Post-FSW Cold-Rolling Simulation of ECAP Shear Deformation and Its Microstructure Role Combined to Annealing in a FSWed AA5754 Plate Joint

被引:9
作者
Cabibbo, Marcello [1 ]
Paoletti, Chiara [1 ]
Ghat, Mohamed [1 ]
Forcellese, Archimede [1 ]
Simoncini, Michela [1 ,2 ]
机构
[1] Univ Politecn Marche, DIISM, Via Brecce Bianche 12, I-60131 Ancona, Italy
[2] Univ eCampus, Via Isimabrdi 10, I-22060 Novedrate, Italy
关键词
FSW; CR; ECAP; TEM; hardness; AA5000; series; STIR WELDING PROCESS; MECHANICAL-PROPERTIES; ALUMINUM-ALLOY; GRAIN-REFINEMENT; WELDED-JOINTS; FRICTION; RECRYSTALLIZATION; PARAMETERS; ROTATION; SPEEDS;
D O I
10.3390/ma12091526
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Friction stir welds are considered reliable joints for their lack of voids, cracks and distortions. When compared to the base material, friction stir welding (FSW) joints typically exhibit finer grain structured (especially at the nugget zone, NZ). Similarly, refined grain structure can also be obtained by severe plastic deformation (SPD) techniques, such as equal channel angular pressing (ECAP). In fact, the fine grain structures produced within the NZ of FSW or friction stir processed (FSP) materials are usually coarser than the ones achieved by ECAP. The former is characterized by lower dislocation density, higher high-angle boundary fraction and different mechanical strength, compared to what can be obtained by ECAP. In this study, a dedicated cold-rolling (CR) set-up, specifically designed to simulate an ECAP-equivalent shear deformation, was used to further refine the grain structure of FSW AA5754 sheets. The effect of ECAP-equivalent deformation induced by CR in a 2 mm-thick AA5754-H111 FSW joint was investigated. FSW was carried out at two different rotational () and translational (v) welding speeds, 600 rpm, 200 mm/min and 1800 rpm, 75 mm/min, respectively. FSW sheets were then CR to obtain an equivalent shear strain of epsilon 1.08, that is equivalent to 1-ECAP pass carried out with an internal die channels intersecting at an angle phi = 90 degrees with a curvature extending over an angle = 20 degrees. By CR, the sheet thickness reduced only by 20%. The role of annealing on the FSW and CR plastically deformed AA5754 was also investigated. This was applied either prior or after FSW, and it resulted that whenever it follows the FSW, the mean volume fraction of dispersoids and Mg-rich particles is higher than the case of annealing preceding the FSW process. On the contrary, it was found that the annealing treatment had a minimal role on the dispersoids and particles mean size. The here reported post-FSW ECAP-simulated deformation, obtained by a customized CR process, showed sheet integrity and a significant concurrent grain size refinement.
引用
收藏
页数:14
相关论文
共 37 条
[1]   Influences of metastable θ", θ′ and stable θ intermetallics formed during cryorolling and friction stir welding process on AA2219 [J].
Babu, K. Kamal ;
Panneerselvam, K. ;
Sathiya, P. ;
Haq, A. Noorul ;
Sundarrajan, S. ;
Mastanaiah, P. ;
Murthy, C. V. Srinivasa .
JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 732 :624-629
[2]   Sustainability analysis of friction stir welding of AA5754 sheets [J].
Bevilacqua, Maurizio ;
Ciarapica, Filippo Emanuele ;
D'Orazio, Alessio ;
Forcellese, Archimede ;
Simoncini, Michela .
10TH CIRP CONFERENCE ON INTELLIGENT COMPUTATION IN MANUFACTURING ENGINEERING - CIRP ICME '16, 2017, 62 :523-528
[3]   The influences of rotational and welding speeds on microstructures and mechanical properties of friction stir welded Al5083 and commercially pure copper sheets lap joints [J].
Bisadi, H. ;
Tavakoli, A. ;
Sangsaraki, M. Tour ;
Sangsaraki, K. Tour .
MATERIALS & DESIGN, 2013, 43 :80-88
[4]   Transmission electron microscopy study of strain-induced low- and high-angle boundary development in equal-channel angular-pressed commercially pure aluminum [J].
Cabibbo, M. ;
Blum, W. ;
Evangelista, E. ;
Kassner, M. E. ;
Meyers, M. A. .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2008, 39A (01) :181-189
[5]   Effect of welding motion and pre-/post-annealing of friction stir welded AA5754 joints [J].
Cabibbo, M. ;
Forcellese, A. ;
Simoncini, M. ;
Pieralisi, M. ;
Ciccarelli, D. .
MATERIALS & DESIGN, 2016, 93 :146-159
[6]   A TEM Kikuchi pattern study of ECAP AA1200 via routes A, C, BC [J].
Cabibbo, M. .
MATERIALS CHARACTERIZATION, 2010, 61 (06) :613-625
[7]  
Cabibbo M, 2016, JOINING TECHNOLOGIES, P7
[8]   Microstructure and Intermetallic Strengthening in an Equal Channel Angular Pressed AA2219. Part II: Strengthening Model [J].
Cabibbo M. ;
Santecchia E. .
Metallography, Microstructure, and Analysis, 2014, 3 (03) :203-212
[9]   Microstructure strengthening mechanisms in different equal channel angular pressed aluminum alloys [J].
Cabibbo, Marcello .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 560 :413-432
[10]   Effect of Cold Rolling on the Mechanical Properties and Formability of FSWed Sheets in AA5754-H114 [J].
Casalino, Giuseppe ;
El Mehtedi, Mohamad ;
Forcellese, Archimede ;
Simoncini, Michela .
METALS, 2018, 8 (04)