Processing and properties of 2D SiC/SiC composites by precursor infiltration and pyrolysis

被引:15
作者
Yu Hai-jiao [1 ]
Zhou Xin-gui [1 ]
Wang Hong-lei [1 ]
Zhao Shuang [1 ]
Yang Jian-gao [2 ]
Huang Ze-lan [2 ]
机构
[1] Natl Univ Def Technol, Coll Aerosp & Mat Engn, Changsha 410073, Peoples R China
[2] Chongyi Zhangyuan Tungsten Co Ltd, Chongyi 341300, Peoples R China
来源
JOURNAL OF CENTRAL SOUTH UNIVERSITY OF TECHNOLOGY | 2009年 / 16卷 / 02期
关键词
SiC/SiC composites; coating; precursor infiltration and pyrolysis; chemical vapor deposition; CHEMICAL-VAPOR INFILTRATION; MECHANICAL-PROPERTIES; SICF/SIC COMPOSITES; MATRIX COMPOSITES; SIC-COMPOSITES; COATINGS; MICROSTRUCTURE; INTERPHASE; DEPOSITION; BEHAVIOR;
D O I
10.1007/s11771-009-0032-4
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Two-dimensional plain-weave silicon carbide fiber fabric reinforced silicon carbide (2D-SiC/SiC) composites were molded by stacking method and densified through precursor infiltration and pyrolysis (PIP) process. SiC coating was deposited as the fiber/matrix interphase layer by chemical vapor deposition (CVD) technique. Fiber/matrix debonding and relatively long fiber pullouts were observed on the fracture surfaces. Additionally, the flexural strength and elastic modulus of the composites with and without fiber/matrix interphase layer were investigated using three-point bending test and single-edge notched beam test. The results show that the fiber fraction and the porosity of 2D-SiC/SiC composites with and without coating are 27.2% (volume fraction) and 11.1%, and 40.7% (volume fraction) and 7.5%, respectively. And the flexural strength and elastic modulus of 2D-SiC/SiC composites with and without coating are 363.3 MPa and 127.8 GPa, and 180.2 MPa and 97.2 GPa, respectively. With a proper thickness, the coating can effectively adjust the fiber/matrix interface, thus causing a dramatic increase in the mechanical properties of the composites.
引用
收藏
页码:190 / 194
页数:5
相关论文
共 24 条
[1]   Influence of weave of carbon fabric in polyetherimide composites in various wear situations [J].
Bijwe, Jayashree ;
Rattan, Rekha .
WEAR, 2007, 263 (7-12 SPEC. ISS.) :984-991
[2]   Processing optimization and mechanical evaluation of hot pressed 2D Tyranno-SA/SiC composites [J].
Dong, SM ;
Katoh, Y ;
Kohyama, A .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2003, 23 (08) :1223-1231
[3]   Cordierite-mullite coating for SiCf/SiC composites [J].
Ferraris, M ;
Salvo, M ;
Smeacetto, F .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (13) :2343-2347
[4]  
Han GW, 2000, J MATER SCI TECHNOL, V16, P466
[5]   Coatings and joining for SiC and SiC-composites for nuclear energy systems [J].
Henager, C. H., Jr. ;
Shin, Y. ;
Bium, Y. ;
Giannuzzi, L. A. ;
Kempshall, B. W. ;
SchwarZ, M. .
JOURNAL OF NUCLEAR MATERIALS, 2007, 367 :1139-1143
[6]   Mechanical properties of SiC/SiC composite with magnesium-silicon oxide interphase [J].
Igawa, N. ;
Taguchi, T. ;
Yamada, R. ;
Ishii, Y. ;
Jitsukawa, S. .
JOURNAL OF NUCLEAR MATERIALS, 2007, 367 :725-729
[7]   Fabrication of SiC fiber reinforced SiC composite by chemical vapor infiltration for excellent mechanical properties [J].
Igawa, N ;
Taguchi, T ;
Nozawa, T ;
Snead, LL ;
Hinoki, T ;
McLaughlin, JC ;
Katoh, Y ;
Jitsukawa, S ;
Kohyama, A .
JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 2005, 66 (2-4) :551-554
[8]   Pulsed reactive chemical vapor deposition in the C-Ti-Si system from H2/TiCl4/SiCl4 [J].
Jacques, S ;
Di-Murro, H ;
Berthet, MP ;
Vincent, H .
THIN SOLID FILMS, 2005, 478 (1-2) :13-20
[9]   Microstructural evolution analysis of NITE SiC/SiC composite using TEM examination and dual-ion irradiation [J].
Kishimoto, H. ;
Ozawa, K. ;
Hashitomi, O. ;
Kohyama, A. .
JOURNAL OF NUCLEAR MATERIALS, 2007, 367 :748-752
[10]   Modeling stress-dependent matrix cracking and stress-strain behavior in 2D woven SiC fiber reinforced CVISiC composites [J].
Morscher, Gregory N. ;
Singh, Mrityunjay ;
Kiser, J. Douglas ;
Freedman, Marc ;
Bhatt, Ram .
COMPOSITES SCIENCE AND TECHNOLOGY, 2007, 67 (06) :1009-1017