Cyclic deformation of dissimilar welded joints between Ti-6Al-4V and Ti17 alloys: Effect of strain ratio

被引:29
|
作者
Wang, S. Q. [1 ,2 ]
Liu, J. H. [1 ]
Lu, Z. X. [3 ]
Chen, D. L. [2 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
[2] Ryerson Univ, Dept Mech & Ind Engn, Toronto, ON M5B 2K3, Canada
[3] Xian Univ Technol, Dept Mat Sci & Engn, Xian 710048, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2014年 / 598卷
基金
加拿大创新基金会; 加拿大自然科学与工程研究理事会;
关键词
Titanium alloy; Electron beam welding; Dissimilar welded joints; Fatigue; Cyclic deformation; Strain ratio; EXTRUDED MAGNESIUM ALLOY; DUAL-PHASE STEEL; ELECTRON-BEAM; FATIGUE PROPERTIES; MECHANICAL-PROPERTIES; TITANIUM-ALLOYS; STAINLESS-STEEL; RARE-EARTH; BEHAVIOR; MICROSTRUCTURE;
D O I
10.1016/j.msea.2014.01.022
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Cyclic deformation characteristics of electron beam welded (EBWed) joints between Ti-6Al-4V and Ti17 (Ti-5Al-4Mo-4Cr-2Sn-2Zr) titanium alloys were evaluated via strain-controlled low-cycle fatigue tests at varying strain ratios at a constant strain amplitude. The welding led to a significant microstructural change across the dissimilar joint, with hexagonal close-packed (HCP) martensite alpha' and orthorhombic martensite alpha '' in the fusion zone (FZ), alpha' in the heat-affected zone (HAZ) of Ti-6A1-4V side, and coarse beta in the HAZ of Ti17 side. A distinctive asymmetrical hardness profile across the joint was observed with the highest hardness in the FZ and a lower hardness in the HAZ of Ti17 side than in the Ti17 base metal (BM), indicating the presence of soft zone. The strength and ductility of the dissimilar joint lay in-between those of two base metals (BMs). Unlike wrought magnesium alloys, the Ti-6A1-4V BM, Ti17 BM, and joint basically exhibited symmetrical hysteresis loops in tension and compression in the fully reversed strain-controlled tests at a strain ratio of R-epsilon = -1. At a strain ratio of R-epsilon=0 and 0.5, a large amount of plastic deformation occurred in the ascending phase of the first cycle of hysteresis loops of Ti-6A1-4V BM, Ti17 BM, and joint due to the high positive mean strain values. Fatigue life of the joint was observed to be the longest at R-epsilon = -1, and it decreased as the strain ratio deviated from R-epsilon = -1. A certain degree of mean stress relaxation was observed in the non-fully reversed strain controlled tests (i.e., R epsilon not equal -1). Fatigue failure of the dissimilar joints occurred in the Ti-6A1-4V BM, with crack initiation from the specimen surface or near-surface defect and crack propagation characterized by fatigue striations. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:122 / 134
页数:13
相关论文
共 50 条
  • [31] Deformation twinning in Ti-6Al-4V during low strain rate deformation to moderate strains at room temperature
    Prakash, D. G. Leo
    Ding, R.
    Moat, R. J.
    Jones, I.
    Withers, P. J.
    da Fonseca, J. Quinta
    Preuss, M.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (21-22): : 5734 - 5744
  • [32] Forming and tensile fracture characteristics of Ti-6Al-4V and T2 Cu vacuum electron beam welded joints
    Guo, Shun
    Peng, Yong
    Cui, Chong
    Zhou, Qi
    Xu, Junqiang
    Zhu, Jun
    VACUUM, 2019, 165 (311-319) : 311 - 319
  • [33] A comparative study on dynamic deformation and ballistic impact response of Ti-4Al-2.5V-1.5Fe-0.25O and Ti-6Al-4V alloys
    Sukumar, G.
    Patra, Achintya Kumar
    Kumar, Amit
    Thakur, Rakesh Kumar
    Singh, B. Bhav
    Bhattacharjee, Amit
    Sarma, V. Subramanya
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 889
  • [34] Impact toughness and fracture analysis of linear friction welded Ti-6Al-4V alloy joints
    Ma, T. J.
    Li, W. -Y.
    Yang, S. Y.
    MATERIALS & DESIGN, 2009, 30 (06) : 2128 - 2132
  • [35] Effect of deformation temperature on mechanical properties, microstructure, and springback of Ti-6Al-4V sheets
    Ertan, Rukiye
    Cetin, Guner
    REVISTA DE METALURGIA, 2021, 57 (04)
  • [36] Ti-6Al-4V welded joints via electron beam welding: Microstructure, fatigue properties, and fracture behavior
    Yang, Xiaoguang
    Li, Shaolin
    Qi, Hongyu
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 597 : 225 - 231
  • [37] Effect of Base Material on Microstructure and Texture Evolution of a Ti-6Al-4V Electron-Beam Welded Joint
    Wang, G. Q.
    Zhao, Z. B.
    Yu, B. B.
    Liu, J. R.
    Wang, Q. J.
    Zhang, J. H.
    Yang, R.
    Li, J. W.
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2017, 30 (05) : 499 - 504
  • [38] Microstructure evolution of electron beam welded joints of Ti-43Al-9V-0.3Y and Ti-6Al-4V alloys
    Chen, Guoqing
    Zhang, Ge
    Yin, Qianxing
    Zhang, Binggang
    Feng, Jicai
    MATERIALS LETTERS, 2018, 233 : 336 - 339
  • [39] Corrosion mechanism of the Ti-6Al-4V/AA6061 dissimilar metal CMT welded joint
    Xu, Hao
    Cao, Rui
    Ma, Xianglong
    Yan, Yingjie
    Fan, Ding
    Dong, Hongbiao
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2025, 35 : 6951 - 6964
  • [40] The effect of post-weld heat treatment on the notched tensile fracture of Ti-6Al-4V to Ti-6Al-6V-2Sn dissimilar laser welds
    Hsieh, C. T.
    Chu, C. Y.
    Shiue, R. K.
    Tsay, L. W.
    MATERIALS & DESIGN, 2014, 59 : 227 - 232