Effects of CuO and Al2O3 additions on the tetragonal phase stability in 2.5 mol% Y-TZP ceramics

被引:0
|
作者
Singh, R [1 ]
Gill, C [1 ]
Lawson, S [1 ]
机构
[1] Univ Sunderland, Sch Engn & Adv Technol, Sunderland SR1 3SD, Durham, England
来源
PROCESSING AND FABRICATION OF ADVANCED MATERIALS VI, VOLS 1 & 2 | 1998年
关键词
Y-TZP; Al2O3; CuO; mechanical properties; hydrothermal ageing;
D O I
暂无
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Yttria-coated zirconia powders were simultaneously doped with up to 0.05 wt% CuO and 0.08 wt% Al2O3 Prepared doped pellets were sintered at 1300 degrees C but at different ramp rates ranging from 5 - 100 degrees C/min. and soaking periods of I to 2 hours. It was found that the 10 degrees C/min. and 2 hours hold cycle gave the overall best mechanical properties. Nevertheless, all of the doped samples revealed excellent resistance to hydrothermal degradation in superheated water at 180 degrees C and 1 MPa regardless of the sintering conditions, developing less than 13% monoclinic phase content after 200 hours of exposure whereas the undoped ceramic failed catastrophically in the early stages of ageing. Possible ageing mechanisms are discussed and the enhanced ageing resistance of the Cu-doped Y-TZPs is in part attributed to the fine grain size of the sintered body resulting from the presence of a transient liquid phase during low temperature sintering.
引用
收藏
页码:785 / 796
页数:12
相关论文
共 50 条
  • [31] Effect of additions on the properties of Al2O3/BN machinable ceramics
    Li, YL
    Qiao, GJ
    Jin, ZH
    RARE METAL MATERIALS AND ENGINEERING, 2004, 33 (07) : 744 - 747
  • [32] Microstructure and Fracture Toughness of Al2O3/3Y-TZP Composites
    李秀华
    索冠伟
    门荣磊
    杨正方
    JournalofRareEarths, 2005, (S1) : 164 - 166
  • [33] Effect of rod-like grain on properties and toughening mechanism of 3Y-TZP/Al2O3 ceramics
    荣守范
    吉泽升
    朱永长
    张敬强
    TransactionsofNonferrousMetalsSocietyofChina, 2008, (02) : 388 - 392
  • [34] Effects of isothermal annealing on the microstructure and mechanical properties of SiC ceramics hot-pressed with Y2O3 and Al2O3 additions
    Cheong, DI
    Kim, J
    Kang, SJL
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (08) : 1321 - 1327
  • [35] Effect of rod-like grain on properties and toughening mechanism of 3Y-TZP/Al2O3 ceramics
    Rong Shou-fan
    Ji Ze-Sheng
    Zhu Yong-chang
    Zhang Jing-qiang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2008, 18 (02) : 388 - 392
  • [36] Microstructure and fracture toughness of Al2O3/3Y-TZP composites
    Li, XH
    Suo, GW
    Men, RL
    Yang, ZF
    JOURNAL OF RARE EARTHS, 2005, 23 : 164 - 166
  • [37] Comparison of sintering behavior and reinforcing mechanisms between 3Y-TZP/Al2O3(w) and 12Ce-TZP/Al2O3(w) composites: Combined effects of lanthanide stabilizer and Al2O3 whisker length
    Yuan, Li-Juan
    Zhang, Peng-Jie
    Zuo, Fei
    Luo, Rui-Xin
    Guo, Zhao-Liang
    Plucknett, Kevin
    Jiang, Bei-Bei
    Nie, Guang-Lin
    Meng, Fan
    Valcarcel-Juarez, Victor
    Maitre, Alexandre
    Lin, Hua-Tay
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2021, 41 (01) : 706 - 718
  • [38] Effects of MgO and Y2O3 on the microstructure and mechanical properties of Al2O3 ceramics
    Liu, Huahe
    Liu, Hanlian
    Huang, Chuanzhen
    Zou, Bin
    Chai, Yacong
    ADVANCES IN MACHINING AND MANUFACTURING TECHNOLOGY XII, 2014, 589-590 : 572 - 577
  • [39] Residual stress and diffraction line-broadening analysis of Al2O3/Y-TZP ceramic composites by neutron diffraction measurement
    Fan, Kunyang
    Ruiz-Hervias, Jesus
    Pastor, Jose Ygnacio
    Gurauskis, Jonas
    Baudin, Carmen
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2017, 64 : 122 - 134
  • [40] The study of mechanical properties of Ti3SiC2/Y-TZP ceramics composites
    Shi, SL
    Pan, W
    Li, JQ
    Fang, MH
    RARE METAL MATERIALS AND ENGINEERING, 2003, 32 : 252 - 255