Influence of loading frequency on implant failure under cyclic fatigue conditions

被引:65
作者
Karl, Matthias [2 ]
Kelly, J. Robert [1 ]
机构
[1] Univ Connecticut, Ctr Hlth, Dept Reconstruct Sci, Farmington, CT 06030 USA
[2] Univ Erlangen Nurnberg, Dept Prosthodont, Erlangen, Germany
关键词
Dental implant; Fatigue testing; Strain rate; Strain; Loading frequency; TEMPERATURE; BEHAVIOR;
D O I
10.1016/j.dental.2009.06.015
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. Preliminary studies on implant fatigue testing suggested that fractures were more likely to occur at 2Hz than at 30 Hz (chi(2), p < 0.05). This investigation explores frequency and base elastic modulus effects on strain, strain rate and failure. Methods. A total of 66 implants were mounted in different base materials (acrylic, glass. filled epoxy, aluminum) and loaded up to 106 cycles per ISO 14801 (20N to 420-500 N) at frequencies of 2Hz and 30 Hz (chosen to accelerate frequency as the stressor). Absolute strain magnitudes and strain rates under varying loading conditions and with different base materials were measured using one strain-gauged implant. Failure probability distributions were analyzed by both Weibull and life data analysis. Measured strain was used to validate an FEA model. Fracture surfaces were examined by SEM. Results. Number of failures and failure-rates-per-cycle differed significantly between implants tested at 2Hz versus 30 Hz (p < 0.05). Strain magnitude was independent of frequency. Strain rates were highly correlated with frequency (linear r(2) > 0.99) and differed significantly under failure conditions (420 N): 2Hz = 8292 mu strain/s; (500 N): 30 Hz = 80,840 mu strain/s. Measured and FEA-calculated strains were similar. Fracture surfaces were indistinguishable (2Hz versus 30 Hz). Significance. Fatigue failure was significantly more likely at 2 Hz than 30 Hz whereas base material and loading magnitude seemed to have only minor influence. Absolute strain was identical at these frequencies suggesting strain rate sensitivity for this commercially pure titanium implant. Both the Weibull and SEM analyses support an identical failure mechanism with damage accumulation more severe at lower frequencies, an interpretation consistent with strain rate sensitivity. (C) 2009 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:1426 / 1432
页数:7
相关论文
共 19 条
[1]  
ADELL R, 1990, International Journal of Oral and Maxillofacial Implants, V5, P347
[2]  
ALBRECHT J, 1999, MAT SCI ENG A-STRUCT, V263, P168
[3]  
Balshi T J, 1996, Int J Oral Maxillofac Implants, V11, P660
[4]   A dislocation-based constitutive law for pure Zr including temperature effects [J].
Beyerlein, I. J. ;
Tome, C. N. .
INTERNATIONAL JOURNAL OF PLASTICITY, 2008, 24 (05) :867-895
[5]   Fractures related to occlusal overload with single posterior implants: A clinical report [J].
Conrad, Heather J. ;
Schulte, John K. ;
Vallee, Mark C. .
JOURNAL OF PROSTHETIC DENTISTRY, 2008, 99 (04) :251-256
[6]   JAW MOVEMENTS IN YOUNG-ADULT MEN DURING CHEWING [J].
GILLINGS, BR ;
GRAHAM, CH ;
DUCKMANTON, NA .
JOURNAL OF PROSTHETIC DENTISTRY, 1973, 29 (06) :616-627
[7]   Natural bites, food consistency and feeding behaviour in man [J].
Hiiemae, K ;
Heath, MR ;
Heath, G ;
Kazazoglu, E ;
Murray, J ;
Sapper, D ;
Hamblett, K .
ARCHIVES OF ORAL BIOLOGY, 1996, 41 (02) :175-189
[8]  
Jemt T, 1993, Int J Oral Maxillofac Implants, V8, P635
[9]   A systematic review of the 5-year survival and complication rates of implant-supported single crowns [J].
Jung, Ronald E. ;
Pjetursson, Bjarni E. ;
Glauser, Roland ;
Zembic, Anja ;
Zwahlen, Marcel ;
Lang, Niklaus P. .
CLINICAL ORAL IMPLANTS RESEARCH, 2008, 19 (02) :119-130
[10]   Evaluation of test protocol variables for dental implant fatigue research [J].
Lee, Cornell K. ;
Karl, Matthias ;
Kelly, J. Robert .
DENTAL MATERIALS, 2009, 25 (11) :1419-1425