Effect of copolymerized butylene terephthalate chains on polymorphism and enzymatic degradation of poly(butylene adipate)

被引:50
作者
Zhao, Lifen
Gan, Zhihua [1 ]
机构
[1] Chinese Acad Sci, Inst Chem, Joint Lab Polymer Sci & Math,BNLMS, CAS Key Lab Engn Phys,Beijing Natl Lab Mol Sci, Beijing 100080, Peoples R China
[2] Chinese Acad Sci, Grad Sch, Beijing 100049, Peoples R China
基金
中国国家自然科学基金;
关键词
biodegradable polymers; polymorphism; recrystallization; enzymatic degradation; motion of polymer chains;
D O I
10.1016/j.polymdegradstab.2006.03.012
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The introduction of aromatic butylene terephthalate (BT) units into the backbone chains of aliphatic poly(butylene adipate) (PBA) not only changes the mechanical performance of the resultant P(BA-co-BT) copolymers but also affects their biodegradability. Because of the polymorphism of PBA homopolymer, the copolymerized BT units may also influence the polymorphic crystal structure as well as the biodegradation behavior. In this work, three P(BA-co-BT) copolymers with BT contents as 10, 20, and 25 mol% were chosen to study their polymorphic crystal structure, thermal properties and enzymatic degradation by means of wide-angle X-ray diffraction (WAXD), differential scanning calorimetry (DSC) and gravimetric methods. The results reveal that the P(BA-co-BT) copolymers with BT contents below 25 mol% can form polymorphic crystal structures after melt-crystallization at different temperatures. However, the recrystallization and transformation of polymorphic crystals are strongly affected by the rigid BT units. The enzymatic degradation rates of P(BA-co-BT) copolymers decrease with increasing the BT contents. The influences of the BT units on the polymorphism and enzymatic degradation are discussed in terms of the motion of PBA chains that copolymerized with BT units. It has been concluded from the examination of solid-state microstructure that the influence of the aromatic BT units on the motion of biodegradable PBA chains heavily influences the biodegradability. (c) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2429 / 2436
页数:8
相关论文
共 31 条
[1]  
ELING WB, 1982, POLYMER, V23, P1587
[2]   Structure and morphology of the aliphatic polyester poly-β-propiolactone in solution-grown chain-folded lamellar crystals [J].
Furuhashi, Y ;
Iwata, T ;
Sikorski, P ;
Atkins, E ;
Doi, Y .
MACROMOLECULES, 2000, 33 (25) :9423-9431
[3]   Metastability and transformation of polymorphic crystals in biodegradable poly(butylene adipate) [J].
Gan, ZH ;
Kuwabara, K ;
Abe, H ;
Iwata, T ;
Doi, Y .
BIOMACROMOLECULES, 2004, 5 (02) :371-378
[4]   The role of polymorphic crystal structure and morphology in enzymatic degradation of melt-crystallized poly(butylene adipate) films [J].
Gan, ZH ;
Kuwabara, K ;
Abe, H ;
Iwata, T ;
Doi, Y .
POLYMER DEGRADATION AND STABILITY, 2005, 87 (01) :191-199
[5]   Solid-state structures and thermal properties of aliphatic-aromatic poly(butylene adipate-co-butylene terephthalate) copolyesters [J].
Gan, ZH ;
Kuwabara, K ;
Yamamoto, M ;
Abe, H ;
Doi, Y .
POLYMER DEGRADATION AND STABILITY, 2004, 83 (02) :289-300
[6]   Temperature-induced polymorphic crystals of poly(butylene adipate) [J].
Gan, ZH ;
Abe, H ;
Doi, Y .
MACROMOLECULAR CHEMISTRY AND PHYSICS, 2002, 203 (16) :2369-2374
[7]   Crystal structures of α and β forms of poly(tetramethylene succinate) [J].
Ichikawa, Y ;
Kondo, H ;
Igarashi, Y ;
Noguchi, K ;
Okuyama, K ;
Washiyama, J .
POLYMER, 2000, 41 (12) :4719-4727
[8]   Crystal transition mechanisms in poly(ethylene succinate) [J].
Ichikawa, Y ;
Noguchi, K ;
Okuyama, K ;
Washiyama, J .
POLYMER, 2001, 42 (08) :3703-3708
[9]  
Ichikawa Y., 1995, POLYM J, V27, P1264, DOI [10.1295/polymj.27.1264, DOI 10.1295/POLYMJ.27.1264]
[10]   Crystal structure, thermal behavior and enzymatic degradation of poly(tetramethylene adipate) solution-grown chain-folded lamellar crystals [J].
Iwata, T ;
Kobayashi, S ;
Tabata, K ;
Yonezawa, N ;
Doi, Y .
MACROMOLECULAR BIOSCIENCE, 2004, 4 (03) :296-307