Nanoporous characterization of modified humidity-sensitive MgO-Al2O3 ceramics by positron annihilation lifetime spectroscopy method

被引:6
|
作者
Klym, H. [1 ]
Ingram, A. [2 ]
Hadzaman, I. [3 ]
Karbovnyk, I. [4 ]
Vasylchyshyn, I. [1 ]
Popov, A. I. [5 ]
机构
[1] Lviv Polytech Natl Univ, 12 Bandera St, UA-79646 Lvov, Ukraine
[2] Opole Univ Technol, 75 Ozimska St, PL-45370 Opole, Poland
[3] Drohobych Ivan Franko State Pedag Univ, 24 I Franko St, UA-82100 Drogobych, Ukraine
[4] Ivan Franko Natl Univ Lviv, 107 Tarnavskogo St, UA-79017 Lvov, Ukraine
[5] Univ Latvia, Inst Solid State Phys, 8 Kengaraga St, LV-1063 Riga, Latvia
来源
FUNCTIONAL MATERIALS AND NANOTECHNOLOGIES (FM&NT 2018) | 2019年 / 503卷
关键词
PORE STRUCTURE; FREE-VOLUME; SENSORS;
D O I
10.1088/1757-899X/503/1/012019
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Investigation of nanopores in the humidity-sensitive MgO-Al2O3 ceramics modified at 1100 degrees C for 2 hours was performed using positron annihilation lifetime spectroscopy method. Lifetimes of the third and fourth components of positron annihilation lifetime spectra obtained by four-component fitting procedure were used for calculation of nanopores radii. Transformation in free volumes was studied in ceramics after drying and exposure to water vapor. It is established that the lifetime of the third component decreases and the intensity of this component increases in ceramics exposed to water vapor reflecting ortho-positronium decay in nanopores simultaneously with annihilation in water bubbles. The characteristics of the fourth component (lifetime and intensity) decrease in ceramics exposed to water vapor reflecting ortho-positronium trapping in free-water volume of nanopores. Final drying of the MgO-Al2O3 ceramics results in returning of ortho-positronium lifetimes and intensities to the initial values confirming good desorption of water from nanopores of ceramics.
引用
收藏
页数:6
相关论文
共 50 条
  • [21] Preparation and characterization of Ru/MgO-Al2O3 catalysts for methane steam reforming
    Carvalho, Luciene Santos
    Martins, Andre Rosa
    Reyes, Patricio
    Oportus, Marcelo
    Albonoz, Alberto
    Vicentini, Valeria
    Rangel, Maria do Carmo
    CATALYSIS TODAY, 2009, 142 (1-2) : 52 - 60
  • [22] Effect of water adsorption on positron-electron annihilation kinetics in the MgO-Al2O3ceramics in the frequency domain
    Fl'unt, Orest
    Klym, Halyna
    Ingram, Adam
    Szatanik, Roman
    APPLIED NANOSCIENCE, 2020, 10 (08) : 2769 - 2774
  • [23] Positron annihilation lifetime study of hydrogen-charged Al-Al2O3 composites
    Haldar, B
    Balasubramaniam, R
    Singru, RM
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1996, 15 (21) : 1858 - 1859
  • [24] Positron Annihilation Lifetime Spectroscopy Insight on Free Volume Conversion of Nanostructured MgAl2O4 Ceramics
    Klym, Halyna
    Karbovnyk, Ivan
    Piskunov, Sergei
    Popov, Anatoli I.
    NANOMATERIALS, 2021, 11 (12)
  • [25] Spark Plasma Sintering of α/β Si3N4 Ceramics with MgO-Al2O3 and MgO-Y2O3 as Sintering Additives
    Yu, F. L.
    Bai, Y.
    Han, P. D.
    Shi, Q. L.
    Ni, S.
    Wu, J. H.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2016, 25 (12) : 5220 - 5224
  • [26] Spark Plasma Sintering of α/β Si3N4 Ceramics with MgO-Al2O3 and MgO-Y2O3 as Sintering Additives
    F. L. Yu
    Y. Bai
    P. D. Han
    Q. L. Shi
    S. Ni
    J. H. Wu
    Journal of Materials Engineering and Performance, 2016, 25 : 5220 - 5224
  • [27] Extended Positron-Trapping Defects in the Eu3+-Doped BaGa2O4 Ceramics Studied by Positron Annihilation Lifetime Method
    Klym, Halyna
    Karbovnyk, Ivan
    Luchechko, Andriy
    Kostiv, Yuriy
    Popov, Anatoli I.
    PHYSICA STATUS SOLIDI B-BASIC SOLID STATE PHYSICS, 2022, 259 (08):
  • [28] Probing free volume in ZnO-P2O5-SeO2:Au2O3 glass ceramics with positron annihilation lifetime spectroscopy
    Reddy, G. Naga Koti
    Kostrzewa, M.
    Sekhar, A. Venkata
    Purnachand, N.
    Ingram, A.
    Reddy, A. Siva Sesha
    Raju, G. Naga
    Kumar, V. Ravi
    Veeraiah, N.
    RADIATION PHYSICS AND CHEMISTRY, 2025, 230
  • [29] Spark plasma sintering of a-Si3N4 ceramics with MgO-Al2O3 as sintering additives
    Yan, Faqiang
    Chen, Fei
    Shen, Qiang
    Zhang, Lianmeng
    COMPOSITE MATERIALS V, 2007, 351 : 176 - +
  • [30] CHEMICO-MINERALOGICAL CHARACTERIZATION OF UNUSED AND USED REFRACTORY BRICKS BASED ON MGO-AL2O3
    BARTHA, P