Study of Electrical, Mechanical, and Nanoscale Free-Volume Properties of NBR and EPDM Rubber Reinforced by Bentonite or Kaolin

被引:27
作者
El-Nashar, D. E. [2 ]
Gomaa, E. [1 ]
Abd-El-Messieh, S. L. [3 ]
机构
[1] Ain Shams Univ, Fac Sci, Dept Phys, Cairo 11566, Egypt
[2] Natl Res Ctr, Dept Polymer & Pigments, Cairo, Egypt
[3] Natl Res Ctr, Dept Microwave Phys & Dielect, Cairo, Egypt
关键词
blends; clay; crosslinking; dielectric properties; fillers; free-volume properties; hardness; rubber; POSITRON-ANNIHILATION SPECTROSCOPY; DIELECTRIC-RELAXATION; CARBON-BLACK; MICROSTRUCTURE; MONTMORILLONITE; NANOCOMPOSITES; LIFETIME; BLEND;
D O I
10.1002/polb.21765
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The effect of Na bentonite, Ca bentonite, and kaolin fillers on the macrostructure and microstructure of acrylonitrile butadiene rubber, ethylene propylene diene rubber, and their blend (50/50) was studied through electrical and mechanical measurements, as well as with positron annihilation lifetime spectroscopy. The real part of permittivity (epsilon'), dielectric loss (epsilon ''), and the crosslinking density were found to increase with increasing filler content. The increase of crosslinking density of the blend with increasing amount of fillers reflects a decrease in the equilibrium swelling up to 21.50 wt % compared with that of the unfilled blends. The mechanical investigation showed pronounced increase in the tensile strength, and in elongation at break with the addition of up to 21.50 wt % of filler. In addition, comparing between different fillers showed that the reinforcing effect of Na bentonite is more effective than Ca bentonite and kaolin but the physico-mechanical of Ca bentonite is less than that for kaolin. The positron annihilation lifetime measurements revealed that the free-volume properties were strongly affected by the amount and type of filler, in particular, the free-volume fraction was dramatically decreased with increasing filler content. Furthermore, correlations were made between the free-volume parameters and both electrical and mechanical properties. (C) 2009 Wiley Periodicals, Inc. J Polym Sci Part 13: Polym Phys 47: 1825-1838, 2009
引用
收藏
页码:1825 / 1838
页数:14
相关论文
共 35 条
[1]   Compatibility investigation of microwave irradiated acrylonitrile butadiene/ethylene propylene diene rubber blends [J].
Abd-El-Messieh, SL ;
El-Nashar, DE ;
Khafagi, MG .
POLYMER-PLASTICS TECHNOLOGY AND ENGINEERING, 2004, 43 (01) :135-158
[2]   Effect of curing time and sulfur content on the dielectric relaxation of styrene butadiene rubber [J].
Abd-El-Messieh, SL ;
Abd-El-Nour, KN .
JOURNAL OF APPLIED POLYMER SCIENCE, 2003, 88 (07) :1613-1621
[3]  
AbdelMessieh SL, 1996, J APPL POLYM SCI, V62, P805, DOI 10.1002/(SICI)1097-4628(19961031)62:5<805::AID-APP13>3.0.CO
[4]  
2-R
[5]  
Ahmadi SJ, 2004, IRAN POLYM J, V13, P415
[6]   Organo-montmorillonite as substitute of carbon black in natural rubber compounds [J].
Arroyo, M ;
López-Manchado, MA ;
Herrero, B .
POLYMER, 2003, 44 (08) :2447-2453
[7]  
Bishai A.M., 2002, INT J POLYM MATER, V51, P793
[8]  
BRANDRUP J, 1967, POLYM HDB
[9]   The use of montmorillonite as a reinforcing and compatibilizing filler for NBR/SBR rubber blend [J].
Essawy, H ;
El-Nashar, D .
POLYMER TESTING, 2004, 23 (07) :803-807
[10]  
EVANS LR, 2001, RUBBER WORLD, V224, P18