Effect of surface mechanical attrition treatment on corrosion resistance of commercial pure titanium

被引:67
作者
Fu, Tianlin [1 ]
Zhan, Zhaolin [1 ]
Zhang, Ling [1 ]
Yang, Yanrong [1 ]
Liu, Zhong [1 ]
Liu, Jianxiong [1 ]
Li, Li [1 ]
Yu, Xiaohua [1 ]
机构
[1] Kunming Univ Sci & Technol, Fac Mat Sci & Engn, Kunming 550093, Peoples R China
关键词
Titanium; EIS; Polarization; Repassivadon; Passive films; IMMERSION ION-IMPLANTATION; TI-6AL-4V ALLOY; STAINLESS-STEEL; BIOMEDICAL APPLICATIONS; NITRIDE COATINGS; ANODIC-OXIDATION; BEHAVIOR; NANOCRYSTALLIZATION; TI; MICROSTRUCTURE;
D O I
10.1016/j.surfcoat.2015.08.041
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
We report on the effects of surface mechanical attrition treatment on the corrosion behavior of commercial pure titanium. The corrosion resistance before and after treatment were investigated by studying potentiodynamic polarization curves and by electrochemical impedance spectroscopy. The potentiodynamic polarization curves for a sample treated by surface mechanical attrition and for an untreated commercial pure titanium sample at room temperature showed that the corrosion potential of the former ranged from -1.11 to -1.06 V. whereas that of the latter was -1.23 V. The corrosion current density for the treated sample ranged from -5.02 x 10(-4) to -4.98 x 10(-4) A.cm(-2), and that for the untreated sample was -4.56 x 10(-4) A.cm(-2). A comparison of current densities at the same polarized potential showed a significant reduction in dissolution current of the treated sample. This indicates a lower corrosion rate for the sample treated by surface mechanical attrition. Surface mechanical attrition treatment was therefore confirmed to have beneficial impacts on corrosion behavior in 3.5 wt% NaCl solution. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:129 / 135
页数:7
相关论文
共 45 条
[21]   Anodic Oxidation of Ultra-Thin Ti Layers on ITO Substrates and their Application in Organic Electronic Memory Elements [J].
Heljo, P. S. ;
Wolff, K. ;
Lahtonen, K. ;
Valden, M. ;
Berger, P. R. ;
Majumdar, H. S. ;
Lupo, D. .
ELECTROCHIMICA ACTA, 2014, 137 :91-98
[22]   Photoelectrochemical analysis on the passive film formed on Ni in pH 8.5 buffer solution [J].
Jang, HJ ;
Park, CJ ;
Kwon, HS .
ELECTROCHIMICA ACTA, 2005, 50 (16-17) :3503-3508
[23]   Electrochemical and passive characterization of a beta type Ti45Zr38Al17 cast rod in nitric acid medium [J].
Jayaraj, J. ;
Shankar, A. Ravi ;
Mudali, U. Kamachi .
ELECTROCHIMICA ACTA, 2012, 85 :210-219
[24]   Effect of surface nanocrystallization on the corrosion behavior of Ti-6Al-4V titanium alloy [J].
Jelliti, S. ;
Richard, C. ;
Retraint, D. ;
Roland, T. ;
Chemkhi, M. ;
Demangel, C. .
SURFACE & COATINGS TECHNOLOGY, 2013, 224 :82-87
[25]   Effect of silicon on corrosion resistance of Ti-Si alloys [J].
Jiang, Zhonglin ;
Dai, Xin ;
Middleton, Hugh .
MATERIALS SCIENCE AND ENGINEERING B-ADVANCED FUNCTIONAL SOLID-STATE MATERIALS, 2011, 176 (01) :79-86
[26]   The formation mechanisms of surface nanocrystallites in β-type biomedical TiNbZrFe alloy by surface mechanical attrition treatment [J].
Jin, Lei ;
Cui, Wenfang ;
Song, Xiu ;
Zhou, Lian .
APPLIED SURFACE SCIENCE, 2015, 347 :553-560
[27]   Effects of surface nanocrystallization on corrosion resistance of β-type titanium alloy [J].
Jin, Lei ;
Cui, Wen-fang ;
Song, Xiu ;
Liu, Gang ;
Zhou, Lian .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2014, 24 (08) :2529-2535
[28]   Contribution to the elucidation of corrosion initiation through confocal laser scanning microscopy (CLSM) [J].
Leiva-Garcia, R. ;
Garcia-Anton, J. ;
Munoz-Portero, M. J. .
CORROSION SCIENCE, 2010, 52 (06) :2133-2142
[29]   Direct observation of thinmembrane passive filmover the growing pit on sputtered nanocrystalline austenitic stainless steel film [J].
Li, Tianshu ;
Liu, Li ;
Zhang, Bin ;
Li, Ying ;
Wang, Xiaolan ;
Wang, Fuhui .
ELECTROCHEMISTRY COMMUNICATIONS, 2015, 52 :80-84
[30]   The electrochemical corrosion behavior of TiN and (Ti,AI)N coatings in acid and salt solution [J].
Li, Y ;
Qu, L ;
Wang, FH .
CORROSION SCIENCE, 2003, 45 (07) :1367-1381