Effect of activation pretreatment of limonitic laterite ores using sodium fluoride and sulfuric acid on water leaching of nickel and cobalt

被引:34
作者
Ma, Baozhong [1 ,3 ]
Yang, Weijiao [1 ,3 ]
Pei, Yanlin [1 ]
Wang, Chengyan [1 ,2 ]
Jin, Bingjie [1 ]
机构
[1] Kunming Univ Sci & Technol, State Key Lab Complex Nonferrous Met Resources Cl, Kunming 650093, Yunnan, Peoples R China
[2] Univ Sci & Technol Beijing, Sch Met & Ecol Engn, Beijing 100083, Peoples R China
[3] Beijing Gen Res Inst Min & Met, Beijing 100160, Peoples R China
基金
中国国家自然科学基金;
关键词
Limonitic laterite; Activation pretreatment; Water leaching; Nickel; Cobalt; ATMOSPHERIC-PRESSURE; NICKELIFEROUS LATERITES; NITRIC-ACID; REDUCTION; EXTRACTION; CONCENTRATE; CARBONATE; KINETICS; IRON;
D O I
10.1016/j.hydromet.2017.02.026
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
This study investigated the effect of activation pretreatment of limonitic laterite ores using sodium fluoride and sulfuric acid on water leaching of nickel (Ni) and cobalt (Co) over iron at atmospheric pressure. X-ray diffraction, thermogravimetric and differential scanning calorimetry, scanning electron microscopy/energy-dispersive spectroscopy, and optical microscopy were used to characterize ore samples before and after activation. Results showed that iron oxides are the major minerals of the original ore, as well as the major Ni-and Co-bearing minerals. Activation pretreatment can break these mineral lattices and expose their Ni and Co to the reaction interface, thereby facilitating easy and selective extraction of both metals over iron under mild leaching conditions. Ni and Co leaching reached 85.3% and 93.9%, respectively, and the Fe dissolution was <8% under optimal conditions. Furthermore, behaviors of Fe, Ni, and Co in the activation process were illustrated. The effects of such behaviors on their leaching were also discussed. (C) 2017 Elsevier B.V. All rights reserved.
引用
收藏
页码:411 / 417
页数:7
相关论文
共 34 条
[1]   Hydrometallurgical process for the separation and recovery of nickel from sulphate heap leach liquor of nickeliferrous laterite ores [J].
Agatzini-Leonardou, S. ;
Tsakiridis, P. E. ;
Oustadakis, P. ;
Karidakis, T. ;
Katsiapi, A. .
MINERALS ENGINEERING, 2009, 22 (14) :1181-1192
[2]  
Burstein G.T., 1997, Corrosion Sci, V39, P1499, DOI [DOI 10.1016/S0010-938X(97)00096-6, 10.1016/S0010-938X(97)00096-6]
[3]   Extraction of nickel from lateritic ores at atmospheric pressure with agitation leaching [J].
Buyukakinci, E. ;
Topkaya, Y. A. .
HYDROMETALLURGY, 2009, 97 (1-2) :33-38
[4]   NATURAL FERRIHYDRITES IN SURFACE DEPOSITS FROM FINLAND AND THEIR ASSOCIATION WITH SILICA [J].
CARLSON, L ;
SCHWERTMANN, U .
GEOCHIMICA ET COSMOCHIMICA ACTA, 1981, 45 (03) :421-429
[5]  
CHANDER S, 1982, T INDIAN I METALS, V35, P366
[6]  
Dalvi A., 2004, The Past and the Future of Nickel Laterites
[7]   Extraction of nickel and cobalt from reduced limonitic laterite using a selective chlorination-water leaching process [J].
Fan, Chuanlin ;
Zhai, Xiujing ;
Fu, Yan ;
Chang, Yongfeng ;
Li, Binchuan ;
Zhang, Ting-an .
HYDROMETALLURGY, 2010, 105 (1-2) :191-194
[8]   A novel hydrometallurgical approach to recover valuable metals from laterite ore [J].
Gao, Jian-Ming ;
Yan, Zhi-Kai ;
Liu, Jing ;
Zhang, Mei ;
Guo, Min .
HYDROMETALLURGY, 2014, 150 :161-166
[9]   Activation pretreatment of limonitic laterite ores by alkali-roasting method using sodium carbonate [J].
Guo, Qiang ;
Qu, Jingkui ;
Qi, Tao ;
Wei, Guangye ;
Han, Bingbing .
MINERALS ENGINEERING, 2011, 24 (08) :825-832
[10]   Leaching behavior of metals from a limonitic nickel laterite using a sulfation-roasting-leaching process [J].
Guo, Xueyi ;
Li, Dong ;
Park, Kyung-Ho ;
Tian, Qinghua ;
Wu, Zhan .
HYDROMETALLURGY, 2009, 99 (3-4) :144-150