Corrosion of metals and alloys in molten glasses. Part 2: nickel and cobalt high chromium superalloys behaviour and protection

被引:44
作者
Di Martino, J [1 ]
Rapin, C [1 ]
Berthod, P [1 ]
Podor, R [1 ]
Steinmetz, P [1 ]
机构
[1] Univ Henri Poincare, Fac Sci & Tech, Lab Chim Solide Mineral, UMR 7555, F-54506 Vandoeuvre Les Nancy, France
关键词
glass; superalloys; electrochemical calculation; SEM; high temperature corrosion;
D O I
10.1016/j.corsci.2003.10.025
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Electrochemical methods have been used for the characterisation of high chromium alloys corrosion in molten glasses (cobalt and nickel base alloys in a borosilicate glass at 1050 degreesC, with rotating working electrodes). All the tested alloys are active but passivable materials. The active state is characterised by a rapid dissolution of the constitutive elements of the alloy in the glass melt. The passive state can be obtained by an air oxidation of the alloys (called preoxidation) or with a temporary anodic polarisation of the alloy. The obtained passive state is due to the presence of a thin protective chromia scale. (C) 2003 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1865 / 1881
页数:17
相关论文
共 9 条
[1]  
BAKER GC, 1958, ANAL CHIM ACTA, V18, P118
[2]  
DIMARTINO J, 2002, P 6 ESG C GLASS OD M
[3]   Enthalpies of chromium oxide solution in soda lime borosilicate glass systems [J].
Kim, CW ;
Choi, K ;
Park, JK ;
Shin, SW ;
Song, MJ .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2001, 84 (12) :2987-2990
[4]  
KOFSTAD P, 1974, SCI TECHNIQUES, V16, P35
[5]  
KORDON T, 1990, GLASTECH BER-GLASS, V63, P213
[6]   Corrosion of nickel-chromium alloys by molten glass at 1100°C:: An electrochemical study [J].
Lizarazu, D ;
Steinmetz, P ;
Bernard, JL .
HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 4, PTS 1 AND 2, 1997, 251-2 :709-719
[7]  
MAZARS P, 1982, MET CORROS-IND, V686, P321
[8]   THEORY OF SQUARE WAVE VOLTAMMETRY [J].
RAMALEY, L ;
KRAUSE, MS .
ANALYTICAL CHEMISTRY, 1969, 41 (11) :1362-&
[9]  
WOLF MB, 1984, GLASS SCI TECHNOLOGY, V7