Defect induced non-ideal dark I-V characteristics of solar cells

被引:66
作者
Breitenstein, O. [1 ]
Bauer, J. [1 ]
Lotnyk, A. [1 ]
Wagner, J. -M. [1 ]
机构
[1] Max Planck Inst Microstruct Phys, D-06120 Halle, Germany
关键词
Solar cells; Silicon; Current-voltage characteristic; Recombination current; Shunts; Pre-breakdown; SHUNTS;
D O I
10.1016/j.spmi.2008.10.025
中图分类号
O469 [凝聚态物理学];
学科分类号
070205 ;
摘要
The non-ideal behavior of the dark current-voltage (I-V) characteristics of typical silicon solar cells is characterized by (1) an unexpectedly large recombination current, often characterized by an ideality factor larger than 2, (2) an ohmic characteristic at low reverse bias, and (3) pre-breakdown at a reverse bias far below the expected breakdown voltage. Experimental evidence, especially from lock-in thermography results, shows that all these features are due to currents flowing locally in the edge region, or at certain extended crystal defects like grain boundaries. Detailed investigations on local breakdown sites in industrial solar cells are introduced. Though a realistic theory of these processes is still missing, a unified explanation of non-ideal dark I-V characteristics is presented and several theoretical approaches to explain different aspects of this non-ideal behavior are discussed. (c) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:182 / 189
页数:8
相关论文
共 19 条
  • [1] Electronic activity of SiC precipitates in multicrystalline solar silicon
    Bauer, Jan
    Breitenstein, Otwin
    Rakotoniaina, Jean-Patrice
    [J]. PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2007, 204 (07): : 2190 - 2195
  • [2] Material-induced shunts in multicrystalline silicon solar cells
    Breitenstein, O.
    Bauer, J.
    Rakotoniaina, J. P.
    [J]. SEMICONDUCTORS, 2007, 41 (04) : 440 - 443
  • [3] Imaging Physical Parameters of Pre-Breakdown Sites by Lock-in Thermography Techniques
    Breitenstein, O.
    Bauer, J.
    Wagner, J. -M.
    Lotnyk, A.
    [J]. PROGRESS IN PHOTOVOLTAICS, 2008, 16 (08): : 679 - 685
  • [4] BREITENSTEIN O, P 17 EUR PHOT SOL EN, P1499
  • [5] Breitenstein O., 2006, PROC 21 EUR PVSEC, P625
  • [6] BREITENSTEIN O, 1994, P 1 WCPEC, P1633
  • [7] BREITENSTEIN O, 1994, SOLID STATE PHENOM, V37, P139
  • [8] Breitenstein O., 2003, Lock-in thermography: basics and use for functional diagnostics of electronic components
  • [9] BREITENSTEIN O, 2006, P 4 WORLD C PHOT EN, P789
  • [10] On the detection of shunts in silicon solar cells by photo- and electroluminescence imaging
    Breitenstein, Otwin
    Bauer, Jan
    Trupke, Thorsten
    Bardos, Robert A.
    [J]. PROGRESS IN PHOTOVOLTAICS, 2008, 16 (04): : 325 - 330