCANDINAVIAN JOURNAL OF METALLURGY, 2001, 30 (03) :175-183