On the R-curve behavior of human tooth enamel

被引:154
作者
Bajaj, Devendra [1 ]
Arola, Dwayne D. [1 ,2 ]
机构
[1] Univ Maryland Baltimore Cty, Dept Mech Engn, Baltimore, MD 21250 USA
[2] Univ Maryland, Baltimore Coll Dent Surg, Dept Endodont Prosthodont & Operat Dent, Baltimore, MD 21201 USA
关键词
Decussation; DEJ; Enamel; Fracture; R-curve; Toughening mechanisms; FATIGUE-CRACK GROWTH; MECHANICAL-PROPERTIES; FRACTURE-TOUGHNESS; DENTINOENAMEL JUNCTION; TOUGHENING MECHANISMS; ELASTIC-MODULUS; DENTIN; RESISTANCE; BONE;
D O I
10.1016/j.biomaterials.2009.04.017
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
In this study the crack growth resistance behavior and fracture toughness of human tooth enamel were quantified using incremental crack growth measures and conventional fracture mechanics. Results showed that enamel undergoes an increase in crack growth resistance (i.e. rising R-curve) with crack extension from the outer to the inner enamel, and that the rise in toughness is a function of distance from the dentin enamel junction (DEJ). The outer enamel exhibited the lowest apparent toughness (0.67 +/- 0.12 MPa m(0.5)), and the inner enamel exhibited a rise in the growth toughness from 1.13 MPa m(0.5)/mm to 3.93 Mpa m(0.5)/mm. The maximum crack growth resistance at fracture (i.e. fracture toughness (K-c)) ranged from 1.79 to 2.37 MPa m(0.5). Crack growth in the inner enamel was accompanied by a host of mechanisms operating from the micro- to the nano-scale. Decussation in the inner enamel promoted crack deflection and twist, resulting in a reduction of the local stress intensity at the crack tip. In addition, extrinsic mechanisms such as bridging by unbroken ligaments of the tissue and the organic matrix promoted crack closure. Microcracking due to loosening of prisms was also identified as an active source of energy dissipation. In summary, the unique microstructure of enamel in the decussated region promotes crack growth toughness that is approximately three times that of dentin and over ten times that of bone. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:4037 / 4046
页数:10
相关论文
共 50 条
  • [1] [Anonymous], 2005, FRACTURE MECH FUNDAM
  • [2] A comparison of fatigue crack growth in human enamel and hydroxyapatite
    Bajaj, Devendra
    Nazari, Ahmad
    Eidelman, Naomi
    Arola, Dwayne D.
    [J]. BIOMATERIALS, 2008, 29 (36) : 4847 - 4854
  • [3] Role of prism decussation on fatigue crack growth and fracture of human enamel
    Bajaj, Devendra
    Arola, Dwayne
    [J]. ACTA BIOMATERIALIA, 2009, 5 (08) : 3045 - 3056
  • [4] Evaluation of a new modulus mapping technique to investigate microstructural features of human teeth
    Balooch, G
    Marshall, GW
    Marshall, SJ
    Warren, OL
    Asif, SAS
    Balooch, M
    [J]. JOURNAL OF BIOMECHANICS, 2004, 37 (08) : 1223 - 1232
  • [5] The effect of prism orientation on the indentation testing of human molar enamel
    Braly, A.
    Darnell, L. A.
    Mann, A. B.
    Teaford, M. F.
    Weihs, T. P.
    [J]. ARCHIVES OF ORAL BIOLOGY, 2007, 52 (09) : 856 - 860
  • [6] Self-assembly of synthetic hydroxyapatite nanorods into an enamel prism-like structure
    Chen, HF
    Clarkson, BH
    Sun, K
    Mansfield, JF
    [J]. JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2005, 288 (01) : 97 - 103
  • [7] Nanoindentation mapping of the mechanical properties of human molar tooth enamel
    Cuy, JL
    Mann, AB
    Livi, KJ
    Teaford, MF
    Weihs, TP
    [J]. ARCHIVES OF ORAL BIOLOGY, 2002, 47 (04) : 281 - 291
  • [8] Fatigue crack propagation path across the dentinoenamel junction complex in human teeth
    Dong, XD
    Ruse, ND
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2003, 66A (01) : 103 - 109
  • [9] ON THE TOUGHENING OF CERAMICS BY STRONG REINFORCEMENTS
    EVANS, AG
    MCMEEKING, RM
    [J]. ACTA METALLURGICA, 1986, 34 (12): : 2435 - 2441
  • [10] EVANS AG, 1984, AM CERAM SOC BULL, V84, P255