Microstructural evolution and grain boundary sliding in a superplastic magnesium AZ31 alloy

被引:128
作者
Panicker, R. [1 ]
Chokshi, A. H. [1 ]
Mishra, R. K. [2 ]
Verma, R. [2 ]
Krajewski, P. E. [2 ]
机构
[1] Indian Inst Sci, Dept Mat Engn, Bangalore 560012, Karnataka, India
[2] Gen Motors R&D, Mat & Proc Lab, Warren, MI USA
关键词
Superplastic; Mg; Grain boundary sliding; Texture; Dislocation creep; DEFORMATION MECHANISMS; ELEVATED-TEMPERATURES; MG ALLOYS; SIZE; DEPENDENCE; DUCTILITY;
D O I
10.1016/j.actamat.2009.04.011
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Tensile experiments on a fine-grained single-phase Mg-Zn-Al alloy (AZ31) at 673 K revealed superplastic behavior with an elongation to failure of 475% at 1 x 10(-4) s(-1) and non-superplastic behavior with an elongation to failure of 160% at 1 x 10(-2) s(-1); the corresponding sponding strain rate sensitivities under these conditions were similar to 0.5 and similar to 0.2. respectively. Measurements indicated that the grain boundary sliding (GBS) contribution to strain xi was similar to 30% under non-superplastic conditions: there was also a significant sharpening in texture during such deformation. Under superplastic conditions, xi was similar to 50% at both low and high elongations of similar to 20% and 120%; the initial texture became more random under such conditions. In non-superplastic conditions, deformation occurred under conditions without grain growth before significant flow localization whereas, under superplastic conditions, there was grain growth during the early stages of deformation, leading to strain hardening. The grains retained equiaxed shapes under all experimental conditions. Superplastic deformation is attributed to GBS, while non-superplastic deformation is attributed to intragranular dislocation creep with some contribution from GBS. The retention of equiaxed grain shapes during dislocation creep is consistent with a model based on local recovery related to the disturbance of triple junctions. (C) 2009 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:3683 / 3693
页数:11
相关论文
共 25 条
[1]   SUPERPLASTICITY IN FINE-GRAINED CERAMICS AND CERAMIC COMPOSITES - CURRENT UNDERSTANDING AND FUTURE-PROSPECTS [J].
CHOKSHI, AH .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1993, 166 (1-2) :119-133
[2]   SUPERPLASTICITY IN ADVANCED MATERIALS [J].
CHOKSHI, AH ;
MUKHERJEE, AK ;
LANGDON, TG .
MATERIALS SCIENCE & ENGINEERING R-REPORTS, 1993, 10 (06) :237-274
[3]   Superplasticity in a magnesium alloy prepared with bimodal grain size distributions developed by dynamic recrystallisation [J].
del Valle, J. A. ;
Ruano, O. A. .
MATERIALS LETTERS, 2008, 62 (19) :3391-3394
[4]   Deformation mechanisms responsible for the high ductility in a Mg AZ31 alloy analyzed by electron backscattered diffraction [J].
Del Valle, JA ;
Pérez-Prado, MT ;
Ruano, OA .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2005, 36A (06) :1427-1438
[5]   Developing superplasticity in a magnesium AZ31 alloy by ECAP [J].
Figueiredo, Roberto B. ;
Langdon, Terence G. .
JOURNAL OF MATERIALS SCIENCE, 2008, 43 (23-24) :7366-7371
[6]  
Frost H.J., 1982, DEFORMATION MECH MAP, P44
[7]   Superplasticity in thin magnesium alloy sheets and deformation mechanism maps for magnesium alloys at elevated temperatures [J].
Kim, WJ ;
Chung, SW ;
Chung, CS ;
Kum, D .
ACTA MATERIALIA, 2001, 49 (16) :3337-3345
[8]  
KOTTADA RS, UNPUB
[9]   Overview of Quick Plastic Forming technology [J].
Krajewski, P. E. ;
Schroth, J. G. .
SUPERPLASTICITY IN ADVANCED MATERIALS, 2007, 551-552 :3-+
[10]   Deformation mechanisms in superplastic AA5083 materials [J].
Kulas, MA ;
Green, WP ;
Taleff, EM ;
Krajewski, PE ;
McNelley, TR .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2005, 36A (05) :1249-1261