The adhesion of hot-filament CVD diamond films on AISI type 316 austenitic stainless steel

被引:33
|
作者
Buijnsters, JG
Shankar, P
van Enckevort, WJP
Schermer, JJ
ter Meulen, JJ
机构
[1] Univ Nijmegen, Dept Appl Phys, NSRIM, NL-6525 ED Nijmegen, Netherlands
[2] Univ Nijmegen, Dept Solid State Phys, NSRIM, NL-6525 ED Nijmegen, Netherlands
[3] Univ Nijmegen, Dept Expt Solid State Phys 3, NSRIM, NL-6525 ED Nijmegen, Netherlands
[4] Indira Gandhi Ctr Atom Res, Met & Mat Grp, Kalpakkam 603102, Tamil Nadu, India
关键词
chemical vapor deposition; diamond films; adhesion; steel;
D O I
10.1016/j.diamond.2003.11.012
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Steel ball indentation and scratch adhesion testing of hot filament chemical vapour deposited diamond films onto AISI type 316 austenitic stainless steel substrates using two different interlayer systems, namely chromium nitride and borided steel, have been investigated. In order to compare the adhesion of these films with that of a well-known and strongly adherent system, detailed adhesion tests were performed on diamond films grown on molybdenum substrates as well. Scanning electron microscopy analysis of various indented regions on the diamond-coated steel and molybdenum samples in combination with the measurement of the acoustic emission signals during loading, indicate that the adhesion of the coatings on the stainless steel substrates with the CrN interlayer is comparable and only slightly less than that of the strongly adhering diamond films on the molybdenum samples. The critical load value derived from the acoustic emission signals at which partial delammation of the diamond films is first observed, is significantly lower for the diamond-coated steel with the boride interlayer than that obtained with the CrN interlayer for the present deposition conditions used. The steel ball indentation tests also show that the hardness and thickness of the interlayer have a strong effect on the penetration depths of the indents. Scratch tests performed on the diamond coated stainless steel specimens with the boride interlayer show no significant coating failure for loads up to 80 N. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:848 / 857
页数:10
相关论文
共 50 条
  • [1] DEPOSITION OF DIAMOND FILMS IN A CLOSED HOT-FILAMENT CVD SYSTEM
    LAI, GR
    FARABAUGH, EN
    FELDMAN, A
    ROBINS, LH
    JOURNAL OF RESEARCH OF THE NATIONAL INSTITUTE OF STANDARDS AND TECHNOLOGY, 1995, 100 (01) : 43 - 49
  • [2] Diamond/WC bilayer formation mechanism by hot-filament CVD
    Neto, M. A.
    Silva, E. L.
    Fernandes, A. J. S.
    Oliveira, F. J.
    Silva, R. F.
    SURFACE & COATINGS TECHNOLOGY, 2012, 206 (13) : 3055 - 3063
  • [3] Effect of substrate temperature on hot-filament CVD grown diamond films at constant filament current
    Ali, M.
    Qazi, I. A.
    INTERNATIONAL JOURNAL OF SURFACE SCIENCE AND ENGINEERING, 2012, 6 (03) : 214 - 230
  • [4] Diamond films synthesized by hot-filament CVD at pressures below 5 mbar
    Zhang, GF
    Buck, V
    NEW DIAMOND AND FRONTIER CARBON TECHNOLOGY, 2002, 12 (01): : 1 - 9
  • [5] The kinetics of diamond films growth over large area by hot-filament CVD
    Wang, AY
    Ke, PL
    Sun, C
    Huang, RF
    Wen, LS
    NEW CARBON MATERIALS, 2005, 20 (03) : 229 - 234
  • [6] FRICTION MEASUREMENTS ON HOT-FILAMENT CVD DIAMOND FILMS DEPOSITED ON ETCHED TUNGSTEN CARBIDE SURFACES
    EVERITT, NM
    SILVA, RF
    VIEIRA, J
    REGO, CA
    HENDERSON, CR
    MAY, PW
    DIAMOND AND RELATED MATERIALS, 1995, 4 (5-6) : 730 - 734
  • [7] Formation and adhesion of hot filament CVD diamond films on titanium substrates
    Peng, XL
    Clyne, TW
    THIN SOLID FILMS, 1997, 293 (1-2) : 261 - 269
  • [8] Diamond films grown without seeding treatment and bias by hot-filament CVD system
    Ali, M.
    Urgen, M.
    SOLID STATE SCIENCES, 2012, 14 (04) : 540 - 544
  • [9] Synthesis of CVD diamond at atmospheric pressure using the hot-filament CVD method
    Kobayashi, T
    Hirakuri, KK
    Mutsukura, N
    Machi, Y
    DIAMOND AND RELATED MATERIALS, 1999, 8 (06) : 1057 - 1060
  • [10] Lower filament temperature limit of diamond growth in a hot-filament CVD system
    Zhang, GE
    Buck, V
    SURFACE & COATINGS TECHNOLOGY, 2002, 160 (01) : 14 - 19