Interfacial microstructure evolution and formation process of the joints prepared by diffusion bonding on DD6 nickel-based single crystal superalloy

被引:35
作者
Peng, Yu [1 ,2 ]
Li, Jinglong [1 ,2 ]
Peng, Xuan [2 ]
Li, Shiwei [2 ]
Xiong, Jiangtao [2 ]
Shi, Junmiao [2 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
[2] Northwestern Polytech Univ, Shaanxi Key Lab Frict Welding Technol, Xian 710072, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2020年 / 9卷 / 06期
关键词
Nickel-based single crystal superalloy; Diffusion bonding; Interlayer; Interface microstructure evolution; BEHAVIOR; PRECIPITATION; TENSILE;
D O I
10.1016/j.jmrt.2020.11.083
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Nickel-based single crystal superalloy DD6 was diffusion bonded in vacuum at 1170 degrees C under 55 MPa for 2-6 h. Two processes, direct bonding and bonding with interlayer, were designed for comparison. A pure 4 mu m nickel (Ni) foil was selected for the interlayer. The joint strength was measured via shear test, whereas the joint microstructure and element distribution were analyzed via scanning electron microscope, electron probe analyzer and transmission electron microscope. The results indicated that the joint direct bonded for 6 h achieved the best joint quality at approximately 353 MPa of shear strength. In this case, the joint morphology and microstructure were characterized by microvoids and carbide precipitation. In contrast, in the joints bonded with interlayer, both carbide precipitation and microvoids disappeared. When 4 mu m nickel foil was used as an interlayer, the foil/DD6 interface became less distinct as the bonding time prolonged. When the bonding time reached 6 h, the gamma' phase crystals connected each other with the misorientation distribution of the joint less than 5 degrees, and maximum shear strength of 727 MPa was obtained. The fracture morphology has a mixed ductile-brittle feature. (C) 2020 The Author(s). Published by Elsevier B.V.
引用
收藏
页码:16317 / 16328
页数:12
相关论文
共 36 条
[1]  
[Anonymous], 1992, ASM HDB ALLOY PHASE
[2]  
Cai YL, 1986, COLOR METALLOGRAPHIC
[3]   Effect of Holding Time on Microstructure and Properties of Transient Liquid-Phase-Bonded Joints of a Single Crystal Alloy [J].
Chai, Lu ;
Huang, Jihua ;
Hou, Jinbao ;
Lang, Bo ;
Wang, Li .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (06) :2287-2293
[4]   An experimental and numerical analysis of residual stresses in a TIG weldment of a single crystal nickel-base superalloy [J].
Chen, Jingwei ;
Salvati, Enrico ;
Uzun, Fatih ;
Papadaki, Chrysanthi ;
Wang, Zifan ;
Everaerts, Joris ;
Korsunsky, Alexander M. .
JOURNAL OF MANUFACTURING PROCESSES, 2020, 53 :190-200
[5]   Welding of nickel base superalloy single crystals [J].
David, SA ;
Vitek, JM ;
Babu, SS ;
Boatner, LA ;
Reed, RW .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 1997, 2 (02) :79-88
[6]   Tensile, creep behavior and microstructure evolution of an as-cast Ni-based K417G polycrystalline superalloy [J].
Du, Beining ;
Hu, Ziyang ;
Sheng, Liyuan ;
Cui, Chuanyong ;
Yang, Jinxia ;
Zheng, Yufeng ;
Sun, Xiaofeng .
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2018, 34 (10) :1805-1816
[7]   Precipitation and evolution of grain boundary boride in a nickel-based superalloy during thermal exposure [J].
Du, Beining ;
Sheng, Liyuan ;
Cui, Chuanyong ;
Yang, Jinxia ;
Sun, Xiaofeng .
MATERIALS CHARACTERIZATION, 2017, 128 :109-114
[8]  
He G, 1994, MAT REV, V1, P12
[9]  
Hu Z Q, 2005, AEROENGINE, V31, P1
[10]  
Huang B.Y., 2006, China Material Engineering Code: Non-Ferrous Metal Material Engineering, V4