Extending the Induction Period of Crystallization Fouling Through Surface Coating

被引:41
作者
Geddert, T. [1 ]
Bialuch, I. [2 ]
Augustin, W. [1 ]
Scholl, S. [1 ]
机构
[1] Tech Univ Carolo Wilhelmina Braunschweig, Inst Chem & Thermal Proc Engn, D-38106 Braunschweig, Germany
[2] Fraunhofer Inst Surface Engn & Thin Films, Braunschweig, Germany
关键词
ADHESION;
D O I
10.1080/01457630902753789
中图分类号
O414.1 [热力学];
学科分类号
摘要
To minimize the negative effects of scale formation in heat exchangers, new anti-fouling strategies are focusing on the modification of heat transfer surfaces. These modifications should lead to tailor-made surfaces for different technical applications. The aim of this surface modification is the extension of the induction period to minimize the negative effects of fouling and maximize the endurance of the heat exchanger. To achieve this, different surface coatings on stainless steel were investigated with respect to fouling tendency. The effects of flow velocity with respect to Reynolds number on the induction time of CaSO4 crystallization fouling were tested in different test units. Diamond-like carbon (DLC) coatings extend the induction time at every measured flow velocity. At higher Reynolds numbers, the effect of different surface crystallization due to energetic modification is reduced because of the dominating effect of the low adhesive surface. Thus the induction time can be extended by the factor of 2 for low fluid velocities (DLC or SICON) and by more than 14 for higher Reynolds numbers (DLC and SICON). The combination of limited nucleation spots due to electro-chemical treatment of the substrate before coating can give a tailor-made surface with maximum induction time for crystallization fouling.
引用
收藏
页码:868 / 875
页数:8
相关论文
共 7 条
[1]  
BEWILOGUA K, 2002, MODERN PLASMA SURFAC, P45
[2]  
Bhushan B., 2004, SPRINGER HDB NANOTEC
[3]  
DYCKERHOFF GA, 1972, ANGEW MAKROMOL CHEM, V21, P169
[4]   Modification of molecular interactions at the interface crystal/heat transfer surface to minimize heat exchanger fouling [J].
Förster, M ;
Bohnet, M .
INTERNATIONAL JOURNAL OF THERMAL SCIENCES, 2000, 39 (07) :697-708
[5]   Influence of the adhesion force crystal/heat exchanger surface on fouling mitigation [J].
Förster, M ;
Augustin, W ;
Bohnet, M .
CHEMICAL ENGINEERING AND PROCESSING-PROCESS INTENSIFICATION, 1999, 38 (4-6) :449-461
[6]   NETWORK MODIFICATION OF DLC COATINGS TO ADJUST A DEFINED SURFACE-ENERGY [J].
TROJAN, K ;
GRISCHKE, M ;
DIMIGEN, H .
PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, 1994, 145 (02) :575-585
[7]   Influence of surface properties and characteristics on fouling in plate heat exchangers [J].
Zettler, HU ;
Weiss, M ;
Zhao, Q ;
Müller-Steinhagen, H .
HEAT TRANSFER ENGINEERING, 2005, 26 (02) :3-17