Combining alloy and process modification for micro-crack mitigation in an additively manufactured Ni-base superalloy

被引:136
作者
Griffiths, S. [1 ]
Tabasi, H. Ghasemi [2 ]
Ivas, T. [2 ]
Maeder, X. [1 ]
De Luca, A. [1 ]
Zweiacker, K. [1 ]
Wrobel, R. [1 ]
Jhabvala, J. [2 ]
Loge, R. E. [2 ]
Leinenbach, C. [1 ]
机构
[1] Empa Swiss Fed Labs Mat Sci & Technol, Uberlandstr 129, CH-8600 Dubendorf, Switzerland
[2] Ecole Polytech Fed Lausanne EPFL, Thermomech Met Lab PX Grp Chair, CH-2002 Neuchatel, Switzerland
关键词
Alloy design; Laser powder bed fusion; Crack mitigation; Ni superalloy; STRAY GRAIN FORMATION; SOLIDIFICATION CRACKING; SINGLE-CRYSTAL; LASER; MICROSTRUCTURE; MECHANISM; STRENGTH; CASTABILITY;
D O I
10.1016/j.addma.2020.101443
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The additive manufacturing (AM) of the gamma' precipitation strengthened Ni-base superalloys still remains a challenge due to their susceptibility to micro-cracking. Post-processing, such as HIPing, has been shown to heal the micro-cracks but it remains desirable to prevent the micro-cracking from even occurring. Numerous studies highlighting potential mechanisms for micro-cracking exist but few solutions have been demonstrated. The intent of this study was to identify the micro-crack mechanisms and demonstrate how process and alloy modifications can reduce the micro-cracking. The micro-crack surfaces exhibit a dendritic appearance that is indicative of solidification cracking. Additionally, Gleeble experiments, simulating the L-PBF induced Heat Affected Zone (HAZ), were conducted below the y' solvus temperature and reveal the existence of grain boundary liquation, indicative of liquation cracking. Two cracking mechanisms are thus coexisting during Laser Powder Bed Fusion (L-PBF) of CM247LC. Based on experimental evidence, reduction in the solidification interval of CM247LC was investigated as a candidate for micro-crack mitigation and a new alloy was developed. As Hf is found to have a significant influence on the freezing range of the alloy, a new CM247LC without Hf was produced and tested. The study also involved two separate and distinct processing conditions to highlight the importance of melt pool geometry on micro-crack density. Samples fabricated with the Hf-free CM247LC, CM247LC NHf, in combination with optimized processing conditions exhibit a reduction in crack density of 98 %. This study demonstrates the importance of both processing conditions and alloy chemistry on micro-cracking in L-PBF fabricated gamma' hardening Ni-base superalloys.
引用
收藏
页数:15
相关论文
共 38 条
  • [1] Origin of stray grain formation in single-crystal superalloy weld pools from heat transfer and fluid flow modeling
    Anderson, T. D.
    DuPont, J. N.
    DebRoy, T.
    [J]. ACTA MATERIALIA, 2010, 58 (04) : 1441 - 1454
  • [2] [Anonymous], 2010, SUPERALLOYS ALLOYING
  • [3] Aune RE, 2005, SUPERALLOYS 718, 625, 706 AND DERIVATIVES, PROCEEDINGS, P467
  • [4] The influence of the laser scan strategy on grain structure and cracking behaviour in SLM powder-bed fabricated nickel superalloy
    Carter, Luke N.
    Martin, Christopher
    Withers, Philip J.
    Attallah, Moataz M.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 615 : 338 - 347
  • [5] Carter LN, 2012, SUPERALLOYS 2012, P577
  • [6] Hot cracking mechanism affecting a non-weldable Ni-based superalloy produced by selective electron Beam Melting
    Chauvet, Edouard
    Kontis, Paraskevas
    Jaegle, Eric A.
    Gault, Baptiste
    Raabe, Dierk
    Tassin, Catherine
    Blandin, Jean-Jacques
    Dendievel, Remy
    Vayre, Benjamin
    Abed, Stephane
    Martin, Guilhem
    [J]. ACTA MATERIALIA, 2018, 142 : 82 - 94
  • [7] Investigations on the microstructure and crack formation of IN738LC samples processed by selective laser melting using Gaussian and doughnut profiles
    Cloots, Michael
    Uggowitzer, Peter J.
    Wegener, Konrad
    [J]. MATERIALS & DESIGN, 2016, 89 : 770 - 784
  • [8] Microstructure of selective laser melted CM247LC nickel-based superalloy and its evolution through heat treatment
    Divya, V. D.
    Munoz-Moreno, R.
    Messe, O. M. D. M.
    Barnard, J. S.
    Baker, S.
    Illston, T.
    Stone, H. J.
    [J]. MATERIALS CHARACTERIZATION, 2016, 114 : 62 - 74
  • [9] Donachie M.J., 2002, SUPER ALLOYS TECHNIC
  • [10] DuPont JohnN., 2009, WELDING METALLURGY W