Improved Fracture Toughness and Crack Arrest Ability of Graphene-Alumina Nanocomposite

被引:4
作者
Akhil Raj, V. R. [1 ]
Hadagalli, Komalakrushna [1 ]
Jana, Premanshu [2 ]
Mandal, Saumen [1 ]
机构
[1] Natl Inst Technol Karnataka NITK, Dept Met & Mat Engn, Surathkal 575025, India
[2] Carborundum Universal Ltd, Electro Minerals Div, Kochi 683109, Kerala, India
关键词
boehmite; composite; fracture toughness; graphene-alumina; hardness; FEW-LAYER GRAPHENE; MECHANICAL-PROPERTIES; HYDROTHERMAL SYNTHESIS; GRAIN-SIZE; MICROSTRUCTURE; CERAMICS; BOEHMITE;
D O I
10.1007/s11665-020-05433-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this work, high fracture toughness graphene-alumina composite was developed through a novel chemical method using boehmite and graphene, which is followed by extrusion and consolidation. The mixed precursors were consolidated by sintering at 1550 degrees C in a nitrogen atmosphere. The plate-like structures of boehmite form alpha-alumina; meanwhile, graphene particles at the grain boundaries hinder the growth of alumina grains. The graphene reinforcement was bonded to alpha-alumina matrix by van der Waals forces. The XRD pattern reveals the presence of graphene with a plane (002) along with alpha-alumina. Properties such as fracture toughness (5.6 +/- 0.01 MPa m(0.5)), Vickers hardness (1872 +/- 25 kgf/mm(2)) and true density (3.8 g/cm(3)) were achieved in 0.5 wt.% graphene-alumina composite when compared to alpha-alumina with fracture toughness (5.3 +/- 0.1 MPa m(0.5)), Vickers hardness (1984 +/- 28 kgf/mm(2)) and true density (3.91 g/cm(3)). The bridging and deviation of cracks in 0.5 wt.% graphene-alumina composite are attributed to the anchoring and dissipation of energy during crack growth, which enhances the fracture toughness, whereas alpha-alumina exhibits failure caused by linear crack propagation. Meanwhile, the slight decrease in Vickers hardness and true density of 0.5 wt.% graphene-alumina composite is due to the tribological and low-density properties of graphene. The obtained properties of composite could be suitable in high-temperature, wear-resistant applications such as crucibles, bearings, etc.
引用
收藏
页码:1234 / 1244
页数:11
相关论文
共 36 条
  • [11] A model for the evaluation of indentation crack arrest fracture toughness of supported films
    B. Bozzini
    M. Boniardi
    Journal of Materials Science, 2001, 36 : 511 - 518
  • [12] Crack Propagation and Fracture Toughness of Graphene Probed by Raman Spectroscopy
    Zhang, Zilong
    Zhang, Xuewei
    Wang, Yunlu
    Wang, Yang
    Zhang, Yang
    Xu, Chen
    Zou, Zhenxing
    Wu, Zehao
    Xia, Yang
    Zhao, Pei
    Wang, Hong Tao
    ACS NANO, 2019, 13 (09) : 10327 - 10332
  • [13] Hot-pressed graphene nanoplatelets or/and zirconia reinforced hybrid alumina nanocomposites with improved toughness and mechanical characteristics
    Ahmad, Iftikhar
    Islam, Mohammad
    Al Habis, Nuha
    Parvez, Shahid
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 40 : 135 - 145
  • [14] Enhancement of fracture toughness of graphene via crack bridging with stone-thrower-wales defects
    Rajasekaran, G.
    Parashar, Avinash
    DIAMOND AND RELATED MATERIALS, 2017, 74 : 90 - 99
  • [15] Nonlinear fracture toughness measurement and crack propagation resistance of functionalized graphene multilayers
    Cao, Changhong
    Mukherjee, Sankha
    Howe, Jane Y.
    Perovic, Doug D.
    Sun, Yu
    Singh, Chandra Veer
    Filleter, Tobin
    SCIENCE ADVANCES, 2018, 4 (04):
  • [16] Indentation fracture mechanics toughness dependence on grain size and crack size: Application to alumina and WC-Co
    Armstrong, RW
    Cazacu, O
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2006, 24 (1-2) : 129 - 134
  • [17] Multiscale investigations into the fracture toughness of SiC/graphene composites: Atomistic simulations and crack-bridging model
    Wang, YongChao
    Zhu, YinBo
    He, ZeZhou
    Wu, HengAn
    CERAMICS INTERNATIONAL, 2020, 46 (18) : 29101 - 29110
  • [18] Development of structural ceramics having large crack-healing ability and fracture toughness
    Takahashi, K
    Yokouchi, M
    Lee, SK
    Ando, K
    SMART MATERIALS III, 2005, 5648 : 276 - 283
  • [19] A procedure for fracture toughness testing using a chevron-notched crack-arrest specimen
    Bonenberger, RJ
    Dally, JW
    Fourney, WL
    JOURNAL OF TESTING AND EVALUATION, 1998, 26 (04) : 376 - 386
  • [20] Graphene/epoxy nanocomposites for improved fracture toughness: A focused review on toughening mechanism
    Khalid, Muhammad Yasir
    Kamal, Abdallah
    Otabil, Adam
    Mamoun, Omar
    Liao, Kin
    CHEMICAL ENGINEERING JOURNAL ADVANCES, 2023, 16