Effect of T6 Heat Treatment on Dry Sliding Frictional Wear Characteristics of Al-20Si-5Cu Alloy

被引:1
作者
Jin, Yunxue [1 ]
Tong, Qiangqiang [1 ]
Wang, Xiaoya [1 ]
Chen, Hongmei [1 ]
机构
[1] Jiangsu Univ Sci & Technol, Prov Key Lab Adv Welding Technol, Zhenjiang 212003, Peoples R China
来源
ADVANCED ENGINEERING MATERIALS III, PTS 1-3 | 2013年 / 750-752卷
关键词
hypereutectic Al-Si alloy; brake disc; T6 heat treatment; frictional wear; wear mechanism;
D O I
10.4028/www.scientific.net/AMR.750-752.591
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of T6 heat treatment on dry sliding friction and wear characteristics of Al-20Si-5Cu under a fixed sliding speed of 200r/min and sliding time of 30mins was illustrated in this paper. The result reveals that T6 heat treatment can improve morphology of primary Si and Al2Cu particles, enhance the hardness of the matrix. Wear rate increased with increasing of applied load. T6 heat treated samples have high wear resistance which is related to the improvement of microstructure, particularly with their increased hardness of matrix. But friction coefficient varies with heat treatment processes and has no sensitivity to applied loads, which fluctuates in a small range, so the friction coefficient can be considered to be stable. The wear mechanisms of T6 heat treated samples are also changed with increasing of applied load, from oxidative wear to fatigue wear.
引用
收藏
页码:591 / 595
页数:5
相关论文
共 16 条
  • [1] Dry Sliding Friction Wear Characteristics of T6 Treated Al-20Si-5Cu Alloy
    Jin Yunxue
    Tong Qiangqiang
    Wang Xiaoya
    RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (06) : 1352 - 1356
  • [2] Dry Sliding Friction and Wear Characteristics of T6 Treated Al-10Si-5Cu-0.75Mg Alloy
    Liu Guanglei
    Li Yushan
    Li Chao
    Zhao Guoshi
    Si Naichao
    RARE METAL MATERIALS AND ENGINEERING, 2019, 48 (02) : 620 - 625
  • [3] Wear of spray deposited Al-6Cu-Mn alloy under dry sliding conditions
    Gui, MC
    Kang, SB
    Lee, JM
    WEAR, 2000, 240 (1-2) : 186 - 198
  • [4] Influence of Sn content on the microstructure and dry sliding wear behaviour of hypereutectic Al-20Si alloy
    Wu, X. F.
    Zhang, G. A.
    MATERIALS AND MANUFACTURING, PTS 1 AND 2, 2011, 299-300 : 265 - +
  • [5] Dry sliding friction and wear properties of Al-25Zn-3Cu-3Si alloy
    Savaskan, Temel
    Bican, Osman
    TRIBOLOGY INTERNATIONAL, 2010, 43 (08) : 1346 - 1352
  • [6] Wear Characteristics of Dry Sliding Friction between the T6 Treated A356/SiC Composite and Semi-metallic Pad
    Jin Yunxue
    Lee, Jung-Moo
    Kang, Suk-Bong
    RARE METAL MATERIALS AND ENGINEERING, 2008, 37 (12) : 2147 - 2151
  • [7] High-Temperature Dry Sliding Friction and Wear Characteristics of T6 Treated SiCp/A356 Composite
    Jin Yunxue
    Wang Xiaoya
    Tong Qiangqiang
    Lee, Jung-Moo
    RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (10) : 2497 - 2501
  • [8] The influence of T6 treatment on fracture behavior of hypereutectic Al-Si HPDC casting alloy
    Yu, Wenbo
    Zhao, Hongbin
    Wang, Lei
    Guo, Zhipeng
    Xiong, Shoumei
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 731 : 444 - 451
  • [9] Effect of Microstructural Variation on Dry Sliding Wear Behavior of Ti-6Al-4V Alloy
    Sahoo, R.
    Jha, B. B.
    Sahoo, T. K.
    Sahoo, D.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2014, 23 (06) : 2092 - 2102
  • [10] Effect of Microstructural Variation on Dry Sliding Wear Behavior of Ti-6Al-4V Alloy
    R. Sahoo
    B. B. Jha
    T. K. Sahoo
    D. Sahoo
    Journal of Materials Engineering and Performance, 2014, 23 : 2092 - 2102