Internal cooling to produce aluminium alloy slurries for rheocasting

被引:19
作者
Birol, Yucel [1 ]
机构
[1] TUBITAK, Marmara Res Ctr, Mat Inst, Gebze, Kocaeli, Turkey
关键词
Metals; Casting; Semi-solid processing; Rheocasting; MICROSTRUCTURE;
D O I
10.1016/j.jallcom.2009.02.104
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Rheocasting is becoming the choice of the casting industry which relies on the semi-solid processing for high integrity structural parts. It is thus of great technological interest to identify simple methods to prepare slurries at reduced cost. The potential of internal cooling to produce slurries for rheocasting was investigated in the present work for several aluminium casting alloys which are technologically important for aluminium foundries. Alloys quenched directly from the liquid state were predominantly dendritic while the slurry samples quenched after an initial fraction of solid phase was first formed, were dominated by alpha-Al rosettes and globules. The solidification of the remaining liquid phase occurred through the growth of the alpha-Al rosettes and globules which have formed during internal cooling before quenching. (C) 2009 Elsevier B.V. All rights reserved.
引用
收藏
页码:365 / 368
页数:4
相关论文
共 17 条
[1]  
Apelian D., 2004, DIE CAST ENG, V48, P22
[2]   Semisolid processing of near-eutectic and hypereutectic Al-Si-Cu alloys [J].
Birol, Yucel .
JOURNAL OF MATERIALS SCIENCE, 2008, 43 (10) :3577-3581
[3]  
Birol Y, 2007, INT J MATER RES, V98, P1019, DOI 10.3139/146.101560
[4]   Semi-solid processing of the primary aluminium die casting alloy A365 [J].
Birol, Yucel .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 473 (1-2) :133-138
[5]   Forming of AlSi8Cu3Fe alloy in the semi-solid state [J].
Birol, Yucel .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 470 (1-2) :183-187
[6]  
Doutre D., 2004, P 8 INT INTERNATIONA, P397
[7]   Microstructure and mechanical properties of rheo-diecast (RDC) aluminium alloys [J].
Fan, Z ;
Fang, X ;
Ji, S .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 412 (1-2) :298-306
[8]   Semisolid metal processing [J].
Fan, Z .
INTERNATIONAL MATERIALS REVIEWS, 2002, 47 (02) :49-85
[9]  
Flemings M.C., 2003, U.S. Patent, Patent No. [US6645323B2, 6645323, 6, 645, 323]
[10]   BEHAVIOR OF METAL-ALLOYS IN THE SEMISOLID STATE [J].
FLEMINGS, MC .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1991, 22 (05) :957-981