Microstructure, Tribological Properties and Corrosion Behaviour of Additively Manufactured 17-4PH Stainless Steel: Effects of Scanning Pattern, Build Orientation, and Single vs. Double scan

被引:46
作者
Lashgari, H. R. [1 ]
Xue, Y. [1 ]
Onggowarsito, C. [1 ]
Kong, C. [2 ]
Li, S. [1 ]
机构
[1] Univ New South Wales, Sch Mat Sci & Engn, Sydney, NSW 2052, Australia
[2] Univ New South Wales, Mark Wainwright Analyt Ctr MWAC, Sydney, NSW 2052, Australia
关键词
Selective laser melting; 17-4PH stainless steel; Wear; Corrosion; Manufacturing parameters; nanohardness; MECHANICAL-PROPERTIES; PROCESS PARAMETERS; LASER; POWDER;
D O I
10.1016/j.mtcomm.2020.101535
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The aim of the present study is to investigate the effect of different process parameters, i.e. scanning pattern (hexagonal vs. concentric), build orientation (vertical vs. horizontal), and single scan vs. double scan on the microstructure, wear resistance and corrosion properties of additively manufactured 17-4PH stainless steel by means of advanced material characterization techniques such as X-ray diffraction (XRD), electron back scatter diffraction (EBSD), and scanning electron microscopy (SEM). The volume fraction of retained austenite varied from 0.7% to 4.4% based upon the orientation and scanning strategy. In both scanning patterns, the maximum variation of nanohardness (along the build-axis and perpendicular to the build axis) was observed in the vertically printed samples using the single scan whereas the double-scan strategy (remelting) decreased the variation in both scanning patterns via lowering the temperature gradient and cooling rate. Remelting enhanced the wear resistance (by almost approximate to 50%) by decreasing the volume fraction of pores and balling defects up to approximate to 60-70% in the hexagon and concentric scanning pattern. The build orientation (vertical vs. horizontal) had more influence on the wear resistance in the concentric scanning pattern than that of hexagon pattern. Oxidative/abrasive wear was found to be the dominant wear mechanism during the reciprocating action in both scanning patterns; however, the oxide film was more prone to fracture in the samples fabricated by the concentric pattern due to the presence of more micropores in the matrix especially in the areas where laser direction changed. In the phosphate-buffered saline (PBS) solution, the corrosion rate of the samples manufactured using the hexagonal scanning pattern was generally less than those manufactured using the concentric pattern owing to the lower porosity. The lower breakdown potential in the concentric scanning pattern indicates that the protective passive layer is broken down easily making it susceptible to pitting corrosion due to the presence of porosities between the laser tracks. The Inductively Coupled Plasma (ICP) analysis revealed that the sample fabricated using single scan with hexagon scanning pattern and orientated vertically released the least amount of ions in the PBS solution, showing the significance for understanding the effect of additive manufacturing parameters on functional materials.
引用
收藏
页数:14
相关论文
共 18 条
[1]  
[Anonymous], 2009, G5997 ASTM
[2]   A critical review of powder-based additive manufacturing of ferrous alloys: Process parameters, microstructure and mechanical properties [J].
Fayazfar, Haniyeh ;
Salarian, Mehrnaz ;
Rogalsky, Allan ;
Sarker, Dyuti ;
Russo, Paola ;
Paserin, Vlad ;
Toyserkani, Ehsan .
MATERIALS & DESIGN, 2018, 144 :98-128
[3]   The status, challenges, and future of additive manufacturing in engineering [J].
Gao, Wei ;
Zhang, Yunbo ;
Ramanujan, Devarajan ;
Ramani, Karthik ;
Chen, Yong ;
Williams, Christopher B. ;
Wang, Charlie C. L. ;
Shin, Yung C. ;
Zhang, Song ;
Zavattieri, Pablo D. .
COMPUTER-AIDED DESIGN, 2015, 69 :65-89
[4]   Laser additive manufacturing of metallic components: materials, processes and mechanisms [J].
Gu, D. D. ;
Meiners, W. ;
Wissenbach, K. ;
Poprawe, R. .
INTERNATIONAL MATERIALS REVIEWS, 2012, 57 (03) :133-164
[5]   An investigation into the effect of process parameters on melt pool geometry, cell spacing, and grain refinement during laser powder bed fusion [J].
Keshavarzkermani, Ali ;
Marzbanrad, Ehsan ;
Esmaeilizadeh, Reza ;
Mahmoodkhani, Yahya ;
Ali, Usrnan ;
Enrique, Pablo D. ;
Zhou, Norman Y. ;
Bonakdar, Ali ;
Toyserkani, Ehsan .
OPTICS AND LASER TECHNOLOGY, 2019, 116 :83-91
[6]   Effect of scan pattern on the microstructure and mechanical properties of Powder Bed Fusion additive manufactured 17-4 stainless steel [J].
Kudzal, Andelle ;
McWilliams, Brandon ;
Hofmeister, Clara ;
Kellogg, Frank ;
Yu, Jian ;
Taggart-Scarff, Joshua ;
Liang, Jianyu .
MATERIALS & DESIGN, 2017, 133 :205-215
[7]  
Lashgari H.R., 2020, WEAR, P456
[8]   Balling behavior of stainless steel and nickel powder during selective laser melting process [J].
Li, Ruidi ;
Liu, Jinhui ;
Shi, Yusheng ;
Wang, Li ;
Jiang, Wei .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2012, 59 (9-12) :1025-1035
[9]   A study on the residual stress during selective laser melting (SLM) of metallic powder [J].
Liu, Yang ;
Yang, Yongqiang ;
Wang, Di .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2016, 87 (1-4) :647-656
[10]   Mechanical properties and microstructural characterization of selective laser melted 17-4 PH stainless steel [J].
Mahmoudi, Mohamad ;
Elwany, Alaa ;
Yadollahi, Aref ;
Thompson, Scott M. ;
Bian, Linkan ;
Shamsaei, Nima .
RAPID PROTOTYPING JOURNAL, 2017, 23 (02) :280-294