Microstructure and mechanical properties of double-wire plus arc additively manufactured Al-Cu-Mg alloys

被引:152
作者
Qi, Zewu [1 ,2 ]
Cong, Baoqiang [1 ,2 ]
Qi, Bojin [1 ,2 ]
Sun, Hongye [1 ,2 ]
Zhao, Gang [1 ,2 ]
Ding, Jialuo [3 ]
机构
[1] Beihang Univ, Sch Mech Engn & Automat, Beijing 100191, Peoples R China
[2] MIIT Key Lab Aeronaut Intelligent Mfg, Beijing 100191, Peoples R China
[3] Cranfield Univ, Welding Engn & Laser Proc Ctr, Cranfield MK43 0AL, Beds, England
关键词
Double-wire plus arc additive manufacturing; Al-Cu-Mg alloy; Microstructure; Mechanical properties; POSTDEPOSITION HEAT-TREATMENT; LAYER COLD-WORKING; POROSITY; 2219-AL;
D O I
10.1016/j.jmatprotec.2017.12.019
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
As the properties of wire + arc additively manufactured Al-6.3Cu alloy cannot meet the applying requirements, a double-wire + arc additive manufacturing system was built to add magnesium into Al-Cu deposits for higher mechanical properties. Two commercial binary wires aluminum-copper ER2319 and aluminum-magnesium ER5087 were chosen as the filler metal to build Al-Cu-Mg components with different compositions by adjusting the wire feed speed. The microstructure and morphology of thin wall samples were characterized by optical micrographs (OM), X-ray diffraction (XRD) and scanning electron microscopy (SEM). The Vickers hardness and tensile properties were investigated. The microstructure of Al-Cu-Mg deposits was mainly composed of coarse columnar grains and fine equiaxed grains with non-uniformly distributing characteristics. With higher Cu but lower Mg content, the strengthen phase turned to Al2Cu + Al2CuMg from Al2CuMg, and the micro hardness presented an increasing trend. The isotropic characteristics of ultimate tensile strength (UTS), yield strength (YS) and elongation were revealed in these samples. The UTS was about 280 +/- 5 MPa both in horizontal and vertical directions for all samples. The YS showed an increasing trend from 156 MPa to 187 MPa with the same content trend, while elongation decreased from 8.2% to 6%. The fractographs exhibited typical brittle fracture characteristics.
引用
收藏
页码:347 / 353
页数:7
相关论文
共 16 条
  • [11] Investigation of the benefits of plasma deposition for the additive layer manufacture of Ti-6Al-4V
    Martina, F.
    Mehnen, J.
    Williams, S. W.
    Colegrove, P.
    Wang, F.
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2012, 212 (06) : 1377 - 1386
  • [12] Oguzhan Y., 2016, P I MECH ENG B-MANAG, V230, P1781, DOI DOI 10.1177/0954405416640181
  • [13] Control of weld composition when welding high strength aluminium alloy using the tandem process
    Pickin, C. G.
    Williams, S. W.
    Prangnell, P. B.
    Robson, J.
    Lunt, M.
    [J]. SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2009, 14 (08) : 734 - 739
  • [14] RP NAGA, 2007, MAT SCI ENG A-STRUCT, V464, P192, DOI DOI 10.1016/j.msea.2007.01.144
  • [15] Application of modern aluminum alloys to aircraft
    Starke, EA
    Staley, JT
    [J]. PROGRESS IN AEROSPACE SCIENCES, 1996, 32 (2-3) : 131 - 172
  • [16] Wire plus Arc Additive Manufacturing
    Williams, S. W.
    Martina, F.
    Addison, A. C.
    Ding, J.
    Pardal, G.
    Colegrove, P.
    [J]. MATERIALS SCIENCE AND TECHNOLOGY, 2016, 32 (07) : 641 - 647