Mechanism of toughening for polypropylene blended with ethylene-propylene-diene rubber following selective crosslinking

被引:0
|
作者
Ishikawa, M [1 ]
Sugimoto, M [1 ]
Inoune, T [1 ]
机构
[1] NIPPON PETROCHEM CO LTD,PLAST LAB,KAWASAKI KU,KAWASAKI,KANAGAWA 210,JAPAN
关键词
UNSATURATED ELASTOMER BLENDS; INJECTION-MOLDED SAMPLES; DEFORMATION MECHANISMS; MOLECULAR-STRUCTURE; POLYOLEFIN BLENDS; IMPACT PROPERTIES; POLYMER BLENDS; MELT RHEOLOGY; CROSS-LINKING; MORPHOLOGY;
D O I
10.1002/(SICI)1097-4628(19961205)62:10<1495::AID-APP1>3.3.CO;2-9
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Toughening mechanism of polypropylene (PP) blended with ethylene-propylene-diene rubber (EPDM) following selective crosslinking was examined in comparison with that of blends of PP before crosslinking. The yield stress, strength of craze, and density of void which are dominant factors for enhancing toughness in PP blends were evaluated and the deformation and fracture mechanism was discussed. It was concluded that toughness of PP blended with EPDM is improved by selective crosslinking, since the improvement of the craze strength is greater than the drop in the release of the constraint of strain. (C) 1996 John Wiley & Sons, Inc.
引用
收藏
页码:1495 / 1502
页数:8
相关论文
共 50 条
  • [21] Dynamically Vulcanized EPDM (Ethylene-Propylene-Diene Polymer)/PP(Polypropylene) Polymer Blend: Performance Index (PI)
    Tasdemir, Munir
    Topsakaloglu, Murat
    Caneba, Gerard T.
    JOURNAL OF POLYMER MATERIALS, 2010, 27 (04): : 337 - 349
  • [22] Effect of Complex Curatives on the Properties for Ethylene Propylene Diene Rubber/Polypropylene Blends
    Tsai, Yuhsin
    Tsai, Ping-Yuan
    Wu, Yao-Tsu
    Leu, Ming-Tsong
    Wu, Jyh-Horng
    JOURNAL OF ELASTOMERS AND PLASTICS, 2009, 41 (03): : 209 - 221
  • [23] Carbon nanotubes induced brittle-ductile transition behavior of the polypropylene/ethylene-propylene-diene terpolymer blends
    Yang, Chao-jin
    Huang, Ting
    Yang, Jing-hui
    Zhang, Nan
    Wang, Yong
    Zhou, Zuo-wan
    COMPOSITES SCIENCE AND TECHNOLOGY, 2017, 139 : 109 - 116
  • [24] Impact Modification of Isotactic Polypropylene with Ethylene-Propylene Diene Monomer Rubber
    Banerjee, J.
    Soliya, P.
    Pallavi, M. B.
    Mukhopadhyay, P.
    Bandyopadhyay, S.
    Chakrabarty, D.
    Dutta, K.
    INTERNATIONAL POLYMER PROCESSING, 2016, 31 (02) : 188 - 197
  • [25] Shear-induced crystallization in phase-separated blends of isotactic polypropylene with ethylene-propylene-diene terpolymer
    Ma, Gui-qiu
    Li, Da
    Sheng, Jing
    CHINESE JOURNAL OF POLYMER SCIENCE, 2015, 33 (11) : 1538 - 1549
  • [26] Analysis and optimization of polypropylene (PP)ethylene-propylene-diene monomer (EPDM)/scrap rubber tire (SRT) mixtures using RSM methodology
    da Costa, H. M.
    Ramos, V. D.
    da Silva, W. S.
    Sirqueira, A. S.
    POLYMER TESTING, 2010, 29 (05) : 572 - 578
  • [27] A novel chemical technique for compatibility of ethylene-propylene-diene monomer rubber and styrene-butadiene rubber in their blends
    Estagy, Sara
    Movahed, Saeed Ostad
    Yazdanbakhsh, Soheil
    Nezhad, Majid Karim
    JOURNAL OF ELASTOMERS AND PLASTICS, 2017, 49 (04): : 298 - 314
  • [28] A type of shape memory material based on ethylene-propylene-diene rubber (EPDM)/ polypropylene (PP) thermoplastic vulcanizates compatibilized by magnesium maleate
    Xu, Mengmeng
    Zong, Yingxia
    Zong, Chengzhong
    POLYMER, 2023, 285
  • [29] In situ reactive compatibilization and reinforcement of peroxide dynamically vulcanized polypropylene/ethylene-propylene-diene monomer tpv by zinc dimethacrylate
    Cao, Liming
    Cao, Xiaodong
    Jiang, Xiujuan
    Xu, Chuanhui
    Chen, Yukun
    POLYMER COMPOSITES, 2013, 34 (08) : 1357 - 1366
  • [30] Effect of blend ratio on the phase structure and ozone aging resistance of ethylene-propylene-diene, butyl, and chlorobutyl rubber blends
    Sukharev, Nikita
    Sukhareva, Ksenia
    Karpova, Svetlana
    Mamin, Eldar
    Popov, Anatoly
    Niu, Yanhui
    Ai, Tao
    POLYMER-PLASTICS TECHNOLOGY AND MATERIALS, 2024, 63 (04): : 432 - 446