Degradation of a polyester-urethane coating: Physical properties

被引:6
|
作者
Makki, Hesam [1 ,2 ]
Adema, Koen N. S. [1 ,2 ]
Peters, Elias A. J. F. [1 ]
Laven, Jozua [1 ]
van der Ven, Leendert G. J. [1 ]
van Benthem, Rolf A. T. M. [1 ,3 ]
de With, Gijsbertus [1 ]
机构
[1] Eindhoven Univ Technol, Lab Mat & Interface Chem, Dept Chem Engn & Chem, NL-5612 AJ Eindhoven, Netherlands
[2] DPI, POB 902, NL-5600 AX Eindhoven, Netherlands
[3] DSM Ahead Performance Mat BV, POB 18, NL-6160 MD Geleen, Netherlands
关键词
degradation; internal stress; mechanical properties; oxygen permeability; polyester-urethane; polyurethanes; Thermal properties; thermomechanical properties; SEMIINTERPENETRATING POLYMER NETWORKS; DYNAMIC-MECHANICAL PROPERTIES; UV AGING CHARACTERIZATION; ORGANIC COATINGS; STRESS; FILMS; PHOTOOXIDATION; PERMEABILITY; TEMPERATURE; RELAXATION;
D O I
10.1002/polb.23958
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
In this article we studied the evolution of thermomechanical properties of a polyester-urethane coating during degradation under different degradation conditions, i.e., aerobic and anaerobic conditions with and without dry/wet cycling during degradation. Dynamic mechanical and thermal analyses show that under aerobic conditions the coatings become stiffer and more brittle in the glassy state. This stiffening is probably due to the increase in the amount of hydrogen bonding and the formation of oxidized groups which increase the polarity of the material and enhance the interactions of the polymer segments. However, oxidation reactions result in a considerable decrease in cross-link density and stiffness in the rubbery state. Both changes, in the glassy and rubbery states, give rise to development of internal stresses. These stresses increase as the degradation process proceeds. Nevertheless, for samples exposed to anaerobic conditions, the stiffness remains constant in the glassy state and the cross-link density slightly increases as a result of degradation. This reconfirms the dominance of the effect of oxidation reactions on the mechanical failure of the coatings. Oxygen permeation measurements show a more-or-less time-independent diffusion coefficient and a gradual decrease in solubility of oxygen as a function of exposure time. This results in a slight decrease in oxygen permeation (mainly in the early stage of the degradation) as degradation proceeds. (c) 2015 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2016, 54, 659-671
引用
收藏
页码:659 / 671
页数:13
相关论文
共 50 条
  • [1] The influence of the exposure conditions on the chemical and physical changes of polyester-urethane coatings during photodegradation
    Adema, Koen N. S.
    Makki, Hesam
    Peters, Elias A. J. F.
    Laven, Jozua
    van der Ven, Leendert G. J.
    van Benthem, Rolf A. T. M.
    de With, Gijsbertus
    POLYMER DEGRADATION AND STABILITY, 2016, 123 : 13 - 25
  • [2] Quantitative spectroscopic analysis of weathering of polyester-urethane coatings
    Makki, Hesam
    Adema, Koen N. S.
    Peters, Elias A. J. F.
    Laven, Jozua
    van der Ven, Leendert G. J.
    van Benthem, Rolf A. T. M.
    de With, Gijsbertus
    POLYMER DEGRADATION AND STABILITY, 2015, 121 : 280 - 291
  • [3] Mechanical property changes and degradation during accelerated weathering of polyester-urethane coatings
    Allen Skaja
    Dilhan Fernando
    Stuart Croll
    JCT Research, 2006, 3 : 41 - 51
  • [4] Mechanical property changes and degradation during accelerated weathering of polyester-urethane coatings
    Skaja, A
    Fernando, D
    Croll, S
    JCT RESEARCH, 2006, 3 (01): : 41 - 51
  • [5] Weathering of a polyester-urethane clearcoat: Lateral inhomogeneities
    Makki, Hesam
    Adema, Koen N. S.
    Hendrix, Marco M. R. M.
    Peters, Elias A. J. F.
    Laven, Jozua
    van der Ven, Leendert G. J.
    van Benthem, Rolf A. T. M.
    de With, Gijsbertus
    POLYMER DEGRADATION AND STABILITY, 2015, 122 : 180 - 186
  • [6] Electrospun polyester-urethane scaffold preserves mechanical properties and exhibits strain stiffening during in situ tissue ingrowth and degradation
    Krynauw, Hugo
    Omar, Rodaina
    Koehne, Josepha
    Limbert, Georges
    Davies, Neil H.
    Bezuidenhout, Deon
    Franz, Thomas
    SN APPLIED SCIENCES, 2020, 2 (05):
  • [7] Electrospun polyester-urethane scaffold preserves mechanical properties and exhibits strain stiffening during in situ tissue ingrowth and degradation
    Hugo Krynauw
    Rodaina Omar
    Josepha Koehne
    Georges Limbert
    Neil H. Davies
    Deon Bezuidenhout
    Thomas Franz
    SN Applied Sciences, 2020, 2
  • [8] Toughening of poly(L-lactide) by polyester-urethane networks based on castor oil-modified ε-caprolactone oligomers
    Fujigasaki, Junya
    Shibata, Mitsuhiro
    JOURNAL OF POLYMER RESEARCH, 2015, 22 (11)
  • [9] Degradation profiles of polyester-urethane (hydroxylated polyester/diphenylmethane diisocyanate) and polyester-melamine (hydroxylated polyester/hexamethoxymethyl-melamine) coatings: An accelerated weathering study
    Narayan, R
    Chattopadhyay, DK
    Sreedhar, B
    Raju, KVSN
    Mallikarjuna, NN
    Aminabhavi, TM
    JOURNAL OF APPLIED POLYMER SCIENCE, 2005, 97 (03) : 1069 - 1081
  • [10] Kinetic Monte Carlo simulation of the photodegradation process of polyester-urethane coatings
    Adema, Koen N. S.
    Makki, Hesam
    Peters, Elias A. J. F.
    Laven, Jozua
    van der Ven, Leendert G. J.
    van Benthem, Rolf A. T. M.
    de With, Gijsbertus
    PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 2015, 17 (30) : 19962 - 19976