Continuous monitoring of thermooxidative degradation products of polystyrene by membrane extraction with sorbent interface and gas chromatography

被引:18
作者
Ciucanu, I [1 ]
Kaykhaii, M [1 ]
Montero, L [1 ]
Pawliszyn, J [1 ]
Szubra, J [1 ]
机构
[1] Univ Waterloo, Dept Chem, Waterloo, ON N2L 3G1, Canada
关键词
D O I
10.1093/chromsci/40.6.350
中图分类号
Q5 [生物化学];
学科分类号
071010 ; 081704 ;
摘要
A novel method for the continuous monitoring of thermooxidative degradation products of polystyrene by membrane extraction with sorbent interface (MESI) and gas chromatography (GC) is developed. The results are compared with solid-phase microextraction-GC, which can extract gases, vapors, and aerosols. The volatile and semivolatile degradation products are identified by mass spectrometry. The membrane used in the MESI-GC analysis shows a high permeation for volatile aromatic hydrocarbons; a low permeation for corresponding volatile aldehydes; and no permeation for less volatile alcohols, acids, and degradation products with a high molecular weight, thus reducing significantly the number of compounds detected from MESI-GC. Sensitivity of the method depends on the time of trapping, which is limited by the breakthrough of the trap. By heating the trap at fixed intervals of time, consecutive gas chromatograms are obtained.
引用
收藏
页码:350 / 354
页数:5
相关论文
共 18 条
[1]   POLYSTYRENE DEGRADATION DURING COMBUSTION [J].
BRAUMAN, SK ;
CHEN, IJ ;
MATZINGER, DP .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 1983, 21 (06) :1831-1845
[2]  
CAMERON GG, 1967, J MACROMOL SCI, V1, P327
[3]   WEAK LINKS IN POLYSTYRENE [J].
CHIANTORE, O ;
CAMINO, G ;
COSTA, L .
POLYMER DEGRADATION AND STABILITY, 1981, 3 (03) :209-219
[4]   Design of continuous-monitoring device based on membrane extraction with sorbent interface and micro-gas chromatograph [J].
Ciucanu, I ;
Pawliszyn, J .
FIELD ANALYTICAL CHEMISTRY AND TECHNOLOGY, 2001, 5 (1-2) :69-74
[5]   THE EFFECT OF THE CHEMICAL-STRUCTURE OF CHAIN ENDS ON THE THERMAL-DEGRADATION OF POLYSTYRENE [J].
COSTA, L ;
CAMINO, G ;
GUYOT, A ;
BERT, M ;
CLOUET, G ;
BROSSAS, J .
POLYMER DEGRADATION AND STABILITY, 1986, 14 (01) :85-93
[6]   STYRENE MONOMER MIGRATION AS MONITORED BY PURGE AND TRAP GAS-CHROMATOGRAPHY AND SENSORY ANALYSIS FOR POLYSTYRENE CONTAINERS [J].
DURST, GL ;
LAPERLE, EA .
JOURNAL OF FOOD SCIENCE, 1990, 55 (02) :522-524
[7]  
HARPER M, 1999, J CHROMATOGR A, V833, P111
[8]   THERMAL-DEGRADATION OF STYRENE BUTADIENE DIBLOCK COPOLYMER .1. CHARACTERISTICS OF POLYSTYRENE AND POLYBUTADIENE DEGRADATION [J].
MCNEILL, IC ;
STEVENSON, WTK .
POLYMER DEGRADATION AND STABILITY, 1985, 10 (03) :247-265
[9]   A DETAILED INVESTIGATION OF THE PRODUCTS OF THE THERMAL-DEGRADATION OF POLYSTYRENE [J].
MCNEILL, IC ;
ZULFIQAR, M ;
KOUSAR, T .
POLYMER DEGRADATION AND STABILITY, 1990, 28 (02) :131-151
[10]  
Nerin C, 1998, FOOD ADDIT CONTAM A, V15, P346, DOI 10.1080/02652039809374650