Effect of short glass fiber/filler particle proportion on flexural and diametral tensile strength of a novel fiber-reinforced composite

被引:19
|
作者
Fonseca, Rodrigo Borges [1 ]
de Almeida, Leticia Nunes [2 ]
Martins Mendes, Gustavo Adolfo [2 ]
Barbosa Kasuya, Amanda Vessoni [2 ]
Favarao, Isabella Negro [2 ]
de Paula, Marcella Silva [2 ]
机构
[1] Univ Fed Goias, Sch Dent, Dept Restorat Dent & Dent Mat, Goiania, Go, Brazil
[2] Univ Fed Goias, Sch Dent, Goiania, Go, Brazil
关键词
Glass fiber; Flexural strength; Diametral tensile strength; Fiber-reinforced composite; Filler particles; LOAD-BEARING CAPACITY; DENTAL COMPOSITES; RESIN COMPOSITES; WATER SORPTION; BOND STRENGTH; SOLUBILITY; FRACTION; MODULUS; SILICA; AGENT;
D O I
10.1016/j.jpor.2015.10.004
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: To evaluate the effect of glass fiber/filler particles proportion on flexural strength and diametral tensile strength of an experimental fiber-reinforced composite. Methods: Four experimental groups (N = 10) were created using an experimental short fiber reinforced composite, having as a factor under study the glass fiber (F) and filler particle (P) proportion: F22.5/P55 with 22.5 wt% of fiber and 55 wt% of filler particles; F25/P52.5 with 25 wt% of fiber and 52.5 wt% of filler particles; F27.5/P50 with 27.5 wt% of fiber and 50 wt% of filler particles; F30/P47.5 with 30 wt% of fiber and 47.5 wt% of filler particles. The experimental composite was made up by a methacrylate-based resin (50% Bis-GMA and 50% TEGDMA). Specimens were prepared for Flexural Strength (FS) (25 mm x 2 mm x 2 mm) and for Diametral Tensile Strength (DTS) (3 x 6 0 mm) and tested at 0.5 mm/min in a universal testing machine. Results: The results (in MPa) showed significance (different superscript letters mean statistical significant difference) for FS (p < 0.009) and DTS (p < 0.001) - FS results: F22.5/P55: 217.24 +/- 20.64(B); F25/P52.5: 245.77 +/- 26.80(AB); F27.5/P50: 246.88 +/- 32.28(AB); F30/P47.5: 259.91 +/- 26.01(A). DTS results: F22.5/P55: 21.82 +/- 4A2(B); F25/P52.5: 22.00 +/- 7.40(B); F27.5/P50: 18.63 +/- 4.41(B); F30/P47.5: 31.05 +/- 2.97(A). In SEM analysis, areas without fiber reinforcement demonstrated to be more prone to the presence of bubbles and crack development. The group F30/P47.5 showed areas with a great quantity of fibers without empty spaces for crack propagation. Conclusion: Increasing fiber content results in higher flexural and diametral tensile strength of an experimental composite reinforced with glass fibers. (C) 2015 Japan Prosthodontic Society. Published by Elsevier Ireland. All rights reserved.
引用
收藏
页码:47 / 53
页数:7
相关论文
共 50 条
  • [31] A tensile strength model for unidirectional fiber-reinforced brittle matrix composite
    Liao, K
    Reifsnider, KL
    INTERNATIONAL JOURNAL OF FRACTURE, 2000, 106 (02) : 95 - 115
  • [32] Evaluation of Tensile, Flexural and Impact Strength of Gongura Fiber Reinforced Epoxy Composite
    Manivel, P.
    Dhamotharan, S.
    Prakasam, R. Justin
    Kishore, G. M.
    3RD INTERNATIONAL CONFERENCE ON ADVANCEMENTS IN AEROMECHANICAL MATERIALS FOR MANUFACTURING: ICAAMM-2020, 2021, 2317
  • [33] Glass Fiber-Reinforced Phenolic Composite
    Iqbal, Javed
    Ahmad, Rafiq
    Zaki, Yousaf
    Jamil, Tahir
    JOURNAL OF THE PAKISTAN INSTITUTE OF CHEMICAL ENGINEERS, 2009, 37 : 55 - 60
  • [34] The effect of fiber-reinforced interleaves on the interlaminar shear strength of continuous glass fiber-reinforced polypropylene laminates
    Fang, Li
    Li, Xuwu
    Zhou, Xiaodong
    JOURNAL OF POLYMER ENGINEERING, 2013, 33 (03) : 221 - 227
  • [35] THE TENSILE-STRENGTH OF A FIBER-REINFORCED CERAMIC
    SCHWIETERT, HR
    STEIF, PS
    INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 1991, 28 (03) : 299 - 315
  • [36] Tensile stiffness and strength of fiber-reinforced concrete
    Grimaldi, A
    Luciano, R
    JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 2000, 48 (09) : 1987 - 2008
  • [37] Short-term tensile strength of carbon fiber-reinforced polymer laminates for flexural strengthening of concrete girders
    Okeil, AM
    El-Tawil, S
    Shahawy, M
    ACI STRUCTURAL JOURNAL, 2001, 98 (04) : 470 - 478
  • [39] Tensile Strength Matrix Composite Waste Glass Fiber Reinforced Plastics
    Mataram, A.
    JURNAL TEKNOLOGI, 2014, 69 (06):
  • [40] Effect of Aramid Fiber on the Properties of Glass Fiber-Reinforced Composite for Cryogenic Applications
    Bang, Seoung-Gil
    Yeom, Dong-Ju
    Jeong, Yeon-Jae
    Kim, Hee-Tae
    Kim, Jeong-Dae
    Kim, Seul-Kee
    Kim, Jeong-Hyeon
    Lee, Jae-Myung
    APPLIED COMPOSITE MATERIALS, 2022, 29 (04) : 1431 - 1448