Evaluation of a 2.5 kWel automotive low temperature PEM fuel cell stack with extended operating temperature range up to 120°C

被引:24
作者
Ruiu, Tiziana [1 ]
Dreizler, Andreas M. [1 ]
Mitzel, Jens [1 ]
Guelzow, Erich [1 ]
机构
[1] German Aerosp Ctr DLR, Inst Engn Thermodynam, Pfaffenwaldring 38-40, D-70569 Stuttgart, Germany
关键词
PEM fuel cell; Stack; Thermal cycling; Long-term test; End-of-life characterization; Degradation phenomena; ACID DOPED POLYBENZIMIDAZOLE; DEGRADATION MECHANISMS; MEMBRANE; DURABILITY; METHANOL; ELECTROOXIDATION; PERFORMANCE; TRANSPORT; HUMIDITY; REVERSAL;
D O I
10.1016/j.jpowsour.2015.10.056
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Nowadays, the operating temperature of polymer electrolyte membrane fuel cell stacks is typically limited to 80 degrees C due to water management issues of membrane materials. In the present work, short-term operation at elevated temperatures up to 120 degrees C and long-term steady-state operation under automotive relevant conditions at 80 degrees C are examined using a 30-cell stack developed at DLR. The high temperature behavior is investigated by using temperature cycles between 90 and 120 degrees C without adjustment of the gases dew points, to simulate a short-period temperature increase, possibly caused by an extended power demand and/or limited heat removal. This galvanostatic test demonstrates a fully reversible performance decrease of 21 +/- 1% during each thermal cycle. The irreversible degradation rate is about a factor of 6 higher compared to the one determined by the long-term test. The 1200-h test at 80 degrees C demonstrates linear stack voltage decay with acceptable degradation rate, apart from a malfunction of the air compressor, which results in increased catalyst degradation effects on individual cells. This interpretation is based on an end-of-life characterization, aimed to investigate catalyst, electrode and membrane degradation, by determining hydrogen crossover rates, high frequency resistances, electrochemically active surface areas and catalyst particle sizes. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:257 / 266
页数:10
相关论文
共 41 条
[1]   Validation of an externally oil-cooled 1 kWel HT-PEMFC stack operating at various experimental conditions [J].
Bujlo, P. ;
Pasupathi, S. ;
Ulleberg, O. ;
Scholta, J. ;
Nomnqa, M. V. ;
Rabiu, A. ;
Pollet, B. G. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2013, 38 (23) :9847-9855
[2]   High temperature (HT) polymer electrolyte membrane fuel cells (PEMFC) - A review [J].
Chandan, Amrit ;
Hattenberger, Mariska ;
El-Kharouf, Ahmad ;
Du, Shangfeng ;
Dhir, Aman ;
Self, Valerie ;
Pollet, Bruno G. ;
Ingram, Andrew ;
Bujalski, Waldemar .
JOURNAL OF POWER SOURCES, 2013, 231 :264-278
[3]   Effects of temperature and humidity on the cell performance and resistance of a phosphoric acid doped polybenzimidazole fuel cell [J].
Chen, Chen-Yu ;
Lai, Wei-Hsiang .
JOURNAL OF POWER SOURCES, 2010, 195 (21) :7152-7159
[4]   Electrochemical impedance study of electrode-membrane assemblies in PEM fuel cells I.: Electro-oxidation of H2 and H2/CO mixtures on Pt-based gas-diffusion electrodes [J].
Ciureanu, M ;
Wang, H .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1999, 146 (11) :4031-4040
[5]   Degradation of polymer electrolyte membranes [J].
Collier, Amanda ;
Wang, Haijiang ;
Yuan, Xiao Zi ;
Zhang, Jiujun ;
Wilkinson, David P. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2006, 31 (13) :1838-1854
[6]  
Cooper K. R., 2009, FUEL CELL MAGAZI JAN, P1
[7]   A review on water balance in the membrane electrode assembly of proton exchange membrane fuel cells [J].
Dai, Wei ;
Wang, Haijiang ;
Yuan, Xiao-Zi ;
Martin, Jonathan J. ;
Yang, Daijun ;
Qiao, Jinli ;
Ma, Jianxin .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2009, 34 (23) :9461-9478
[8]   Influence of ageing in fuel cell on membrane/electrodes interfaces [J].
Danerol, A. S. ;
Bas, C. ;
Flandin, L. ;
Claude, E. ;
Alberola, N. D. .
JOURNAL OF POWER SOURCES, 2011, 196 (07) :3479-3484
[9]   Durability and degradation issues of PEM fuel cell components [J].
de Bruijn, F. A. ;
Dam, V. A. T. ;
Janssen, G. J. M. .
FUEL CELLS, 2008, 8 (01) :3-22
[10]   Experimental study of water transport in a polybenzimidazole-based high temperature PEMFC [J].
Galbiati, Samuele ;
Baricci, Andrea ;
Casalegno, Andrea ;
Marchesi, Renzo .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2012, 37 (03) :2462-2469