Influence of mineral by-products on compressive strength and microstructure of concrete at high temperature

被引:21
作者
Sahani, Ashok Kr [1 ]
Samanta, Amiya K. [1 ]
Roy, Dilip K. Singha [1 ]
机构
[1] NIT Durgapur, Dept Civil Engn, MG Ave, Durgapur 713209, W Bengal, India
关键词
fly ash; GBFS; elevated temperatures; weight loss; compressive strength; microstructure; BLAST-FURNACE SLAG; HIGH-PERFORMANCE CONCRETE; FIRE-DAMAGED CONCRETE; FLY-ASH; MECHANICAL-PROPERTIES; ELEVATED-TEMPERATURES; LIGHTWEIGHT CONCRETE; FINE AGGREGATE; DURABILITY PERFORMANCE; RESIDUAL PROPERTIES;
D O I
10.12989/acc.2019.7.4.263
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In the present work, Granulated Blast Furnace Slag (GBFS) and Fly ash (FA) were used as partial replacement of Natural Sand (NS) and Ordinary Portland Cement (OPC) by weight. One control mix, one with GBFS, three with FA and three with GBFS-FA combined mixes were prepared. Replacements were 50% GBFS with NS and 20%, 30% and 40% FA with OPC. Preliminary investigation on development of compressive strength was carried out at 7, 28 and 90 days to ensure sustainability of waste materials in concrete matrix at room temperature. After 90days, thermo-mechanical study was performed on the specimen for a temperature regime of 200 degrees-1000 degrees C followed by furnace cooling. Weight loss, visual inspection along with colour change, residual compressive strength and microstructure analysis were performed to investigate the effect of replacement of GBFS and FA. Although adding waste mineral by-products enhanced the weight loss, their pozzolanicity and formation history at high temperature played a significant role in retaining higher residual compressive strength even up to 800 degrees C. On detail microstructural study, it has been found that addition of FA and GBFS in concrete mix improved the density of concrete by development of extra calcium silicate gel before fire and restricts the development of micro-cracks at high temperature as well. In general, the authors are in favour of combined replacement mix in view of high volume mineral by-products utilization as fire protection.
引用
收藏
页码:263 / 275
页数:13
相关论文
共 83 条
[21]   Effects of non-ground slag and bottom ash as fine aggregate on concrete permeability properties [J].
Bilir, Turhan .
CONSTRUCTION AND BUILDING MATERIALS, 2012, 26 (01) :730-734
[22]   Performance of ground blast furnace slag and ground basaltic pumice concrete against seawater attack [J].
Binici, Hanifi ;
Aksogan, Orhan ;
Gorur, Ela Bahsude ;
Kaplan, Hasan ;
Bodur, Mehmet Nuri .
CONSTRUCTION AND BUILDING MATERIALS, 2008, 22 (07) :1515-1526
[23]  
bis, 2009, IS 10262
[24]   Residual strength and pore structure of high-strength concrete and normal strength concrete after exposure to high temperatures [J].
Chan, YN ;
Peng, GF ;
Anson, M .
CEMENT & CONCRETE COMPOSITES, 1999, 21 (01) :23-27
[25]   Compressive strength and pore structure of high-performance concrete after exposure to high temperature up to 800°C [J].
Chan, YN ;
Luo, X ;
Sun, W .
CEMENT AND CONCRETE RESEARCH, 2000, 30 (02) :247-251
[26]   Compressive behavior of steel fiber reinforced recycled aggregate concrete after exposure to elevated temperatures [J].
Chen, G. M. ;
He, Y. H. ;
Yang, H. ;
Chen, J. F. ;
Guo, Y. C. .
CONSTRUCTION AND BUILDING MATERIALS, 2014, 71 :1-15
[27]   Influence of GGBS on durability and corrosion behavior of reinforced concrete [J].
Cheng, A ;
Huang, R ;
Wu, JK ;
Chen, CH .
MATERIALS CHEMISTRY AND PHYSICS, 2005, 93 (2-3) :404-411
[28]   Stress-strain curves for high strength concrete at elevated temperatures [J].
Cheng, FP ;
Kodur, VKR ;
Wang, TC .
JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2004, 16 (01) :84-90
[29]   Residual strength of concrete containing recycled materials after exposure to fire: A review [J].
Cree, D. ;
Green, M. ;
Noumowe, A. .
CONSTRUCTION AND BUILDING MATERIALS, 2013, 45 :208-223
[30]  
Dash Manoj Kumar, 2016, International Journal of Sustainable Built Environment, V5, P484, DOI 10.1016/j.ijsbe.2016.04.006