Synthesis and properties of hydrogenated natural rubber

被引:24
作者
Inoue, Shin-ichi
Nishio, Tomohiro
机构
[1] Aichi Inst Technol, Dept Appl Chem, Aichi 4700392, Japan
[2] Nitta Corp Ltd, Ctr Tech, Dept Product Dev, Yamato Koriyama, Nara 6391085, Japan
关键词
homogeneous hydrogenation; linear polymer; hydrogenated natural rubber (HNR); vulcanized 100% HNR;
D O I
10.1002/app.25158
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
A series of hydrogenated natural rubbers, HNRs, were prepared by homogenous hydrogenation using H-2 gas with a rhodium catalyst (chlorotris(triphenylphosphine)rhodium) in toluene. The HNRs were linear polymers with molecular weights greater than 800,000. These rubbers were vulcanized using sulfur and peroxide compounds. Vulcanized 100% HNR has a low glass transition temperature (T-g = -43 degrees C) and excellent abrasion resistance, and is resistant to oxidation and ozonolysis ageing. (c) 2006 Wiley Periodicals, Inc.
引用
收藏
页码:3957 / 3963
页数:7
相关论文
共 22 条
[1]  
AHAGON A, 1995, J SOCI RUBBER IND JP, V68, P595
[2]  
FUKAHORI Y, 1995, J SOCI RUBBER IND JP, V68, P605
[3]  
Gan SN, 1996, J APPL POLYM SCI, V59, P63, DOI 10.1002/(SICI)1097-4628(19960103)59:1<63::AID-APP10>3.0.CO
[4]  
2-9
[5]  
KUBO Y, 1986, J SOC RUBBER IND JPN, V59, P442
[6]  
MCMANUS NT, 1995, J MACROMOL SCI R M C, VC35, P239
[7]   MRI-negative rotator cuff tears [J].
Nakatani, T ;
Fujita, K ;
Iwasaki, Y ;
Sakai, H ;
Kurosaka, M .
MAGNETIC RESONANCE IMAGING, 2003, 21 (01) :41-45
[8]  
NAKAZAWA Y, 2003, BIOTECH S PREPR JPN, V21, P117
[9]  
ONISHI T, 2002, J SOCI RUBBER IND JP, V75, P268
[10]  
OOHARA R, 1995, J SOCI RUBBER IND JP, V68, P587