Cyclic deformation of dissimilar welded joints between Ti-6Al-4V and Ti17 alloys: Effect of strain ratio

被引:29
作者
Wang, S. Q. [1 ,2 ]
Liu, J. H. [1 ]
Lu, Z. X. [3 ]
Chen, D. L. [2 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
[2] Ryerson Univ, Dept Mech & Ind Engn, Toronto, ON M5B 2K3, Canada
[3] Xian Univ Technol, Dept Mat Sci & Engn, Xian 710048, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2014年 / 598卷
基金
加拿大自然科学与工程研究理事会; 加拿大创新基金会;
关键词
Titanium alloy; Electron beam welding; Dissimilar welded joints; Fatigue; Cyclic deformation; Strain ratio; EXTRUDED MAGNESIUM ALLOY; DUAL-PHASE STEEL; ELECTRON-BEAM; FATIGUE PROPERTIES; MECHANICAL-PROPERTIES; TITANIUM-ALLOYS; STAINLESS-STEEL; RARE-EARTH; BEHAVIOR; MICROSTRUCTURE;
D O I
10.1016/j.msea.2014.01.022
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Cyclic deformation characteristics of electron beam welded (EBWed) joints between Ti-6Al-4V and Ti17 (Ti-5Al-4Mo-4Cr-2Sn-2Zr) titanium alloys were evaluated via strain-controlled low-cycle fatigue tests at varying strain ratios at a constant strain amplitude. The welding led to a significant microstructural change across the dissimilar joint, with hexagonal close-packed (HCP) martensite alpha' and orthorhombic martensite alpha '' in the fusion zone (FZ), alpha' in the heat-affected zone (HAZ) of Ti-6A1-4V side, and coarse beta in the HAZ of Ti17 side. A distinctive asymmetrical hardness profile across the joint was observed with the highest hardness in the FZ and a lower hardness in the HAZ of Ti17 side than in the Ti17 base metal (BM), indicating the presence of soft zone. The strength and ductility of the dissimilar joint lay in-between those of two base metals (BMs). Unlike wrought magnesium alloys, the Ti-6A1-4V BM, Ti17 BM, and joint basically exhibited symmetrical hysteresis loops in tension and compression in the fully reversed strain-controlled tests at a strain ratio of R-epsilon = -1. At a strain ratio of R-epsilon=0 and 0.5, a large amount of plastic deformation occurred in the ascending phase of the first cycle of hysteresis loops of Ti-6A1-4V BM, Ti17 BM, and joint due to the high positive mean strain values. Fatigue life of the joint was observed to be the longest at R-epsilon = -1, and it decreased as the strain ratio deviated from R-epsilon = -1. A certain degree of mean stress relaxation was observed in the non-fully reversed strain controlled tests (i.e., R epsilon not equal -1). Fatigue failure of the dissimilar joints occurred in the Ti-6A1-4V BM, with crack initiation from the specimen surface or near-surface defect and crack propagation characterized by fatigue striations. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:122 / 134
页数:13
相关论文
共 74 条
[1]   Investigation of the weldability of titanium alloys produced by different methods of melting [J].
Akhonin, S. V. ;
Mishchenko, R. N. ;
Petrichenko, I. K. .
MATERIALS SCIENCE, 2006, 42 (03) :323-329
[2]   Fatigue behavior of tailor (laser)-welded blanks for automotive applications [J].
Anand, D ;
Chen, DL ;
Bhole, SD ;
Andreychuk, P ;
Boudreau, G .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 420 (1-2) :199-207
[3]   ADVANCED MATERIALS FOR AIRCRAFT ENGINE APPLICATIONS [J].
BACKMAN, DG ;
WILLIAMS, JC .
SCIENCE, 1992, 255 (5048) :1082-1087
[4]   CHARACTERIZATION OF THE WELD HEAT-AFFECTED ZONE IN AN ALPHA-2 TITANIUM ALUMINIDE [J].
BAESLACK, WA ;
PHILLIPS, D ;
SCARR, GK .
MATERIALS CHARACTERIZATION, 1992, 28 (01) :61-73
[5]   Fatigue Performance of Gas Tungsten Arc, Electron Beam, and Laser Beam Welded Ti-6Al-4V Alloy Joints [J].
Balasubramanian, T. S. ;
Balasubramanian, V. ;
Muthumanikkam, M. A. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2011, 20 (09) :1620-1630
[6]   The role of microtexture on the faceted fracture morphology in Ti-6Al-4V subjected to high-cycle fatigue [J].
Bantounas, Ioannis ;
Dye, David ;
Lindley, Trevor C. .
ACTA MATERIALIA, 2010, 58 (11) :3908-3918
[7]   The effect of grain orientation on fracture morphology during high-cycle fatigue of Ti-6Al-4V [J].
Bantounas, Ioannis ;
Dye, David ;
Lindley, Trevor C. .
ACTA MATERIALIA, 2009, 57 (12) :3584-3595
[8]   Low cycle fatigue properties of an extruded AZ31 magnesium alloy [J].
Begum, S. ;
Chen, D. L. ;
Xu, S. ;
Luo, Alan A. .
INTERNATIONAL JOURNAL OF FATIGUE, 2009, 31 (04) :726-735
[9]   Strain-Controlled Low-Cycle Fatigue Properties of a Newly Developed Extruded Magnesium Alloy [J].
Begum, S. ;
Chen, D. L. ;
Xu, S. ;
Luo, Alan A. .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2008, 39A (12) :3014-3026
[10]   Effect of strain ratio and strain rate on low cycle fatigue behavior of AZ31 wrought magnesium alloy [J].
Begum, S. ;
Chen, D. L. ;
Xu, S. ;
Luo, Alan A. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 517 (1-2) :334-343