Microstructure-performance relationships in gas tungsten arc welded Hastelloy X nickel-based superalloy

被引:37
|
作者
Ghasemi, Ali [1 ]
Kolagar, Ali Mohammad [2 ]
Pouranvari, Majid [3 ]
机构
[1] McMaster Univ, Dept Mech Engn, Hamilton, ON L8S 4L7, Canada
[2] MavadKaran Engn Co, Mapna Grp, Res & Dev Dept, Tehran, Iran
[3] Sharif Univ Technol, Dept Mat Sci & Engn, Tehran 113659466, Iran
关键词
Fusion welding; Hastelloy X; Microstructure; Stress-rupture; Tensile properties; Post weld heat treatment; RESIDUAL-STRESS; HEAT-TREATMENT; MECHANICAL-PROPERTIES; PULSED NDYAG; SOLIDIFICATION; TEMPERATURE; BEHAVIOR; CRACKING; STRAIN; FIBER;
D O I
10.1016/j.msea.2020.139861
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This study aims at understanding the metallurgical and mechanical response of Hastelloy X nickel-based superalloy to the thermal cycle of gas tungsten arc welding (GTAW), post welding solution treatment (ST), and aging. In the as-weld condition, the weldment was characterized by the formation of the M6C carbide, sigma phase, and micro-solidification cracks in the interdendritic zones of the weld metal, and constitutional liquation of M6C carbide in the heat-affected zone. It is demonstrated that neither the weld metal nor the heat-affected zone could adversely affect mechanical properties of the welded joint in as-weld condition. However, to alleviate the microstructural heterogeneity, tensile residual stresses, and non-equilibrium microstructure developed due to the welding thermal cycle, the weldment was subjected to the solution treatment cycle (1177 degrees C/5 min) as post-weld heat treatment. The post-weld heat treatment enabled complete elimination of sigma phase. The tensile and creep properties of the weldment after the solution treatment cycle were compared to that of the asweld condition. Despite the 8% decrease in the strength of the weldment after the ST cycle, the sample not only still met the minimum mechanical requirements but also benefited from a homogenized and nearly equilibrium microstructure. Microstructural observations of the weldment after the aging cycle (800 degrees C/8h), as well as its mechanical response, revealed that the formation of continuous Cr-rich carbides at the grain boundaries of the base metal deteriorates the room temperature ductility and creep life of the joints.
引用
收藏
页数:13
相关论文
共 50 条
  • [11] Disclosing connection links between microstructure and mechanical performance in pulsating current gas tungsten arc welding of Hastelloy B-2 superalloy
    Dezfuli, Mehdi Khalasi
    Moghadam, Ali Heidary
    Hasab, Mehdi Ghobeiti
    Ashiri, Rouholah
    JOURNAL OF ADVANCED JOINING PROCESSES, 2024, 10
  • [12] Effect of Pulsed Current Gas Tungsten Arc Process on the Dissimilar Weldments between Nickel-based Superalloy/Austenitic Stainless Steel
    Sharma, Sumitra
    Taiwade, Ravindra Vasantrao
    Vashishtha, Himanshu
    ISIJ INTERNATIONAL, 2017, 57 (06) : 1080 - 1086
  • [13] Characterization of microstructure and mechanical properties of nickel based superalloy 617 by pulsed current gas tungsten arc welding technique
    Mageshkumar, K.
    Kuppan, P.
    Arivazhagan, N.
    MATERIALS RESEARCH EXPRESS, 2018, 5 (06):
  • [14] Investigation on the multi-pass gas tungsten arc welded Bi-metallic combination between nickel-based superalloy and Ti-stabilized austenitic stainless steel
    Sharma, Sumitra
    Taiwade, Ravindra V.
    Vashishtha, Himanshu
    JOURNAL OF MATERIALS RESEARCH, 2017, 32 (16) : 3055 - 3065
  • [15] Investigation on the multi-pass gas tungsten arc welded Bi-metallic combination between nickel-based superalloy and Ti-stabilized austenitic stainless steel
    Sumitra Sharma
    Ravindra V. Taiwade
    Himanshu Vashishtha
    Journal of Materials Research, 2017, 32 : 3055 - 3065
  • [16] Microstructure-Performance Relationships of sPEEK-Based Catalyst Layers
    Peron, Jennifer
    Edwards, Dave
    Besson, Arthur
    Shi, Zhiqing
    Holdcroft, Steven
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2010, 157 (08) : B1230 - B1236
  • [17] Microstructure, Mechanical Properties and Fatigue Crack Growth Behavior of Gas Tungsten Arc Welding Welded Joint of the Hastelloy N Alloy
    Wang, Sai
    Ma, Baoyun
    Feng, Daochen
    Chen, Shuangjian
    Ma, Yinghe
    Li, Huaxin
    Lv, Chuanyang
    Zheng, Wenjian
    Yang, Jianguo
    MATERIALS, 2023, 16 (19)
  • [18] Assessment of Microstructure and Tensile Behavior of Hot Wire Gas Tungsten Arc Welded Pure Nickel Tubes
    C. Pravin Tamil Selvan
    K. Kalaiselvan
    I. Dinaharan
    R. Palanivel
    Transactions of the Indian Institute of Metals, 2021, 74 : 355 - 368
  • [19] Assessment of Microstructure and Tensile Behavior of Hot Wire Gas Tungsten Arc Welded Pure Nickel Tubes
    Pravin Tamil Selvan, C.
    Kalaiselvan, K.
    Dinaharan, I.
    Palanivel, R.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2021, 74 (02) : 355 - 368
  • [20] Solidification and solid-state phenomena during keyhole-gas tungsten arc welding of IN617 nickel-based superalloy
    Latifi, Reza
    Ara, Masoud Vatan
    Yazdizadeh, Morteza
    Pouranvari, Majid
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2025, 30 (01) : 25 - 33