Relevant Influence of Limestone Crystallinity on CO2 Capture in The Ca-Looping Technology at Realistic Calcination Conditions

被引:52
作者
Valverde, J. M. [1 ]
Sanchez-Jimenez, P. E. [2 ]
Perez-Maqueda, L. A. [2 ]
机构
[1] Univ Seville, Fac Phys, E-41012 Seville, Spain
[2] Univ Seville, CSIC, Inst Ciencia Mat Sevilla, Seville 41092, Spain
关键词
CARBONATION REACTION; CARRYING-CAPACITY; CALCIUM-OXIDE; ATOMIC-SCALE; DECOMPOSITION; DIFFUSION; SORBENTS; CACO3; SURFACE; MODEL;
D O I
10.1021/es5014505
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
We analyze the role of limestone crystallinity on its CO2 capture performance when subjected to carbonation/calcination cycles at conditions mimicking the Ca-looping (CaL) technology for postcombustion CO2 capture. The behavior of raw and pretreated limestones (milled and thermally annealed) is investigated by means of thermogravimetric analysis (TGA) tests under realistic sorbent regeneration conditions, which necessarily involve high CO2 partial pressure in the calciner and quick heating rates. The pretreatments applied lead to contrasting effects on the solid crystal structure and, therefore, on its resistance to solid-state diffusion. Our results show that decarbonation at high CO2 partial pressure is notably promoted by decreasing solid crystallinity. CaO regeneration is fully achieved under high CO2 partial pressure at 900 degrees C in short residence times for the milled limestone whereas complete regeneration for raw limestone requires a minimum calcination temperature of about 950 degrees C. Such a reduction of the calcination temperature and the consequent mitigation of multicyclic capture capacity decay would serve to enhance the efficiency of the CaL technology. On the other hand, the results of our study suggest that the use of highly crystalline limestones would be detrimental since excessively high calcination temperatures should be required to attain full decarbonation at realistic conditions.
引用
收藏
页码:9882 / 9889
页数:8
相关论文
共 59 条
[1]   Development of synthetic CaO sorbents via CTAB-assisted sol-gel method for CO2 capture at high temperature [J].
Akgsornpeak, Akarat ;
Witoon, Thongthai ;
Mungcharoen, Thumrongrut ;
Limtrakul, Jumras .
CHEMICAL ENGINEERING JOURNAL, 2014, 237 :189-198
[2]   Atomistic Simulation of Surface Selectivity on Carbonate Formation at Calcium and Magnesium Oxide Surfaces [J].
Allen, Jeremy P. ;
Marmier, Arnaud ;
Parker, Stephen C. .
JOURNAL OF PHYSICAL CHEMISTRY C, 2012, 116 (24) :13240-13251
[3]   Undesired effects in the determination of CO2 carrying capacities of CaO during TG testing [J].
Alonso, M. ;
Criado, Y. A. ;
Abanades, J. C. ;
Grasa, G. .
FUEL, 2014, 127 :52-61
[4]   Pore-size and shape effects on the recarbonation performance of calcium oxide submitted to repeated calcination/recarbonation cycles [J].
Alvarez, D ;
Abanades, JC .
ENERGY & FUELS, 2005, 19 (01) :270-278
[5]   SELF-DIFFUSION OF CARBON AND OXYGEN IN CALCITE BY ISOTOPE EXCHANGE WITH CARBON DIOXIDE [J].
ANDERSON, TF .
JOURNAL OF GEOPHYSICAL RESEARCH, 1969, 74 (15) :3918-+
[6]  
Arias B., 2013, INT J GREENHOUSE GAS, V18, P237
[7]   Post-combustion calcium looping process with a highly stable sorbent activity by recarbonation [J].
Arias, Borja ;
Grasa, Gemma S. ;
Alonso, Monica ;
Carlos Abanades, J. .
ENERGY & ENVIRONMENTAL SCIENCE, 2012, 5 (06) :7353-7359
[8]  
BARKER R, 1973, J APPL CHEM BIOTECHN, V23, P733
[9]  
BERUTO D, 1984, J AM CERAM SOC, V67, P512
[10]   Microstructure, kinetic, structure, thermodynamic analysis for calcite decomposition: free-surface and powder bed experiments [J].
Beruto, DT ;
Searcy, AW ;
Kim, MG .