Alkali-silica reaction in concrete containing glass

被引:79
作者
Dhir, Ravindra K. [1 ]
Dyer, T. D. [1 ]
Tang, M. C. [1 ]
机构
[1] Univ Dundee, Concrete Technol Unit, Dundee DD1 4HN, Scotland
关键词
Alkali-silica reaction; Glass; Particle size; Expansion; Concrete;
D O I
10.1617/s11527-008-9465-8
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The use of surplus waste glass in concrete has been avoided on the grounds that it is known to undergo harmful alkali-silica reaction (ASR). As part of a research project to develop draft specifications for glass in concrete, a major ASR testing programme was undertaken to establish appropriate use of glass in concrete which avoided harmful ASR. The British Standard for assessing ASR reactivity of aggregate-BS 812-123-was used. Testing was conducted on concrete mixes containing glass as either fine aggregate, filler aggregate, or as a Type II addition. Glass used as fine aggregate was found to produce significant expansion for both green and amber glass. GGBS and metakaolin had the effect of reducing this expansion considerably. Concrete containing powdered glass displayed much less expansion. A simple schematic model for the alkali-silica reaction of glass, based on glass dissolution mechanisms is proposed, and related to the test results.
引用
收藏
页码:1451 / 1462
页数:12
相关论文
共 20 条
  • [1] [Anonymous], 1994, C126094 ASTM
  • [2] *ASTM, 2008, C129308A ASTM
  • [3] Bazant ZP, 2000, J ENG MECH-ASCE, V126, P226
  • [4] Mathematical model for kinetics of alkali-silica reaction in concrete
    Bazant, ZP
    Steffens, A
    [J]. CEMENT AND CONCRETE RESEARCH, 2000, 30 (03) : 419 - 428
  • [5] *BRIT STAND I, 1999, 8121231999 BS BRIT S
  • [6] *BRIT STAND I, 2002, 12602002 BS EN BRIT
  • [7] British Standards Institution, 2000, 20612000 BS EN BRIT
  • [8] *BUILD RES EST, 1999, 330 BRE 2
  • [9] CHARLES RJ, 1958, J APPL PHYS, V29, P1549, DOI 10.1063/1.1722991
  • [10] DENTGLASSER LS, 1982, CEMENT CONCRETE RES, V12, P321